Before you slice you choose three things, and every number in the G-code comes from them: the printer profile (the machine), the filament profile (the material on the spool) and the process profile (how you want to print this part). With all three right, dry material and a machine in good order, the defaults already print well; calibration fine-tunes the rest. A value changed in the wrong profile is lost the moment you load another spool or pick another printer.
Why three and not one
Orca and Bambu Studio call them printer, filament and process; PrusaSlicer calls them printer, filament and "Print Settings"; Cura calls them printer, material and print settings. The rest of the vocabulary is in Orca, Bambu Studio, PrusaSlicer and Cura.
Each profile groups settings that change together. The printer hardly changes: you own one or two. The filament changes every time you load another spool. The process changes with every part. With a single profile you would need a copy per combination: 2 printers × 6 filaments × 3 qualities is 36 profiles to maintain. Kept separate, that drops to 2 + 6 + 3 = 11.
The printer profile describes the machine. Bed size and shape, nozzle diameter, the firmware's "G-code flavor", motion limits (maximum speed, acceleration, jerk or junction deviation), the start and end G-code (heating, homing, bed probing, the purge line), the default retraction and how many extruders or filament slots it has. The start G-code is copied into the file verbatim, and every coordinate of the part is laid out from the bed size: a wrong printer profile can send the nozzle off the bed or into it (What a slicer does explains what the G-code carries).
The filament profile describes what the material needs. Nozzle and bed temperatures (first layer and the rest), flow, max volumetric speed, cooling and minimum layer time, density and diameter (for grams and cost), pressure advance, and the retraction and Z-hop overrides. Orca has its own pressure advance field on the filament tab; in PrusaSlicer you write it as M572 in the filament's start G-code. They live here because they change with the spool, not with the part. What flow and max flow are, and how to measure them, is covered in Volumetric flow sets the speed and Flow ratio and max flow tests.
The process profile describes what you want from this print. Layer height, line widths, walls, top and bottom layers, infill, speeds and accelerations per line type, supports, seam, brim, ironing. The quality names in the list ("0.20mm Standard", "0.20mm SPEED", Cura's quality levels and, on UltiMaker printers, intent profiles such as Engineering or Visual) are process profiles. Bambu Studio's "0.20mm Standard" profile for the X1C, for example, asks for 200 mm/s on the outer wall, 300 on inner walls and 270 on infill.
The speed in the process profile is a ceiling, and the printer does not always reach it. The real ceiling is the hotend's flow, which the filament profile sets as its max volumetric speed: speed = flow / (line width × layer height) (Volumetric flow sets the speed). Acceleration has its own ceiling, the printer's motion limits. A fast process with a cautious filament profile prints at the filament's pace.
When two profiles set the same value
Some values appear in more than one profile. In Orca, Bambu Studio and PrusaSlicer, retraction and Z-hop sit in the printer profile, and the filament profile can override them: "Setting Overrides" in Orca and Bambu Studio, the "Filament Overrides" tab in PrusaSlicer. If the override is ticked, the filament's value wins; if not, the printer's. It exists because TPU needs a different retraction from PLA on the same machine.
Above the profiles sit two more layers. One holds the values you set on the plate for a single object: per-object settings and modifiers (Modifiers by region and height). The other holds the unsaved changes in the open project. The order, strongest to weakest: object or modifier, your unsaved change, user profile and, at the bottom, the system profile it inherits from.
Cura works the same way, with more layers and different names. It is a stack in which the highest layer that defines a setting wins: your current changes (the values with the reset arrow), the custom profile you saved, quality and intent, material, nozzle variant and, at the bottom, the printer definition. Cura has no pressure advance field and no per-material start G-code: a K value written into the start G-code ("Machine Settings") follows the printer, not the spool, and you have to change it by hand when you switch material.
The working rule is to change each value in the profile the cause belongs to. Stringing with only one filament: filament profile, as an override. An uneven first layer with any material: printer or calibration. Walls too thin for this part: process.
System profiles: start with the manufacturer's
System profiles are the ones the slicer ships with. They are written and tested by the printer manufacturer or the slicer's contributors, one per printer, nozzle and filament. In Orca and Bambu Studio they appear as "System presets"; in PrusaSlicer, with a padlock. They are read-only: you can change a value on screen, but you cannot save over them. They update automatically: PrusaSlicer and Bambu Studio download profile updates, and Orca ships them with each release.
