kapy academy

Overhang and bridge settings

17 min readUpdated Nov 2026

Between the face that prints cleanly on its own and the face that needs support lies a band of overhangs and bridges the slicer can rescue by changing how it lays the bead: slower, with more air, with a different wall order, or with a thicker or thinner bead. Any machine handles 45° from vertical and a modern, well-cooled one reaches 50–60°; with these settings you get to 60–70°, and to 90° in special cases. In PLA, a modern machine spans bridges up to 20 mm cleanly and up to 50 mm with some sag.

How the slicer measures an overhang

The part of the bead that hangs out has nothing below it to draw heat away or hold it up. It takes longer to solidify, sags under its own weight and, because its top cools first, shrinks there and curls upwards. Every overhang setting does one of two things: it gives the bead more time to solidify (speed, fan) or it gives it something to lean on (wall order, extra perimeters).

On a sloped wall, each layer sticks out past the one below by layer height × tan(angle from vertical). OrcaSlicer, Bambu Studio and PrusaSlicer do not look at the angle: they look at how much of each outer-wall bead lies outside the bead below, as a percentage of line width. With 0.20 mm layers and 0.45 mm beads, a 45° overhang shifts each layer 0.20 mm and leaves 44 % of the bead in the air. At 60° the shift is 0.35 mm, 77 %. From about 66° the shift exceeds the whole bead, and that bead is in practice a bridge.

angle from vertical30°≈ 26 %45°44 %layer height × tan(angle)60°77 %the bead is now a bridge70°100 %0 %10 %25 %50 %75 %100 %unsupported (Orca, Bambu Studio)100 %75 %50 %25 %0 %overlap (PrusaSlicer)
The same 0.45 mm bead at four angles with 0.20 mm layers: the hanging part grows fast, and at about 66° nothing is supported. Orca and Bambu Studio count what hangs; PrusaSlicer counts what rests.

Thinner layers leave less of the bead in the air at the same angle. At 0.12 mm, a 60° overhang shifts each layer 0.21 mm, 46 %, the same as 45° at 0.20 mm. That is why variable layer height helps on a steep underside (Layer height and line width).

Slicer labels are quoted as they appear on screen. Be careful when comparing percentages across slicers. Orca and Bambu Studio name their bands by the unsupported share of the bead (10, 25, 50, 75 and 100 %). PrusaSlicer names them by overlap with the layer below ("speed for 0% overlap (bridge)", 25, 50 and 75 %), so Prusa's 25 % is roughly Orca's 75 %. Cura uses an angle, "Overhanging Wall Angle", set to 90° in the generic profile, which means off. The other naming differences are in Orca, Bambu Studio, PrusaSlicer and Cura.

Overhang-dependent speed

The slower the nozzle crosses the void, the more air each millimeter of bead gets, and the less the nozzle drags it outwards while it is still soft. On an overhang, going slower means more time to cool.

Default overhang speeds, end of 2026
Slicer and profile Setting Bands and speeds
Bambu Studio (Bambu profiles) and Orca (Bambu profiles and generic Custom) "Slow down for overhangs", on 10–25 % unsupported: wall speed; 25–50 %: 50 mm/s; 50–75 %: 30 mm/s; 75–100 %: 10 mm/s; 100 % (Bambu): 10 mm/s
PrusaSlicer, MK4S and CORE One profiles "Enable dynamic overhang speeds", on (off in the factory configuration, with no printer profile) 0 % overlap: 15 mm/s; 25 %: 25 mm/s; 50 %: 30 mm/s; 75 %: 80 % of external perimeter speed
Cura "Overhanging Wall Speeds" list of percentages of wall speed (e.g. [75, 50]); only acts on walls steeper than "Overhanging Wall Angle"

In Orca and Bambu Studio, "Slow down for overhangs" only applies if "Detect overhang walls" is on, and it is by default. In Orca, the fully unsupported part runs at bridge speed; Bambu Studio gives it a value of its own (10 mm/s in its profiles). Bambu's filament profiles can impose their own overhang speeds per material. PrusaSlicer's "Enable dynamic overhang speeds" interpolates linearly between its four points and never exceeds the maximum volumetric flow. In Cura, with the factory angle at 90°, the setting does nothing until you lower it; 45–50° is a good starting point.

