kapy academy

Sanding and smoothing

13 min readUpdated Nov 2026

Run a fingernail sideways across a printed wall and you feel one ridge per layer. Sanding takes them off; filler primer buries them. Both change the size of the face they touch, so you plan them in the model, not at the workbench. Here the tools are abrasive paper, filler primer and filler on a part that has already been cleaned up; solvent smoothing (Vapor and chemical smoothing) and coatings (Coatings and epoxy) have their own.

Layer lines: hills and valleys

Each bead leaves the nozzle with a rounded flank and joins the one below through a neck narrower than itself. Cut a vertical wall in section and you see a row of hills with a valley between each pair.

sanding cuts the hills downtarget surfacehillsvalleysfills the valleysfiller primer
A printed wall in section, face up: sanding brings the hills down to the floor of the valleys; filler primer brings the valleys up to the hills.

On a vertical wall at 0.20 mm layers, the valley floor sits a few hundredths below the crest, around 0.02 to 0.04 mm depending on how wide the neck comes out. That is an estimate from the bead shape, not a measurement. Thinner layers give shallower valleys, but they are still there.

Slope matters far more. On a face tilted at an angle α from horizontal, the layers form steps roughly h · cos α deep, measured perpendicular to the face. With h = 0.20 mm that is ≈0.19 mm at 15°, ≈0.14 mm at 45° and ≈0.05 mm at 75°. These are the steps with 0.75, 0.20 and 0.05 mm treads explained in Layer height and line width. A dome or a shallow chamfer needs about six times as much sanding as a vertical wall.

There is one more detail. The slicer cuts each layer through its middle, so on a slope the model surface runs through the middle of each step: half the sawtooth sits above it and half below. Sand down to the bottom of the steps and the face ends up ≈h · cos α / 2 below the model, about 0.1 mm at 15°.

Two printed faces in section, magnified fifty times and turned face up: on the left a vertical wall, on the right a 15° slope, with 0.20 mm layers. A sanding block passes four times over each and takes off, band by band, the orange that stands above the valleys: on the wall, the round flanks of the beads, a few hundredths; on the slope, a tooth almost a whole step deep per layer, and the face ends up below the dashed model surface
At 0.20 mm layers, sanding removes hundredths from a vertical wall; on a 15° slope it removes almost a full step (h · cos α ≈ 0.19 mm), and the face ends up ≈0.1 mm below the model. Section magnified ×50, to scale.

So the goal is to bring the whole face down to the floor of the valleys, or bring the valleys up to the crests. Knock off only the crests and the valleys still cast shadows; the lines come back the moment you paint.

The cheapest sanding is the sanding you never do. Variable layer height on domes (Layer height and line width), ironing on flat top faces (Top surfaces), the seam on a hidden edge (Where the seam goes) and an orientation that keeps the visible face vertical (Orientation and overhangs) save you hours. A fuzzy skin or textured surface is never sanded: leave it as printed (Fuzzy skin and textures).

The grit sequence

Each grit only has to remove the scratches of the one before. A fine grit will not take out a coarse scratch in any reasonable time: it polishes the edges and leaves it there. So never more than double from one grit to the next: P120 to P240, yes; P120 to P400, no.

A grit route for FDM (P scale, FEPA)
Step Grit When
Rough P120–P180 only pronounced steps or filler
First pass on a wall P220–P240 vertical wall at 0.20 mm
Refine P320–P400 removes the roughing scratches; wet from here on. On bare plastic, stop here if filler primer goes on next
Before color P600–P800 final sanding of the primer; P800–P1000 for metallics or gloss
Polish P1000–P2000 + polishing compound bare, glossy finish: best on ABS, ASA or resin; PLA takes it wet and with light pressure

Mind the P. European paper is graded on the P (FEPA) scale; American paper, with no P, on the CAMI scale. They roughly agree up to P240 (CAMI 220) and then diverge: P1500 matches CAMI 800 and P2000 matches CAMI 1000. When a North American video says "600", it means a much finer paper than your P600, closer to P1200.

For the dry, coarse steps, aluminum oxide paper or sanding sponges will do. From P320 on, use silicon carbide wet-and-dry paper. On curves, foam-backed pads.

Wet sanding starts at P320: water with a drop of washing-up liquid. The water carries the swarf away, so the paper keeps cutting instead of clogging, and it cools the surface. Dry the part completely before priming: water that has seeped into the infill through a gap comes out days later and lifts the paint.

Block, fingers and guide coat

A hard sanding block, or paper wrapped round a flat strip of wood or a file, keeps flat faces flat and edges sharp. It rides on the crests and only reaches the valleys once the crests have come down. Fingers do the opposite: they push the paper into the valleys and round over every edge. Fingers and foam are for curves only.

With the first grit you can sand along the layer lines to bring the crests down evenly. From then on, change direction by about 45° with each grit: that way you can tell the previous grit's scratches apart and see when they have gone.

The guide coat tells you when to stop. It is a light mist of primer in a different color or, on bare plastic, a few pencil scribbles. Sand until the color is gone across the whole face: anything still marked is a low spot. Without one you sand by eye and stop too early or too late.

Edges and small details are the first to go. A block crossing an edge cuts it several times faster than the flat face, and raised lettering disappears in two passes. Mask the edges you want to keep sharp, or stop before you reach them.

Power tools have their place: an orbital or detail sander on large faces, a rotary tool only at its lowest speed. PLA softens at around 55–60 °C (HDT 57 °C at 0.45 MPa), and friction at high revs melts and smears it instead of cutting it. For the same reason, do not press hard when sanding by hand.