Start with them because the manufacturer's printer profile carries the start G-code, the real motion limits and the flow limits measured on that hotend. On closed-ecosystem machines it is usually the only correct source (Closed and open ecosystems). In the first-run wizard ("Configuration Wizard" in PrusaSlicer, printer selection in Orca and Bambu Studio, "Add printer" in Cura) choose the exact model and nozzle. With a "similar" model, the bed, the start G-code or the limits will be wrong.
Filament profiles come in two kinds: branded (Bambu PLA Basic, Prusament PETG, Polymaker…) and generic ("Generic PLA", "Generic PETG"). For a spool of another brand of the same type, the generic profile is a safe starting point; another manufacturer's branded profile is no better than the generic one. Some filament switchers read the RFID tag on their own brand's spools: all of Bambu's AMS units (the AMS lite included), Creality's CFS and Elegoo's CANVAS, among others. They fill in the slot's type and color, and the slicer loads the branded profile when you sync with the switcher.
If your printer is not in your slicer's list, look in Orca first: it ships system profiles for most brands. If it is not there either, start from the profile of a printer with the same kinematics and the same firmware, and copy the bed size, nozzle, limits and start G-code from the manufacturer's documentation. A profile downloaded from a forum describes someone else's machine and spool: use it to read values from, not as a starting point.
Your own profiles: save the difference
When you change a value, the profile name shows it has been modified (an asterisk, or "(modified)" in PrusaSlicer) and the value is flagged, with an arrow to return to the system value. Nothing has been saved yet. Click the save icon next to the profile name and give it a new name: that is a user profile ("User presets" in Orca and Bambu Studio). In Cura, you create a custom profile with "Create profile from current settings/overrides".
In Orca, Bambu Studio and PrusaSlicer, a user profile inherits from the system profile it came from and stores only the values you changed. When the manufacturer improves the system profile, everything you left alone improves with it. The price is that an update can move a value you took as fixed, and the same user profile will slice differently. Cura's custom profile also stores only the changes on top of a quality profile.
In PrusaSlicer and Orca, "Detach from system preset" turns the profile into a full copy that no update touches. Use it for a profile you have validated for production parts; leave the rest inheriting.
Give it a name that says what it holds, not the date: printer, nozzle, material brand and type, and what you have tuned. For example, "P1S 0.4 · eSUN PETG · dried" or "0.20 thick walls". A user filament profile stays tied to the printers you created it for (compatible printers, in Orca and Bambu Studio). For another printer or another nozzle, create it again; do not force it by ticking it as compatible.
If you switch to another profile with unsaved changes, Orca, Bambu Studio and PrusaSlicer offer three buttons: Transfer (carry the edited values over to the new profile, unsaved), Discard or Save. Cura asks "Discard or Keep changes". "Transfer" is the one that bites: the new profile is flagged as modified, and if you close or switch again without saving, those values are lost or travel to yet another profile. If you ticked the box asking it to remember your choice, the dialog box stops appearing; turn it back on in the preferences.
In Orca, Bambu Studio and PrusaSlicer, a 3MF project stores the profiles it was sliced with, and on opening it the slicer may offer to load them or keep yours (STL, 3MF or STEP for the slicer).
Where each calibration goes
Every calibration yields a number that belongs to a profile. Flow, max volumetric speed, pressure advance, temperature and retraction go in the filament profile, retraction as an override. Motion limits and resonance compensation belong to the printer or the firmware. Write each number into the right user profile and save it: a calibration written into the process profile carries over to the next spool, whether or not it suits it. Which tests to run is in What to calibrate, and in what order.
Some values live outside the slicer. In Klipper, pressure advance and resonance compensation usually sit in the printer configuration, and a single pressure_advance there applies to every material. To make it follow the spool, use the pressure advance field in Orca's filament profile, which emits SET_PRESSURE_ADVANCE with the Klipper G-code flavor, or write that command in the filament's start G-code in PrusaSlicer. Bambu printers store the result of the flow dynamics calibration on the printer itself, per filament and nozzle, and the slicer picks it up. If the slicer and the printer set the same value, whichever comes last in the G-code wins: check the start G-code (Pressure advance and clean corners, Firmware: Marlin, Klipper and closed systems).