The catch is banding. A big jump from a fast wall to a slow overhang changes the pressure in the nozzle and leaves a visible stripe on the outer wall. "Smooth speed discontinuity area" (on in Bambu Studio) spreads the change, and Orca's "Enable adaptive pressure advance for overhangs (beta)" corrects the same mark. If the stripe bothers you more than the drooping overhang, raise the 25 % and 50 % bands first. The mark itself is explained in Wall marks: ringing, VFA and Z-banding.

"Slow down for curled perimeters" slows the nozzle further where earlier layers have already lifted, as on the bow of the Benchy test boat. In Orca it is off by default and on in the generic Custom profile. Turn it on when you hear the nozzle strike a steep, curved overhang. PrusaSlicer also has "Avoid crossing curled overhangs (Experimental)", which reroutes travel moves so they do not pass over those edges.

Overhang and bridge cooling

Overhang cooling solidifies the bead before it sags. It is the same part-cooling fan running faster, only where the slicer detects an overhang or a bridge.

Orca and Bambu Studio use three settings: "Force cooling for overhangs and bridges", "Overhangs and external bridges fan speed" and "Overhang cooling activation threshold". With the threshold at 0 % the fan boosts on the whole outer wall; at 95 %, only on bridges. In Orca, with "Internal bridges fan speed" at −1, internal bridges take the overhang value. In PrusaSlicer, "Bridges fan speed" covers bridges, and the MK4S PLA profiles add "Enable dynamic fan speeds" with the fan at 100 % at 0 and 25 % overlap. In Cura, "Bridge Fan Speed" defaults to 100 %, but only takes effect with "Enable Bridge Settings" turned on.

The layer fan is set per material, from nearly full on PLA to very little on ABS (Speed and cooling). On overhangs and bridges it goes up: PLA to 100 %, PETG to 50–90 % and ABS and ASA up to 80 %, the last two always in an enclosed printer. If one side of a round overhang droops and the other does not, no setting fixes it: the air does not reach both sides equally, and the same article covers how to check the duct.

Walls that lean on each other

Wall order. With inner walls first and the outer wall last ("Inner/Outer" in Orca and Bambu Studio; "External perimeters first" off in PrusaSlicer, as in the MK4S profile), the outer bead of the overhang leans sideways on the inner bead laid a moment before. With the outer wall first, or with "Inner/Outer/Inner", the outer bead has no neighbor and the overhang suffers; Orca's own help text warns about it. The cost in dimensional accuracy is explained in Walls, perimeters and infill.

"Reverse on even" (Orca only, off). Overhanging walls change direction on alternate layers, so each pass cancels the pull and curl of the one before. "Reverse threshold" defaults to 50 % of line width. It helps on very steep overhangs and reduces edge lift, which is useful in ABS and ASA; "Reverse only internal perimeters" leaves the outer wall untouched.

"Extra perimeters on overhangs" (off in Orca and in PrusaSlicer 2.6 or later, where it is labeled "Experimental"). Where an area has no anchor for a bridge, the slicer fills it with perimeters that grow out from the supported edge, each bead stuck to the one before. It is slow and the underside shows concentric rings, but it can close a 90° shelf that would otherwise need support.

Seams. A seam on an overhang is a blob in mid-air. Orca skips the scarf seam on overhangs above 40 % ("Conditional overhang threshold"), and Bambu Studio has "Seam placement away from overhangs (experimental)". The rest is in Where the seam goes.

When the slicer changes the part

Orca's "Make overhangs printable" (off, with a 55° maximum angle and hole area 0) and Cura's "Make Overhang Printable" (off, with "Maximum Model Angle" at 50°) add volume under steep overhangs: a cone at the angle you set, sliced with the same walls and infill as the rest of the part. You save the support at the cost of changing the geometry: a hole in the underside gets filled unless it exceeds the area limit, and the part no longer matches the drawing.

If the part is yours, put that chamfer in CAD, where you can dimension it (Designing out supports). Keep the slicer option for a downloaded mesh you cannot edit.

