kapy academy

Functional multi-material parts

15 min readUpdated Nov 2026

You want a tool handle with a soft grip, a box whose lid carries its own gasket, a base with rubber feet or a phone stand that does not slide. For color, the second plastic only has to stay where it was put; for a functional part, the second material has to stay in place while the part is working. Two bodies of the same material fuse like any two neighboring beads. Two different materials may bond well, bond a little or not bond at all, and then the boundary between them is the weakest surface in the part.

Three printed parts on a gray bench: a gray rigid handle with a soft, ribbed black grip wrapped all the way round it, a box lid face up with a black gasket printed into a groove along its rim, and a white base upside down with its four soft black feet facing up (generated illustration)
Three printed parts on a gray bench: a gray rigid handle with a soft, ribbed black grip wrapped all the way round it, a box lid face up with a black gasket printed into a groove along its rim, and a white base upside down with its four soft black feet facing up (generated illustration)

Why two plastics bond (or do not)

A bead sticks to the one below or beside it because it arrives hot and remelts the surface of the bead already there. The chains of both polymers cross the boundary and tangle while everything cools. It is the same mechanism that holds layers together (Layer adhesion and anisotropy). With two different materials you need two conditions at once, and a third difference can still break the joint when both are met.

Chemical compatibility. The chains of the two polymers have to be able to mix, and in practice that takes a similar polarity. If they cannot, each stays on its own side however hot you print: at the boundary there are two surfaces touching, not a weld. You already know the proof from supports: PLA and PETG are used as support interfaces for each other precisely because they do not adhere and come apart cleanly, and Prusa documents exactly that for the XL. A pair that makes a good support makes a bad functional joint.

Heat at the contact. The boundary has to stay hot for long enough. If one material prints much cooler than the other, a bead of the cooler material cannot soften the surface of the other: PLA at 190–230 °C landing on PC printed at 260–290 °C sits on a plastic it cannot melt. Overlapping nozzle temperature ranges help, as with PLA (190–230 °C), TPU (200–250 °C) and PETG (230–270 °C).

Different shrinkage. Even when they bond, each material shrinks by a different amount as it cools: roughly 0.2–0.5 % for PLA, 0.3–0.5 % for PETG, 0.5–0.8 % for ABS, 0.5–1 % for TPU and 1.5–2.5 % for PP. Between two rigid materials with different shrinkage, such as PLA with ABS, a long flat boundary behaves like a bimetallic strip and the part curls. Between rigid and soft, TPU is too flexible to bend the core, so the mismatch comes out elsewhere: stress gathers at the ends of the boundary and the joint peels from there. Either way, shorten long boundaries or break them into segments. Shrinkage and dimensional stability covers this in depth.

Which pairs bond

The table is a practical guide, not a list of measured strengths. Additives, colorants and each brand's quality shift the result somewhat, so test the pair with the spools you are going to use.

Common pairs (indicative)
Pair Level What to expect
Any material with itself (PLA + PLA in two colors) Fuses Like a single-material part
ABS + ASA, PC + ABS, PETG + PCTG Fuses, in practice Closely related chemical families
TPU + PETG Bonds Users report it as TPU's best partner
TPU + PLA Bonds, but less Usable; better with interlocking or a key
TPU + ABS Bonds, according to users Test it first
PLA + PETG Does not bond A support pair: it separates cleanly
PP + common filaments (PLA, PETG, ABS, TPU) Does not bond Only fuses to other PP
PLA + PC, PLA + PA Does not bond Different chemistry and a large temperature gap

That TPU adheres better to PETG than to PLA rests on user reports; there is no published measurement. When Bambu Lab introduced its TPU 90A for printing alongside PLA and PETG on the H2D, it paired it with the slicer's beam interlocking, not an unreinforced joint.

PP is the extreme case: it will not even stay on the bed without a PP sheet or packing tape. With any of the common filaments, the joint has to be mechanical.

Fiber-filled filaments usually adhere worse than their base polymer, because there is less free polymer at the surface to diffuse. With a PA-CF or a PETG-CF, design a key in from the start.

Supports are the other use of a second material: a pair chosen precisely because it does not bond, or a soluble material. Their chemistry and interface design are in Support materials.

Design the joint: area, load, edges and orientation

ShearRigidSoftLoad spreadPeelRigidSoftLoad at the edgeSharp cornerRounded
In shear, the joint spreads the load across the whole boundary; in peel, it concentrates it at the edge that lifts. A rounded corner on the rigid part relieves that edge.

