kapy academy

Top surfaces

16 min readUpdated Nov 2026

The top face is the one people look at and touch, and the only one no later layer covers. For a closed, even top face with any current profile, use ≈1 mm of top layers over at least 15 % infill, a monotonic pattern, a single wall on top, lower acceleration on the top layer and a calibrated flow. Ironing adds a pass that makes a flat face genuinely smooth, at a heavy cost in time. Thickness and infill are covered in Walls, perimeters and infill.

How a top face is built

A top surface is any area of a layer with nothing printed directly above it. That is the roof of the part, but also every step, every ledge, the top of a boss and the face of every raised letter. The slicer finds them by comparing each layer with the next. The layers immediately below those areas become solid infill, and the last one gets the top surface line type, with its own pattern, width, flow and speed. You can see them in the preview colored by line type (What a slicer does).

From the bottom up: first the infill, which is mostly air inside. On top of it, the first solid layer, which spans the infill cells: that is the internal bridge, and its settings are in Overhang and bridge settings. Then more solid layers, each now resting on plastic and correcting the sag of the one below. Last, the top layer. What closes the cells is thickness, not the layer count: ≈1 mm with a 0.4 mm nozzle. Bambu Studio's 0.20 Standard profile uses 5 layers (1.0 mm); PrusaSlicer's MK4S profile uses 5 layers with a 0.7 mm minimum. The full table is in Walls, perimeters and infill.

Every layer in between disappears under the next, so only the top layer decides the finish. Beads laid side by side leave a texture of ridges and valleys: one valley per line, at a pitch of ≈0.42–0.45 mm. Light reflects off those ridges. That is why the direction and order of the lines matter, as well as whether the face is flat.

The top layer pattern

Rectilinear (zigzag)different sheenholeMonotonictravel over the holeinner wall ringsSingle wall on topfill reaches the outer walloverlap side
With zigzag rectilinear lines, a hole splits the face into two islands and the slicer fills each one in a different direction: the bead leans on its neighbor from different sides, and each island reflects light differently. With monotonic ordering, every line advances in the same direction across the whole face, even if that means traveling over the hole. With a single wall on top, the top layer fill reaches the outer wall and the inner rings disappear.

With zigzag rectilinear lines, when a hole, a boss or some text splits the face, the slicer fills the islands one at a time and the line direction changes between them. Each new bead presses against its neighbor on one side. Where that side flips, the ridge leans the other way and the area reflects light differently. The result: a flat face with patches of different sheen.

Monotonic ordering prints every line with its neighbor already laid on the same side, across the whole surface, even when that costs extra travel moves: a few seconds on a large face. The overlap is the same everywhere and the sheen comes out even. Monotonic lines are the same ordering with separate lines, without the short turns that join them at the ends, so the edge next to the wall does not get a double dose of plastic at every turn; according to Prusa, it avoids overlapping the perimeter. It is called "Monotonic line" in Orca and Bambu Studio and "Monotonic lines" in PrusaSlicer. As of late 2026 it is the default top pattern in Orca, in Bambu Studio and in PrusaSlicer's MK4S and CORE One profiles.

Cura uses "Lines", and its monotonic ordering needs one more step. "Monotonic Top Surface Order" is on by default, but it only acts on "Top Surface Skin Layers", which defaults to 0. Set it to 1 or more so the last layer gets ordered. At 0, "Monotonic Top/Bottom Order" takes over, and that one is off by default.

The concentric pattern follows the outline. It works on round faces, such as a lid or a knob, where straight lines would end in lots of short runs against the curve. On large faces it works less well: the center fills with tiny loops and gaps. "Hilbert curve", "Archimedean chords" and "Octagram spiral" are decorative textures: they make the layer longer without improving the finish.

The default line angle, usually 45°, runs the lines diagonally across a rectangular part. On a narrow face, rotate it so the lines run along the long side: you save hundreds of short lines and their turns.

A single wall on the top face

On top layers, the slicer keeps only the outer wall and gives the inner walls' space to the top pattern. In Orca it is called "Only one wall on top surfaces"; in Bambu Studio the same setting offers "Top surfaces" or "Topmost surface"; in PrusaSlicer it is "Single perimeter on top surfaces". Bambu Studio's profiles turn it on for every top face. PrusaSlicer leaves it at "Disabled". Orca ships with it off by default, but its profiles for Bambu printers turn it on.

On a top face, inner walls show as concentric rings with a texture unlike the rest of the layer. And the joint between the last inner wall and the top layer fill is where a gap or a ridge appears. With a single wall, that fill reaches almost to the edge and the face has one continuous texture.

The rule has a width threshold. A narrow top area would end up as one wall and a thin strip of fill, so below a certain width it does not apply. In Orca it is "One wall threshold", 300 % of the inner wall width by default. Bambu Studio applies an internal 200 % threshold that does not appear in the normal interface. Orca warns that this setting can leave defects under fine details on the next layer, such as lettering: if raised text comes out with flaws at its base, set "One wall threshold" to 0.