The motion limits in the printer profile can be written into the G-code or used only to estimate time. In PrusaSlicer, "How to apply limits" offers "Emit to G-code", "Use for time estimate" and "Ignore"; Orca has a single tick box, "Emit limits to G-code", and with it unticked they serve only for the estimate. Emit them lower than the firmware's and you slow the machine down. Emit them higher and, on Marlin, you raise them above what the manufacturer considered safe. Leave them out and a mismatch only throws off the time estimate.
A worn or replaced nozzle, a new hotend or a different spool of the "same" filament changes these numbers. Treat each profile as a dated calibration record (When your numbers drift).
How not to lose your profiles
User profiles are files in the slicer's configuration folder. To open it: Help › Show Configuration Folder in PrusaSlicer, Orca and Cura. PrusaSlicer stores INI files per type; Orca and Bambu Studio, JSON per type in a user folder; Cura, .inst.cfg files in a folder per version. Copying that folder is the crudest backup, but a complete one.
To export:
- Orca and Bambu Studio:
File › Export › Export Preset Bundle. You pick printer, filament and process profiles and they are saved into a single file; you bring it back with "Import Configs". - PrusaSlicer:
File › Export › Export Config Bundle. The "Export Config Bundle With Physical Printers" variant adds the physical printers: a printer profile plus the address and key you send jobs to it with. - Cura: in
Preferences › Profiles, "Export" saves the print profile as a.curaprofile.
Export a bundle after every calibration session and before every major slicer update.
PrusaSlicer takes a configuration snapshot before every automatic profile update, and also when you ask for one with Configuration › Take Configuration Snapshot. To roll back, pick one in "Configuration Snapshots" and click "Activate". Use it when a profile update changes your results.
As of late 2026, Bambu Studio syncs user profiles to your Bambu account when you sign in, and once you pass the account's profile limit, new ones stay local only. Recent versions of Orca sync to their own account, not Bambu's; when you sign in they copy your local profiles into that account's folder. When Orca and Bambu Studio shared an account, some users lost profiles or found them overwritten. Export a bundle before you turn on any sync.
A bundle from the Slic3r family will not open in Cura, and vice versa. Within the family, import only partly works. The safe route is to recreate the profile in the target slicer starting from its own system profile and copy across only what you changed. You already have that list: it is the modified-values view.
When it fails
| Symptom | Cause | Fix |
|---|---|---|
| A value you changed is gone the next day or after a spool change | You did not save the profile, or saved it in the process profile when it belonged to the filament | Change it in the profile it belongs to, save it as a user profile and check that the name no longer shows the asterisk |
| The printer profile's retraction does nothing with one filament | The filament profile overrides it | Untick the override or change the value in the filament profile |
| The same user profile prints differently after a slicer update | It inherits from a system profile that changed | Compare against the modified-values view; detach validated profiles from the system; roll back with a snapshot (PrusaSlicer) or reimport your bundle |
| Your filament profile is missing from the list | You created it for another printer or another nozzle | Create it again for this printer and nozzle from its system or generic filament |
| Your changes have vanished, or turn up in a profile you never touched | Transfer carried unsaved values to the new profile and you then closed or switched again | Save changes under a name as soon as you make them; turn the dialog box back on in the preferences if you silenced it |
| Profiles are gone after a reinstall, a new computer or turning on sync | They lived only in the old folder, or sync overwrote them | Restore the exported bundle or the copied folder; export after every calibration |
| You set 300 mm/s and the printer never goes past about 230 | The filament's max volumetric speed caps it | Raise it only after a max flow test, in the filament profile |
| The nozzle crashes, the part lands off the bed or the start temperatures are not what you expected | G-code sliced with another printer's profile or with the start G-code of a downloaded profile | Slice again with the system profile for your exact printer |
| You change material on Klipper or Cura and the corners get worse | Pressure advance is fixed in the printer or in its start G-code | Move it to the filament profile (Orca, PrusaSlicer) or change it by hand with each material |
See also
- What a slicer does: where these values end up in the G-code.
- Orca, Bambu Studio, PrusaSlicer and Cura: what each slicer calls each setting.
- What to calibrate, and in what order: the numbers your filament profile should carry.
- Modifiers by region and height: changing one object without touching the profile.