kapy academy

Painting and priming

14 min readUpdated Nov 2026

Paint turns a printed part into something that looks like a product, and it forgives nothing: gloss over unsanded layer lines makes them stand out. Most of the work happens before the color goes on: cleaning, leveling and priming. For the designer, paint is also a thickness added to every painted face, and the model has to allow for it. Leveling the layers belongs to Sanding and smoothing; here you start with a part that is already level. Painting with filament and light uses no liquid paint and is outside the scope of this article.

A system of coats, not a can

Every coat in a paint job that lasts is there because the next one would not stick without it. Before you start, remove the support marks and bring the fit faces to size (Support removal and cleanup).

  1. Clean and degrease. Finger grease and traces of glue stick or release agent from the bed make paint pull back into islands and peel later. Wash with soap and water, rinse, let it dry completely and wipe down with isopropyl alcohol. From here on, wear nitrile gloves.
  2. Key the surface. A pass with a gray scuff pad or P400–P600 paper leaves a matt, scratched surface. Those scratches are the key: the primer flows into the grooves and locks on mechanically.
  3. Primer. It grips the plastic, evens out the color and absorbency of the whole part, and shows up the defects you missed.
  4. Color. Two or three thin coats.
  5. Clear coat. It protects the color from rubbing, sets the final finish (matt, satin or gloss) and, outdoors, adds UV resistance.

Bare plastic is a poor base. It is usually too smooth for the color to bite, every material takes paint differently, and the color of the plastic shows through. Primer is formulated to wet and grip plastic; color is formulated to grip primer. Skip the primer and you are asking the color to do a job it was not made for.

Filler primer is a different product: thick and sandable, it fills layer lines; Sanding and smoothing covers how to use it. Even if you use it, the last coat before the color is a normal, thin primer.

The color of the primer matters too. Gray for almost everything. White under yellows, reds and oranges, which cover poorly and come out dull over gray or need many more coats. Black under metallics and dark colors.

sanded plastic≈10–50 µm per coatclear coatcolorprimerkey≈0.10–0.25 mmthin on the edgepools in the corner
A paint system in section: key, primer, color and clear coat; each spray coat adds a few tens of microns and the whole stack one or two tenths of a millimeter per face.

Chemical compatibility: strong solvent underneath

Water-based acrylic can go over almost any paint that has dried. A strong solvent, such as the one in a nitrocellulose lacquer or a two-component (2K) paint, attacks a weaker paint underneath it, such as a synthetic enamel or an acrylic: it softens it, lifts it and wrinkles it. The safe order is the strong-solvent paint underneath and the milder one on top. The other way round is risky even when the lower coat has cured: an enamel cures in 5–7 days according to its datasheet, but can take weeks to withstand the solvent of a lacquer. Do not mix systems: stay within one range, or test the combination first on a scrap part.

The same goes for the plastic. The strong solvents in lacquers can soften ABS and ASA; it is the same chemistry that smooths them in Vapor and chemical smoothing. A vapor-smoothed part must be free of solvent before you paint it.

Adhesion depends on the plastic

For paint to stick, the liquid has to wet the surface: spread into a film that touches the plastic at molecular scale. On low surface energy plastics such as PP and PE, paint beads up like water on a non-stick pan and never makes that contact. The fix is an adhesion promoter: a very thin chemical bonding layer, not a thicker primer.

Painting by material
Material What happens Preparation
PLA (silk and matte too) Paints well Clean, key (silk thoroughly, as it is smoother), any plastic primer
PETG, PCTG Smooth, solvent-resistant surface: primer grips poorly Key thoroughly, adhesion promoter or a dedicated plastic primer
ABS, ASA The easiest: primer takes without trouble Beware strong-solvent lacquers
PA (nylon) Absorbs water and flexes Dry the part first, flexible primer, expect weaker adhesion
PP, PE Low surface energy: almost nothing sticks PP-specific promoter; the bond stays fragile. See Polypropylene
TPU Flexes and cracks rigid paint Flexible paint, or leave it unpainted
Fiber-filled (CF, GF) Fibers stick out of the surface Prime first to bury the fiber
Resin (SLA, MSLA) If the surface is not cured, it stays tacky under the paint Full post-cure before priming. See Washing and curing resin parts

The design consequence: if a part needs a durable painted finish, choose a material that takes paint from the start.