A lid or a plate loaded in bending relies on its top skin rather than its walls, so you lose nothing there. If the face will be sanded or has to be watertight, keep all the walls.

Flow, width and speed on the top layer

Flow comes first. An over-extruded top layer leaves raised ridges, and the nozzle drags through them: you can hear it scraping the face, and a mark is left at the end of every line. An under-extruded one leaves grooves between lines. Calibrate the flow ratio before touching anything else. The flow test in Orca and Bambu Studio is judged by exactly that: how smooth the top face comes out (Flow ratio and max flow tests).

"Top surface flow ratio" (Orca and Bambu Studio, 1.0 by default) adjusts only the top layer. In Cura, "Top Surface Skin Flow" does the same, but only when "Top Surface Skin Layers" is 1 or more. Use it after calibrating, in small steps: start between 0.97 and 1.0. Lowering it to hide a badly calibrated global flow leaves every solid layer underneath uncorrected.

On width, with a 0.4 mm nozzle, Bambu Studio uses 0.42 mm for both the top layer and solid infill. PrusaSlicer's MK4S profiles set the top line to 0.42 mm, narrower than the 0.45 mm solid infill line: the ridge pitch is finer and the texture smoother.

The top layer runs at lower acceleration than the infill. Every line ends in a stop and a restart, and nozzle pressure lags behind the motion. With less acceleration, pressure swings less, the bead comes out at an even width, corners do not bulge and edges show no ringing. On the X1C, Bambu Studio's 0.20 Standard profile prints the top face at 200 mm/s with 2,000 mm/s², against 10,000 mm/s² overall; PrusaSlicer's "0.20mm SPEED" for the CORE One, at 100 mm/s with 2,000 mm/s². The full table and the reasoning behind it are in Speed and cooling. Cura also lets you slow the outer wall on the top face ("Top Surface Outer Wall Speed").

Small faces, such as the tip of a pin or a boss, are another story: there, minimum layer time and cooling decide the finish. If a small top face comes out soft and sunken, the problem is heat (Speed and cooling).

Ironing

same height as the top layerline width ≈0.42 mmtravel direction10 % flowflat nozzle facefilled valleysunironed ridgestop layer: lines at 0.42 mmironing: passes at 0.1 mmfour times as many lines
Ironing goes back over the top layer at the same height: the hot, flat face of the nozzle presses the ridges into the valleys, and a trickle of plastic, about 10 % of normal flow, fills what is missing. To cover the face, the passes are 0.1 mm apart: four times as many lines as the top layer, at a fraction of its speed.

Once the top layer is printed, the nozzle goes back over the same area, at the same height, barely extruding: that is ironing. The hot, flat face around the nozzle orifice melts the tips of the ridges and pushes that plastic into the valleys; the little new plastic fills whatever is left. Only the nozzle face touches the ridges: it does not remelt the whole layer or heat the part. The result is a flat, glossier face on which the lines barely show.

Two identical PLA plates: the one on the left with the top layer lines visible, the one on the right ironed and smooth
Two identical PLA plates: the one on the left with the top layer lines visible, the one on the right ironed and smooth
Ironing: defaults
Slicer Flow Spacing Speed On by default
Orca (generic profiles) 10 % 0.1 mm 20 mm/s no
Bambu Studio (profiles) 10 % 0.15 mm 30 mm/s no
PrusaSlicer 15 % 0.1 mm 15 mm/s no
Cura 10 % 0.1 mm 20 mm/s no

Orca with a Bambu printer profile inherits the Bambu Studio row. In Orca you turn it on by setting "Ironing type" to anything other than "No ironing"; in PrusaSlicer, with "Enable ironing", and in Cura, with "Enable Ironing". What you actually decide is which faces to iron: only the roof of the part ("Topmost surface only" in Orca) or every step and every ledge ("All top surfaces"). Ironing every solid layer is rarely worth the time.

Too much ironing flow leaves a ridge at the end of every pass and the face comes out matt and wavy. Too little and the original lines still show. Too much spacing leaves stripes. Orca and Bambu Studio also have "Ironing fan speed" in the filament profile (−1 disables it): turning the fan down keeps such a low flow from cooling in the tip and clogging it.

What it costs is time. A 50 × 50 mm face is 2,500 mm². With lines at 0.42 mm (Bambu Studio's width), that is 2,500 / 0.42 ≈ 6,000 mm of top line: at 200 mm/s, with the braking at the end of every line at 2,000 mm/s², under a minute (about 45 s). Ironed with passes 0.1 mm apart, it is 2,500 / 0.1 = 25,000 mm: at 20 mm/s, 1,250 s, about 21 minutes. With Bambu's values (0.15 mm at 30 mm/s) it is about 9 minutes. Ironing a single face adds as much time as printing a small part; "All top surfaces" on a stepped part multiplies it.

