kapy academy

Designing flexible parts

13 min readUpdated Nov 2026

Rubber feet, bumpers, phone cases, grips, gaskets, strain reliefs: in every one you want a part that gives exactly as much as you planned and springs back. The stiffness of a TPU part is the stiffness of the material multiplied by the stiffness of the geometry. Going from 85A to 95A multiplies it by about three; wall thickness, infill and shape change it tenfold or more. So decide first how much the part has to give, then pick the hardest grade that still gives enough: hard TPU prints far more reliably than soft.

Three ways to give

LoadLtBendingLoadLoadBonded: barely givesFree sides: givesSame volumeCompressionLoadBuckling
A strip gives by bending and a thin wall by buckling. A solid block bonded top and bottom barely deforms: rubber keeps its volume and has nowhere to go.

Bending. A strip or a thin wall bends. Its stiffness rises with the cube of the thickness and falls with the cube of the length: the same law you meet in Ribs, gussets and fillets and in a snap-fit arm. That is how the lip of a phone case or the tail of a strain relief gives.

Compressing solid rubber. TPU is almost incompressible: its Poisson's ratio is close to 0.5. Squeeze it and it keeps its volume, so it has to bulge sideways. If it is bonded top and bottom to rigid faces, it cannot bulge and ends up much stiffer than the material itself. A tall, slender block, or one with free sides, gives more. In rubber anti-vibration mounts this is called the shape factor, and it explains why a TPU foot printed at 100 % feels far harder than its Shore hardness suggests.

Buckling of walls and cells. Thin walls and infill cells fold under load, give at an almost constant force and stiffen once they close up against each other (densification). Nearly all the softness of a printed TPU part comes from here: sparse infill is a foam you design yourself.

The classic mistake: a solid block of TPU, chosen "because TPU is soft", that hardly deforms at all. The fix is to give the rubber somewhere to go: hollow it, slot it or lower the infill.

Why shape beats Shore hardness

×1×2×4×8×30×100Shore 85A → 95A (≈ ×3)Infill density doubled (×2–×4)Wall twice as thick, in bending (×8)95A → 68D (×30–×100)Stiffness factorlog scale
How much each lever multiplies stiffness. Moving from a soft grade to a hard one changes it less than doubling a wall's thickness; a 68D TPU is a different class of material.

Shore hardness is not proportional to modulus. By Gent's empirical relation, going from 85A to 95A multiplies the modulus by about three. Treat that as an estimate for comparison, not a datasheet figure.

Doubling a wall's thickness multiplies its bending stiffness by 8 (2³). Doubling the density of an infill whose cells work in bending multiplies it by about 4, because in those cells stiffness grows with the square of relative density (Gibson and Ashby's scaling law; printed cells stray from it, but the order of magnitude holds). In Z compression with vertical-wall patterns such as grid or honeycomb, the walls act as columns and the gain is closer to ×2, until they buckle. And freeing the sides of a solid block changes its compressive stiffness more than any change of grade.

Datasheets confirm the jump between classes. Bambu Lab quotes a modulus of 9.2 MPa in XY for its TPU 95A, and 1190 MPa for its AMS-compatible TPU, a 68D grade. On that datasheet the 68D comes out more than a hundred times stiffer than the 95A; across brands the typical gap is tens of times, because 9.2 MPa is low for a 95A. Either way, a 68D "TPU" is a tough semi-rigid material. Only compare grades on datasheets from the same brand: every manufacturer tests its own way, and moduli from different brands are not comparable.

One more lever changes softness without touching the geometry: foaming TPUs, whose density and stiffness depend on nozzle temperature and flow. How to print them is in TPU and flexible filaments.

Walls and infill: fine-tuning stiffness

Walls, top and bottom layers and infill are explained in Walls, perimeters and infill. In TPU each has a mechanical job. The walls carry bending and form the outer skin. The infill sets the softness in compression. The top and bottom layers form a sandwich that raises bending stiffness.

Starting points for TPU (0.4 mm nozzle)
Part Walls Infill Top/bottom layers
Soft foot, bumper, grip 2 10–20 % gyroid 2–3
Case, strain relief (works in bending) 2–3 15–25 % 3
Gasket, tread, wear pad as many as needed 100 % solid

The test coupons in the last section give you the final values.

Load2 wallsSparse gyroidTop/bottom layers2 walls + 15 % gyroid: givesLoad100 % solid: barely gives
Two identical TPU feet in section, under the same load. With two walls and sparse gyroid, the cells bend and the foot squashes. Solid and bonded to the plate and the table, it barely gives.

The pattern matters. Pick one whose lines do not cross within a layer. In a crossing pattern such as grid, every intersection stacks two lines: you get a stiff lump and the nozzle drags through soft plastic. Gyroid has no crossings and responds much the same in every direction, so it is the safe choice, although at equal density it comes out stiffer than Cross 3D. As of late 2026, Cura's documentation recommends Cross 3D for flexible parts for its near-isotropic response, and PrusaSlicer's lists concentric, Archimedean chords and octagram spiral as patterns that help flexibility. If you want the softest possible part at a given density, try one of those; if you want a predictable response, stick with gyroid.

If one region has to hold (a mounting boss) and another has to give, you do not need to change the model: add a modifier volume with more walls or more infill where the part must grip and less where it must give. Modifiers by region and height explains how.

Modeling flexibility

When the slicer is not enough, build the flexibility into the model. Hollow the part to the wall you want, cut slots or reliefs through a block, use bellows walls for axial travel, put thin columns or ribs under a foot so they buckle, or model a lattice with graded stiffness. Every one of these turns compression into bending or buckling, the two modes that actually give.