Arc overhangs

Arc overhangs (Steven McCulloch, 2022) grow the toolpath in concentric arcs over the void, each bead resting on the one before, so a horizontal shelf prints without support, slowly and with a ring pattern on its underside. As of late 2026 they are still outside the official slicer releases, available as a post-processing script or in community forks, like their 2026 wave-shaped variant (Advanced toolpaths); the closest thing the slicers ship is "Extra perimeters on overhangs".

It pays off on a flat shelf you cannot reorient or support. It does not pay off in a production run or on a visible underside.

What the slicer treats as a bridge

A bridge is a set of strands (the bridge's beads) stretched between two anchors, each solidifying in the air before gravity pulls it down. It needs three things at once: an anchor at both ends, tension (moderate speed and flow equal to or slightly below normal) and fast cooling. Bridge speed is neither flat out nor 10–15 mm/s: it runs slower than the walls, with the fan at 100 % in PLA and a flow ratio around 1.0.

The slicer calls a region a bridge when it has nothing below and support on two opposite sides. With support on one side only it is an overhang, and only support or "Extra perimeters on overhangs" will do there. The slicer picks the direction that crosses the shortest anchored span; "Bridge infill direction" or "Bridging angle" (0 = automatic) let you fix it. Change it only when the automatic choice runs along the long side of a slot.

Anchor wallsOpeningAnchoredAlong the long side: longer unsupported spanThin bridgeh = layer heightSmooth undersideThick bridgeh = nozzle diameterNext layerRibbed underside
Strands cross the short side of the opening and anchor in the walls. In section, a thin bridge leaves a smooth face; a thick one leaves separate round strands the next layer has to fill.

In Orca and Bambu Studio, "Max bridge length" defaults to 10 mm and only applies while the switch that leaves every bridge unsupported is off (its label is in the fault table below). When to put support under a bridge is decided in Support settings.

Thick or thin bridges

A thick bridge is extruded at a height equal to the nozzle diameter (0.4 mm with a 0.4 mm nozzle): round strands with gaps between them. It is stronger and tolerates long spans and weak cooling, but the underside comes out ribbed and the layer above has to fill the grooves. A thin bridge uses the normal layer height: flat strands that touch and a smoother underside, reliable only on short spans.

Default thick bridges, end of 2026
Slicer External Internal
Orca "Thick external bridges": off "Thick internal bridges": on
Bambu Studio "Thick bridges": off —
PrusaSlicer "Thick bridges": on in the factory configuration, off in the MK4S and CORE One profiles —

On a modern machine, use thin bridges on visible faces, and thick ones when a long or hidden bridge keeps sagging or snapping. In Orca, "Bridge line width" defaults to 100 % of the nozzle; do not raise it. For a smoother underside, try a narrower line with higher density.

Bridge flow, speed and acceleration

Flow. "Bridge flow ratio" is 1.0 in Orca, in PrusaSlicer and in Bambu's 0.20 mm profiles (0.95 in the base profile they inherit from), and it multiplies the filament's flow ratio. Below 1 the strand comes out thinner and stays taut, so it sags less; go too low and strands break or leave gaps. Adjust in steps of 0.05. In Cura, "Bridge Skin Flow" (60 %) and "Bridge Wall Flow" (50 %) apply the same idea with much lower values, and only take effect once "Enable Bridge Settings" is on.

Default bridge speed and acceleration
Slicer and profile Bridge speed Acceleration
Bambu Studio (Bambu profiles) 50 mm/s (external) —
PrusaSlicer, MK4S profile 50 mm/s (30 in some Prusa profiles) 1,500 mm/s²
Orca, generic 25 mm/s external; internal at 150 % 50 % of outer wall acceleration
Cura "Bridge Skin Speed" 15 mm/s: a low generic value; on a modern machine, 25–50 mm/s like the rest —

There are two reasons for a moderate speed. Too slow, and the strand cools before it is pulled taut, so it droops and bunches up; too fast, and it snaps or does not solidify before it reaches the far anchor. Harsh acceleration tears the first strand off its anchor.

Pressure. On a bridge the nozzle extrudes with nothing beneath it, pressure drops and the bead right after the bridge comes out thin. If you see a short gap at the end of every bridge, pressure advance is too high there: lower it on bridges with "Pressure advance for bridges", in Orca's filament settings.