It works on large, flat PLA top faces: lids, name plates, panels, the front of a sign. It does not work on curved or sloped faces, which print as steps: every step is a narrow strip of top surface, the slicer irons each flat strip and the steps stay. That is what variable layer height is for (Layer height and line width). It is no use on tiny faces or raised text either, because it irons the face of every letter and can round off its edges. PETG and TPU stick to the nozzle and then drop onto the face as blobs. On matt PLA, the ironed area comes out glossy. On multicolor parts, it can smear one color onto its neighbor along the boundary between them (Painting with filament and light).

Ironing does not fix holes and bumps over the infill, or a badly calibrated flow: it polishes a closed face, it does not close an open one. Sort that out first.

Holes and bumps over the infill (pillowing)

When the top face fails to close, holes and bumps appear over the infill cells (pillowing). The mechanism is explained with a drawing in Walls, perimeters and infill. It has no single cause. Check these five, in this order:

  1. Top thickness too low for the layer height: with thin layers, you need more layers to reach the same ≈1 mm.
  2. Cells too large: infill below ≈15 %, or large-cell patterns such as Lightning or a sparse gyroid, need more thickness on top.
  3. The internal bridge sags or breaks: it is the first solid layer over the infill, and its thickness, flow and fan are in Overhang and bridge settings.
  4. Too little cooling on the top layers: PETG with the fan at 30–60 %, or a hot chamber, let each layer sag further.
  5. Under-extrusion: wet filament, or a top layer that exceeds the hotend's maximum flow (Volumetric flow sets the speed).

Fix it in the same order. Raise the thickness first: it is the cheapest change and introduces no new faults. Then the infill density, or a band of denser infill right under the roof with a height modifier (Modifiers by region and height). Then the internal bridge and cooling. Flow last.

Travel scratches and dots

When the nozzle travels over a freshly printed top face, it can scratch it or leave a dot of oozed plastic. Two settings prevent it. The first is Z hop: the nozzle lifts before it travels. It only needs to lift over top faces ("Top Only" in Orca), and you lose no time elsewhere. The second is "Avoid crossing walls" in Orca ("Avoid crossing wall" in Bambu Studio, "Avoid crossing perimeters" in PrusaSlicer): travel moves do not cross walls and stay inside the part. Strings and blobs in general are covered in Stringing and blobs.

If the edge of a face lifts, the nozzle hits it too. That is not a top surface problem: it is an overhang curling upwards (Overhang and bridge settings).

Designing with the top face in mind

Choose which face goes on top. The bed face is the flattest and copies the texture of the plate. Apart from it, only the top face can come out genuinely flat and even. Put the visible face, or the one that mates with another part, on top or on the bed; never on supports (The face on the bed).

Model a face horizontal or with a clear slope. A face 0.5° off horizontal prints as a few wide steps with visible edges. A dome or a gentle slope shows contour lines; variable layer height smooths them (Layer height and line width), and toolpaths that follow the slope in Z are covered in Advanced toolpaths.

Raised text on a top face needs at least 3 mm character height, 0.5 mm stroke and 0.4 mm of relief (two layers) (Minimum features and text). The letters interrupt the top face beneath them. "Top surface expansion", in recent Orca releases, merges that face under the letters into a single continuous fill and leaves the area around them cleaner; it defaults to 0 (off), and "Top expansion wall margin" keeps it away from the outer wall so it does not leave a shrinkage mark. Engraved text cuts through the top layers: keep the depth within the top skin, or the infill will show at the bottom of the letters.

When it fails

The top face: symptom, cause and fix
Symptom Cause Fix
Holes over the cells Too little top thickness, sparse infill, broken internal bridge Go to ≈1 mm or more; raise infill density; check the internal bridge
Bumps over the cells Sagging internal bridge, too little cooling Tune the internal bridge; more fan on the top layers
The infill pattern shows through a closed face Thickness at the limit: the infill walls print through Add one or two top layers
Rings or a gap next to the edge Inner walls on the top face, flow at the joint Turn on a single wall on top; check the flow
Patches of different sheen, especially around holes Non-monotonic pattern Switch to "Monotonic line"
Scratches across the face Over-extrusion or travel without Z hop Calibrate the flow; turn on Z hop over top faces
A ridge at the end of every ironing pass, matt and wavy face Ironing flow too high Lower it by 2 or 3 points
The lines still show after ironing Ironing flow too low or spacing too wide Raise it by 2 or 3 points; go back to the default spacing

How to test it

Print a 50 × 50 mm square about 3 mm tall with ironing on, and look at it under raking light. Adjust the ironing flow in steps of 2 or 3 points (10 → 12 → 15 %): raise it if the lines show, lower it if a ridge is left at the end of every pass. The same square without ironing checks the top layer flow.

See also

Design it in KapyCAD

Many of these problems are cheaper to fix in the model than in the slicer: wall thickness, overhangs, the face the part stands on.

Free plan, no card. Runs in your browser, nothing to install.

Open the editor