Area. Adhesion acts per unit of surface, so the first thing you can increase is the contact area. On a 10 mm cube, a TPU pad on the top face touches 100 mm². Carry it down all four sides as well and you add another 400 mm²: five times the area. Wrap the rigid part in the soft material instead of resting it on a single face.

Shear or compression, never peel. In shear, the load spreads across the whole boundary. In peel it concentrates on the line where the soft material lifts, and a joint that holds well in shear tears in peel, starting at an edge. A grip squeezed by the hand works in compression and shear: fine. A rubber strap pulling away from the face it is anchored to works in peel: it needs a key.

Edges. Where soft meets rigid, the soft side stretches and the rigid side does not, so the strain piles up at the edge of the joint. Round the corners of the rigid part at the boundary rather than leaving a sharp step, and taper the soft overmold to a feather edge instead of ending it square. In tests of interlocked PLA and TPU joints, failure starts at the smallest features, where stress concentrates.

Orientation relative to the layers. A vertical boundary, with both materials side by side in the same layer, is welded bead to bead in every layer, and the slicer's interlocking can weave it. A horizontal boundary, with one material stacked on the other, is a single layer-to-layer joint: it inherits the Z weakness of every printed part, and on top of that it joins two plastics that bond less well. In practice, orient the part so the boundary is vertical when you can, though this competes with the other orientation criteria.

Print order. Printing rigid on soft is harder than the reverse: a rigid bead landing on a few layers of TPU can push them sideways, as Prusa warns for the XL. If the design allows it, put the rigid material at the bottom and the soft one on top.

The slicer's interlocking

Near the boundary, the slicer replaces each material's solid infill with beams that change direction from one band of layers to the next and pass through the other material. The two lattices end up woven into each other, and the joint holds by geometry, not chemistry.

The idea comes from work at TU Delft (Kuipers and colleagues, Additive Manufacturing, 2022) and reached Cura as "Generate Interlocking Structure" in version 5.3. The authors tested it with PLA and PP, a pair with no chemical adhesion at all: in the diagonal orientation the lattice reached 82 % of its theoretical ceiling of 8.6 MPa, comparable to a dovetail. That is why it matters: it works with pairs that do not bond at all.

As of late 2026, every major slicer has it:

Interlocking in each slicer
Slicer Option
Cura "Generate Interlocking Structure"
OrcaSlicer, Bambu Studio "Interlocking beam"
PrusaSlicer "Use beam interlocking"

They all offer the same settings: beam width, direction, layers per beam, depth and boundary avoidance. Depth and boundary avoidance are measured in cells. Fewer layers per beam make a stronger joint, but more defects appear. There are no universal figures: start from the values your profile ships with and compare them on a coupon. PrusaSlicer and Orca also have the "Interface shells" option, which puts walls on the boundary between materials and changes how they meet; try it on the same coupon, with and without.

It has limits: the published lattice is designed for vertical boundaries, and the authors left other orientations for future work. On a horizontal stacked boundary you gain little, and against a peel load do not count on it alone.

It also needs room: the beams are generated some depth into the boundary and kept away from the outer surface, so a 1 mm soft skin over a rigid core leaves them hardly any space. Give the joint a few millimeters of material on each side.

One incompatibility is worth knowing: in PrusaSlicer, turning on beam interlocking disables the painting depth settings ("Maximum width of a segmented region" and "Interlocking depth of a segmented region"). Those settings are covered in Assigning colors in the slicer.

Keys you model yourself

Butt jointAdhesion onlyRigidSoftBeam interlockingGenerated by the slicerRigidSoftModeled keyHolds without adhesionRigidSoft
A butt joint relies on adhesion alone; the slicer's interlocking weaves the two materials; a modeled key traps the soft material and holds even with zero adhesion.

When the pair bonds poorly or the load is in peel, design the joint to hold without adhesion: the soft material has to be trapped by the rigid one, so it cannot come out without tearing.

Plastic rivets. A row of through holes in a rigid flange. The TPU fills them, joins the two faces and forms rivets. The minimum for them to come out as clean holes is a diameter of two line widths (with a 0.4 mm nozzle the line width is around 0.45 mm, 0.42 in Bambu Studio), but a 0.9 mm TPU pin tears under the slightest load: a rivet's strength goes with its cross-section. In practice, use 2–4 mm holes, space them at least one diameter apart and leave rigid walls of 1.2 mm or more between them (never less than two beads, 0.9 mm).

Undercuts. Dovetail or T-slots along the rigid part that the soft material fills; a mushroom-headed post; a lip the soft material wraps around. Orient them to print without supports, with the usual overhang rule (Orientation and overhangs).