Every plastic sands differently

  • PLA: sands well if you keep it cool (wet, light pressure, no rush). Scratches turn white. Silk PLA loses its sheen the moment you sand it, because that sheen is the as-printed surface: sand silk only if you are going to paint it.
  • PETG and PCTG: hard and rubbery. They fuzz and clog the paper. Take the high spots down first with a scraper or a deburring tool, and sand wet from P320. Expect a matt, slightly hazy face. If you plan to paint, primer grips poorly on them: key the surface well and apply a plastic adhesion promoter first.
  • ABS and ASA: the most rewarding to sand and polish, and they take vapor smoothing too.
  • Nylon (PA) and TPU: they fuzz and barely sand. Do not plan on a sanded finish with them. A quick pass with a heat gun can lay down the fuzz on PA; TPU stays as printed. PA also absorbs water and swells: if you sand it, do it dry and with a mask; if you sand it wet, dry it in the filament dryer before priming.
  • Carbon- or glass-filled: sanding exposes the fibers, leaves a matt, furry face, and the dust carries short fibers. Leave them as printed or prime them first.
  • Resin: layers are much thinner than in FDM, so the main job is removing support stubs. Sand wet and only after a full cure: dust from under-cured resin can sensitize skin (Washing and curing resin parts).

By late 2026 silk, PCTG and fiber-filled filaments are stock items in any shop; how they sand depends on the base polymer, not the brand.

White scratches on colored PLA or PETG are stress whitening. On a bare part, a quick pass of hot air, keeping the gun moving, brings the color back; linger and thin walls sag. On a part you are going to paint it does not matter: the primer covers it.

Filler primer: bringing the valleys up

Filler primer is a thick, sandable spray primer. The car trade sells it as high-build primer, and the hobby world as surfacer. It builds up more in the valleys than on the crests. Block-sand it and the crests show through bare while the valleys stay filled: you level the face while removing almost no plastic.

Left to right: plastic as printed, half-sanded filler primer left only in the valleys, and the face leveled (generated illustration)
Left to right: plastic as printed, half-sanded filler primer left only in the valleys, and the face leveled (generated illustration)

The cycle is short: two or three light coats, the drying time on the can, sanding at P320–P400 until the crests show, then repeat. Primer that has not dried clogs the paper and tears off in strips. Lines from 0.20 mm layers usually take two or three cycles. The streaks left after sanding act as a guide coat: while you can still see parallel lines, you need another cycle.

Where primer cannot reach, filler takes over: deep steps, the seam between two glued halves, pinholes. Use one-part filler in thin layers: thick ones shrink and crack as they dry. For gaps over 1 mm, a two-part filler. Block-sand it from P180–P240.

Primer and filler add thickness; sanding takes it away. On a cosmetic face they cancel out. On a fit face none of the three belongs. The paint system, masking and what each color coat adds are in Painting and priming.

A sanded part is a smaller part

Sanding to the floor of the valleys lowers the whole face: a few hundredths on a wall at 0.20 mm, up to half a layer below the model on a 15° slope, plus the depth of the coarse grit's scratches. A sanded shaft comes out thinner, a sanded hole larger, a mating face lower.

Never sand a face with a functional dimension: bearing seats, slots, the mating faces of two halves, the hooks of a snap fit. Leave them as printed and mask them while you sand and prime around them. A fit face is scraped to size, as in Support removal and cleanup, not sanded. The fit itself is designed in Real printed clearances.

When a face is both visible and a fit, such as the outside of a box that has to match its lid, model a sanding allowance on that face alone. Sand it to size, checking with callipers as you go: the allowance only gives you margin, because it is the same order as the printer's own error (±0.05–0.15 mm); the callipers set the size.

Allowance for a visible fit face (0.20 mm layers)
Face Allowance Why
Vertical wall ≈0.1 mm valleys of hundredths plus the grit scratches
Shallow slope or dome ≈0.1–0.15 mm the sanded face sits half a step below the model
Fit face none not sanded

Adding 0.2–0.5 mm to every face is wasted sanding: the allowance goes only on visible faces that carry a dimension, and what brings you to size is measuring, not excess. In KapyCAD, apply "Offset faces" with a positive distance to those faces only (Offset Body and Offset Faces).

If the same face has to be both a fit and cosmetic, split it in the model so you can finish one part and protect the other.

When it fails

Symptom, cause and fix
Symptom Cause Fix
Lines show after painting you only knocked the crests down guide coat and another primer cycle
Paper fills with plastic pills frictional heat, or PETG sand wet, less pressure, scraper first
Rounded edges, lettering lost fingers or the block crossed the edge block on flat faces only, tape on the edges
White scratches on a bare part stress whitening finer grit and brief hot air, or prime
Primer peels off in sheets water trapped in the infill, soap or grease, or PETG, PP or PA without adhesion promoter remove anything loose, key, degrease with isopropyl alcohol, promoter on PETG, PP or PA, dry and prime again
Fit too tight or too loose after finishing a fit face was sanded or primed mask the fits; reprint the part or scrape to size
Fuzz that will not go away PA, TPU or fiber-filled stop sanding; prime or leave as printed

See also

Design it in KapyCAD

Many of these problems are cheaper to fix in the model than in the slicer: wall thickness, overhangs, the face the part stands on.

Free plan, no card. Runs in your browser, nothing to install.

Open the editor