Laying down the coats

Thin coats, never one heavy one. A thin coat gives off its solvent evenly and pulls tight as it dries. A heavy one sags, orange-peels and traps solvent that leaves it soft for days. The first is the tack coat: a light mist, almost transparent, that the following coats grip.

With a rattle can:

  • Shake the can for 1–2 minutes once the ball starts to rattle.
  • Spray from about 20–30 cm, or the distance on the label.
  • Start spraying off the part, pass over it and release past the far edge. That way the spatter the valve throws as it starts and stops lands off the part.
  • Overlap each pass by half.
  • Put the part on a stand or turntable and turn it rather than walking round it.
  • In a cold room, warm the can in lukewarm water below 40 °C: an overheated can may burst.

Work at around 20 °C and moderate humidity. Cold and damp blush the clear coat milky and lengthen the cure. Data sheets quote times at 21 °C and 50 % relative humidity; colder than that, everything takes longer.

Do not speed up drying with heat. PLA softens under light load at around 57 °C (HDT at 0.45 MPa), so keep it below about 50 °C: a thin wall in a warm oven or next to a radiator can warp. PETG (69–71 °C) and ABS (87 °C) give more margin, but the drying time is set by the paint, not by what the part can stand.

Times for a DIY spray enamel (for example Rust-Oleum Painter's Touch 2X, at 21 °C and 50 % RH)
Stage Time
Touch dry 20 min
Handle 1 h
Recoat (per the label) within 1 h or after 48 h

These figures are for one product, but almost every enamel follows the same pattern: there is a recoat window. Put another coat on while the previous one is half cured and the fresh solvent softens and wrinkles it. Water-based acrylics can be recoated after anything from a few minutes to an hour.

Dry is not cured. A touch-dry film no longer marks, but it is still soft inside. A synthetic enamel usually takes several days to cure fully (in the order of 5–7, per the data sheet); a water-based acrylic, a few hours to a day. Mask over it, assemble or stack before the full cure and the tape pulls the paint off or the parts stick together. Before the clear coat, let the color cure as long as the data sheet says.

You do not need to sand between coats. A light pass with P800–P1000 is only for knocking down a dust nib; respecting the window and the cure matters more.

For small parts, gradients and miniatures, an airbrush with thinned acrylics lays thinner coats than a rattle can. The brush is for details and for resin miniatures over a sprayed primer. As of late 2026, ranges such as Vallejo, Citadel, Tamiya, AK and Mr. Hobby cover both uses.

Printed part on a turntable stand being primed, with one fit face covered in masking tape (generated illustration)
Printed part on a turntable stand being primed, with one fit face covered in masking tape (generated illustration)

Masking

Mask everything that has to stay to size or unpainted: fit faces, bearing seats, threads, heat-set insert bores, snap-fits, electrical contacts and the faces you are going to glue, because paint between the adhesive and the plastic would be the weak link. Joints are glued and filled before priming (Gluing and welding printed parts).

  • Masking tape, low-tack, washi or modeling type. Run a fingernail along the edge so paint cannot creep under.
  • Liquid mask for awkward shapes.
  • In holes, a foam plug or a cocktail stick. A screw threaded into an insert protects it and doubles as a handle.

Put the tape on over a coat that has already cured and pull it when the coat you last sprayed is touch-dry but not yet cured, folded back on itself and at a low angle. That leaves a clean edge; once the film has hardened, the tape takes chunks with it.