In a TU Delft thesis on PLA and TPU joints, three geometric solutions gave similar figures in the same test series: an interlocking bridge pattern held 491 N, Cura's mesh overlap option 415 N and a flat interlocking shape 504 N. These are figures from a single study, not a rule, but they show that more than one geometric route reaches similar strength.

Model the two materials as separate bodies that meet face to face: the soft body fills the rigid one's holes and slots exactly, with no gap and no overlap. If they overlap, the slicer decides which material takes the shared volume; if there is a gap, you get a slit. It is the same discipline as Designing for multicolor.

Printing the two materials

Machine. Soft TPU (85A, 90A, 95A) cannot be pushed through the long tube of a filament switcher: it needs a short, direct path, like a toolchanger's or a second nozzle with its own extruder (Toolchangers, IDEX and dual nozzles). A filament switcher prints rigid pairs and D-hardness TPU, such as Bambu Lab's "TPU for AMS", which has a Shore hardness of 68D. The limit is hardness, not the TPU label: the AMS 2 Pro does not accept generic TPU or TPE (Filament switchers: AMS, MMU, CFS and ACE). Careful with the X2D: its second nozzle is Bowden-fed and does not accept TPU.

Purge. On a toolchanger each material has its own nozzle, but the incoming one has to be primed: Prusa tested TPU on the XL with a minimum purge of 35 mm³ per tool and suggests going up to 70 mm³ if it strings or oozes. If a D-hardness TPU shares a nozzle with a rigid material on a filament switcher, the change needs more purge than a color change; tune it on a coupon. The rest is in Purge and multicolor waste.

Drying. Dry TPU at 70–75 °C for 8–18 h. If it is damp, it strings over the rigid part (Drying and storing filament).

Bed. There is one bed temperature for two materials. PLA (35–65 °C) and TPU (30–45 °C) share a range; PETG (60–80 °C) and TPU do not. Put the material that needs the hotter bed on the first layer and let the other start higher up. PrusaSlicer takes the bed temperature of the first layer from the first material it prints, and the one for the rest of the part from the first material of the second layer. If the temperatures differ a lot, it warns. To decide it yourself, pick in "Bed temperature by extruder" (print settings, multiple extruders section) the extruder of the first-layer material. In an enclosed printer, open the door for PLA or TPU once the bed is above about 45 °C, so the filament does not soften before it reaches the nozzle (Enclosures and heated chambers).

Speed. TPU paths run slowly, capped by TPU's maximum volumetric flow, and every mixed layer costs at least one material change. Expect a long print; it is not a fault.

An example: a handle with a grip

A screwdriver-style handle in PETG with a TPU 95A grip, printed on a toolchanger or with the TPU through the direct-drive nozzle. PETG and TPU adhere, so the chemistry helps. The grip goes all the way round, so the area is as large as it can be. The hand squeezes and twists it: it works in compression and shear, never in peel. Under the grip, the core carries lengthwise ribs that the TPU fills, a key against torque that prints without supports with the handle standing up. Standing up also makes the boundary vertical, so the slicer's interlocking can weave it. The bottom end is solid PETG, so the first layers are PETG on a 70 °C bed and the TPU starts higher up; on an enclosed machine, door open for the TPU. Taper the grip to a feather edge at both ends so the edge does not lift.

When it fails

Faults in a multi-material joint
Symptom Cause Fix
The soft part peels off whole, in one clean sheet Incompatible pair or cold boundary Interlocking or rivets; rigid at the bottom
The joint tears from one end Peel load, sharp corner or long rigid-to-soft boundary Wrap the part, round the corner, shorten or break up the boundary
The whole part curls like a banana Different shrinkage between two rigid materials Break up the boundary or shorten it
The grip spins on the core Adhesion carries all the torque Ribs or slots along the core
Jams, short purges or oozing The machine, not the joint design Multi-material failures

How to test it

Test the joint on a coupon before you print the part. Print three pairs of bars, one rigid and one soft, overlapping by 10–15 mm: one unreinforced, one with interlocking and one with a row of rivets. Pull each one by hand, first in shear and then in peel. If the unreinforced pair comes apart cleanly, the pair does not bond: rely on geometry (Test coupons).

See also

Design it in KapyCAD

Many of these problems are cheaper to fix in the model than in the slicer: wall thickness, overhangs, the face the part stands on.

Free plan, no card. Runs in your browser, nothing to install.

Open the editor

Still have a question?