The layer above. PrusaSlicer's "Over bridges" (50 % of solid infill speed in the MK4S profile) and Cura's second and third bridge layers slow down the layers directly above so they do not break the bridge.

Bridge density and extra bridge layers

Orca's "External bridge density" and "Internal bridge density" default to 100 %. They change the spacing between strands, not the flow in each one, so do not confuse them with the flow ratio. Above 100 %, if your version allows it, strands overlap and the face comes out smoother but overextruded. Below, they sit apart, cool faster and form a first layer that the next one closes. Cura's "Bridge Skin Density" follows the same scheme: 100 % and a second layer at 75 %.

Orca's "Extra bridge layers (beta)", off, prints a second bridge layer over the first so the solid infill above rests on something firm. Orca recommends at least "External bridge only". It helps on fast machines, where bridge speed and infill speed differ a lot.

Internal bridges and counterbores

The first solid infill layer over sparse infill is a bridge between the infill walls. If it sags, the top surface comes out with bumps and holes. What to adjust: thick internal bridges (on by default in Orca), internal bridge flow and density, Orca's "Filter out small internal bridges" set to "Limited filtering" or "No filtering" on curved or sloped top surfaces, and "Internal bridge support thickness" in Bambu Studio. The number of top layers and the rest of the problem are in Top surfaces.

A counterbore over a through hole leaves a ring-shaped step with nothing below it. Orca's "Bridge counterbore holes" offers "None", "Partially bridged" and "Sacrificial layer". The sacrificial layer lays a full bridge over the hole, which you then drill or cut through. It is the slicer's version of the sacrificial layer you can also model (Captive nuts and clearance holes).

When it fails

Symptom, cause and fix
Symptom Cause Fix
Rough or drooping underside on a steep overhang The bead hangs soft for too long: too little air or too much speed Overhang fan and its threshold; slower 50 % and 75 % bands; thinner layers
Edges lifting, nozzle striking them The overhang's edge curls upwards as it cools "Slow down for curled perimeters"; "Reverse on even"; more fan
Stripe on the outer wall at overhang height A sharp speed jump between wall and overhang Raise the 25 % and 50 % bands; smooth the transition
Bridge strands drooping in the middle The strand comes out slack or cools late Fan at 100 % (PLA); flow ratio 0.90–0.95; thick bridges
Strands broken or loose at the anchor Bridge acceleration or speed too high Lower bridge acceleration and speed
Gap right after the bridge Pressure advance too high leaving the bridge "Pressure advance for bridges" (Orca)
Bumps on the top surface An internal bridge sagged under the solid infill Internal bridge settings; Top surfaces
90° shelf with no anchor It rests on one side only: an overhang, not a bridge "Extra perimeters on overhangs", support or a redesign
Short bridges get support, or long ones get none "Don't support bridges" on, or a "Max bridge length" that does not match your machine Leave "Don't support bridges" off and set "Max bridge length" to the span your machine prints cleanly
The settings barely change the result The geometry is outside the band Reorient the part (Orientation and overhangs) or give it support

How to test it

Before you touch any setting, find out where your machine's limits are. Print two tests with your usual profile, no supports and the material you will actually use: an overhang test with steps every 5° from 30° to 70°, and a bridge test with spans from 10 to 50 mm. PETG and ABS usually land 5–10° below PLA on overhangs and span shorter bridges.

A bridge and overhang test: the short bridges come out taut, the long ones droop, and the steepest overhangs come out rough (generated illustration)
A bridge and overhang test: the short bridges come out taut, the long ones droop, and the steepest overhangs come out rough (generated illustration)

Judge the result strictly: a bridge that sagged and recovered has failed. In a current Bambu Studio, Orca or PrusaSlicer profile, overhang slowdown, overhang cooling and the bridge settings are already on with sensible values; start from them. Change one setting per test print, in this order: the fan (is it really blowing harder on the overhang?), the speed, the wall order, the flow ratio and, last, the special tools.

See also

Design it in KapyCAD

Many of these problems are cheaper to fix in the model than in the slicer: wall thickness, overhangs, the face the part stands on.

Free plan, no card. Runs in your browser, nothing to install.

Open the editor

Still have a question?