A bellows is a chain of short strips in bending: travel adds up fold by fold and the stiffness is shared between them. Give it a wall of at least 1.2 mm so each fold prints solid, and round the inside of every fold (the next section explains why).

The wall minimums still apply. A single-line TPU wall is a membrane that tears and buckles unpredictably. Keep at least 2 lines, 0.9 mm with a 0.4 mm nozzle; the minimums for detail and text are in Minimum features and text.

Lattices and auxetic cells as cushioning are in Auxetics and lattices, and TPU and lattice springs in TPU and lattice springs.

It stretches a long way, but tears at notches

According to Bambu Lab's datasheet, its TPU 95A stretches more than 700 % in XY before it breaks, and more than 500 % in Z. What limits it is not stretch but tearing. A sharp inside corner or a cut concentrates the strain, and a tear starts there at a fraction of that elongation.

Round every inside corner that stretches or folds, with a radius of at least the wall thickness. End slots in a round hole, never in a square end.

The bonds between layers are notches in Z, and here the grade decides. Soft grades weld well between layers: the same maker's TPU 85A keeps 88 % of its XY strength in Z. Hard grades do not: its TPU 68D breaks at 31 % elongation in Z versus more than 650 % in XY, and its impact strength drops from 124 kJ/m² in XY to 9.6 in Z. Make the part stretch and fold along the lines, and print straps and bands lying flat. More in Layer adhesion and anisotropy. If you are designing a hinge, the lines run across the hinge axis, perpendicular to it, never parallel; the geometry is in Living hinges and flexures.

TPU dissipates part of the energy in every loading and unloading cycle (hysteresis): that is why it damps, and why it suits anti-vibration feet and bumpers. It also stiffens noticeably in the cold: a foot or gasket outdoors in winter will feel harder than it did in the workshop.

Sealing gaskets

Squeeze 15–30 % of hLidGasket (height h)GrooveLid openLidFree spaceLid closedGroove full: extrudes
A compressed gasket keeps its volume and bulges sideways: the groove needs free space. A gasket that fills the groove exactly stops the lid closing or squeezes out through the gap.

Incompressibility rules here too. A compressed gasket keeps its volume, so the groove has to leave it room to bulge. For a static seal, compress it by 15 to 30 % of its height and make the groove larger than the gasket, with a maximum fill of around 85 %. These are the usual O-ring values, adapted to printed TPU: check them on your enclosure.

Print it solid, at 100 % infill and with enough walls, so it seals through the material and not through the gaps in the infill. Seal with the top face and set the top-layer pattern to concentric, so the beads run along the gasket rather than across it: grooves that cross the gasket's width are leak paths. The bottom face, printed on textured PEI, comes out textured and does not seal well. Dry the TPU first, 8 to 18 hours at 70–75 °C: wet, it leaves pores and strings (Drying and storing filament).

Under constant compression and heat, TPU creeps (compression set) and loses force over the months. For a lid you open often, a printed gasket works. For a permanent seal that runs hot, buy an O-ring and design the groove for it. If you want to print the gasket straight onto the rigid lid, see Functional multi-material parts.

Interference, clearances and overhangs

A TPU case, bumper or grip holds a rigid part by stretching around it, so it accepts an interference that would crack a rigid part. Size it as a strain percentage, not in tenths of a millimeter: start with a few percent of the diameter and test. The rigid fit scale in Choosing the fit: clearance, transition, interference does not apply here.

Holes and gaps in TPU close up more than in PLA: the material oozes and the soft wall yields when you squeeze the callipers, so the measurement lies. A print-in-place mechanism in TPU fuses solid at clearances that work in PLA; give it more gap and test (Print-in-place clearances).

Design without supports. Printed TPU support fuses to the part and is hard to remove, and bridges sag because an elastic strand will not hold tension. Stay within 45° from vertical (Designing out supports), give the part a flat face on the bed and keep small details thick: TPU strings and blobs (Stringing and blobs). If your printer has two nozzles or a toolchanger, a support interface in another material, such as PLA, releases far better than TPU support; material pairings are in Functional multi-material parts.

Feeding, speed, retraction and the extruder belong to printing, not design: they are in TPU and flexible filaments and Extruders: direct drive or Bowden. Using glue stick as a release agent on textured PEI is covered in Bed prep for each material.

When it fails

Symptom, cause and fix
Symptom Cause Fix
The solid foot does not give Rubber bonded top and bottom has nowhere to go Drop the infill to 10–20 %, free the sides or hollow it
The part was meant to be soft and came out hard It was sliced with another profile, or with a grid pattern that stacks beads at the crossings Switch to gyroid and record the profile
The strap splits between layers on the first pull It was printed standing up, or the grade is hard Print it flat and make it stretch along the beads
The slot tears from its end The end was square Finish it in a round hole and round the inside corners
The lid will not close with the gasket fitted The gasket fills the groove Enlarge the groove to an 85 % fill at most
The gasket leaks even though the lid closes It is sealing on the textured face, or the top-layer grooves cross the gasket Seal with the top face, printed concentric

How to test it

Before the real part, print three or four small blocks, around 20 × 20 × 10 mm, with the walls and infills you are considering. Press them with your thumb or put a known weight on them, measure how far they squash and keep the one that works. Each block takes a few minutes and all four less than an hour: far less than reprinting a six-hour case. The method is in Test coupons. Record the winning profile next to the model (walls, infill, pattern and grade).

See also

Design it in KapyCAD

Draw the part with these clearances and walls, and change any dimension later without redrawing it.

Free plan, no card. Runs in your browser, nothing to install.

Open the editor

Still have a question?