On a two-color part you can also mask one color to paint the other. If the colors follow the geometry, it is usually less work to print them in color in the first place: Designing for multicolor covers that, and Four ways to print in color the alternatives.

Paint has thickness: budget for it in the model

According to manufacturers' data sheets, one spray coat leaves a dry film of 25 to 50 µm. In Rust-Oleum's automotive range, for example, the primer leaves 25–50 µm per coat, and the filler primer and color 25–37 µm. A spray clear coat leaves around 10–30 µm. With an airbrush and thinned acrylics, each coat is thinner.

Add up a typical system: two coats of primer (50–100 µm), two of color (50–75 µm) and two of clear (20–60 µm). That comes to about 0.12–0.24 mm. Rounded, 0.10–0.25 mm per face. If you leave filler primer on, add its thickness, which is greater.

That thickness builds up on both walls of any gap. A slot painted on both walls narrows by twice the thickness of the system. A pin painted all round grows in diameter by twice that thickness.

unpaintedslot paintedtongue painted too0.20 mm per side0.05 mm: rubsinterference: will not go in0.15 mm of paint
Paint grows on both walls: at 0.15 mm per face, a sliding-fit slot loses 0.30 of its 0.40 mm of clearance; paint the tongue as well and the clearance becomes interference.

An example: on a modern bedslinger, a sliding fit has 0.20 mm per side, 0.40 mm in total. With 0.15 mm of paint on each wall of the slot you are left with 0.10 mm, and the tongue rubs. Paint the tongue too and you add another 0.30 mm: the clearance turns into interference and the part no longer goes in.

The thickness is not even, either. On a sharp convex edge, surface tension draws the liquid away: the film is thin there and it is the first place to chip. In inside corners and small holes it pools. Small text and fine relief fill in. A fillet or chamfer on visible edges holds the paint better.

What to do, in order:

  1. Do not paint the fits. Mask them and leave them at their printed size.
  2. If a fit face has to be painted, increase the clearance by the thickness of the system for each painted face, measured on a painted coupon. In KapyCAD, move only those faces with "Offset faces" using a negative value, for example −0.15 mm on top of the clearance they already have (Offset Body and Offset Faces). Do not touch the FIT_SLIDE constant: it is your printer's calibration, and changing it would open every sliding fit in the design, painted or not.
  3. Never paint the contact face of a press fit or a snap-fit. A couple of tenths of a millimeter too much ruins either.

Designing fits is covered in Real printed clearances and Choosing the fit: clearance, transition, interference. If the paint is part of a tolerance chain across several parts, see Assemblies and tolerance stackups.

Do not guess your thickness: measure it. Paint a coupon with your exact system and measure it with calipers before and after (Test coupons).

When it fails

Paint failures: symptom, cause and fix
Symptom Cause Fix
Paint peels in sheets, or the tape lifts it No key, greasy surface, PETG or PP without promoter, or masked before cure Degrease, key, adhesion promoter, wait for the cure
Wrinkles or lifts Recoated outside the recoat window, or strong solvent over mild paint Strip or sand back to sound paint, respect the window, do not mix systems
Sags and runs Coat too heavy or too close Let it cure, sand flat, lighter passes
Orange peel Too far away, heavy coat, or cold can or room Warm the can and the room, correct distance
Clear coat blushed, milky Humidity Warm, dry room; with lacquers, one more light coat sometimes clears it
Craters, fish eyes Silicone or oil on the surface Degrease, sand and repaint
Layer lines show through the paint Surface not leveled Back to Sanding and smoothing with filler primer
The fit seizes after painting Paint on the fit faces Mask, or scrape and open up the clearance
Tacky paint on resin that never cures Uncured resin surface Full post-cure before priming

See also

Design it in KapyCAD

Many of these problems are cheaper to fix in the model than in the slicer: wall thickness, overhangs, the face the part stands on.

Free plan, no card. Runs in your browser, nothing to install.

Open the editor

Still have a question?