kapy academy

Multi-material failures

21 min readUpdated Nov 2026

Your multicolor print has stopped with an error, or it has finished with colors in the wrong place, dirty transitions or the prime tower on the plate. On a single-nozzle filament switcher, every change is a relay of five or six legs, from the cut to the purge (Filament switchers: AMS, MMU, CFS and ACE), and each leg has a maximum time or distance that sensors watch. The message on the screen names the leg that did not finish in time, not the cause, which is usually one leg earlier or later.

Find the leg that failed

The four-color cube on the Bambu Lab wiki needs 153 changes at 0.20 mm layers. If each change fails once in a hundred, only one in five of those prints reaches the end (0.99^153 ≈ 0.21). That is why old filament, worn tubes and a blunt cutter show up here before anywhere else.

"Failed to pull back" or "Load to extruder failed" tell you where the relay stopped, not why: the cause can be a bad cut upstream, a worn tube in the middle or a tangle on the spool. If the print stopped at the unit, look at the spool and the tube; if it stopped at the toolhead, the cut, the extruder and the hotend; if it finished with dirty transitions, the purge or the ooze.

diagram
First, whether the print stopped or finished badly; then, at which leg. Each end box points to the article or section that covers that failure.
spoolsfeedermerge point123bufferPTFE tubeloadunload4sensorextrudercutterhotend5678wiperpurge chute10prime tower91tangle, end still clipped, cardboard slipping2gear chewing the filament, soft filament wrapped up3broken piece blocking every slot4groove or kink in the tube5load not detected6blunt cutter, lever that does not return7clog, heat creep, mushroomed end8ooze, purge stuck to the nozzle9blob on the tower, tower knocked over10full chute
Each numbered point is a place where the relay can break. The error comes from the sensor that is waiting, which is not always where the fault is.

Place the message on the path and check three things before you open the machine:

  1. Which slot. Move the spool to another slot. If the failure stays with the original slot, whatever the filament, it is in that slot's feeder or tube. If it travels with the spool, it is in the spool or the filament.
  2. Which direction. A failure pulling the filament out (unload, retraction) points to the cut or the tip: the end left behind cannot get back up the tube. A failure feeding it in (load) points to the path or the extruder.
  3. When. If it fails on the first change, it is usually configuration: the assigned slot, a filament you have never tried in this unit, or a slot material that does not match the one in the slicer (PETG on a PLA profile forms a poor tip and oozes). If it fails after several hours, suspect wear, a tangle deep in the spool, filament that has picked up moisture or a full chute.

Then cancel the print and repeat only the leg that failed: Prusa's MMU3 has a "Loading Test" in its menu, and Bambu Lab machines load and unload each slot from the screen or the slicer. If it fails again, it is mechanical. If it works cold and fails after hours of printing, the difference is the state of the machine: suspect heat creep in a hot toolhead, a cutter lever that stops halfway or a cutter worn out after hundreds of cuts.

On units such as Creality's CFS, Anycubic's ACE or the Qidi Box, the path is the same (spool, buffer, merge point, cutter in the toolhead), and their errors read the same way, leg by leg.

At the spool and in the tube

Tangle or snag on the spool. The unit pulls, the spool does not turn and the load fails, or you get a high-resistance or motor-overload warning. The usual causes are a crossed wrap (common in the last third of the spool or on a badly seated refill), the end still clipped into the hole in the flange or taped down, and an off-center refill rubbing on its housing. Some machines watch for tangles at the toolhead, such as Bambu Lab's A1 series with the AMS lite, but their wiki notes that this check does not work with every filament. On a machine without that check, the extruder runs dry and the part shows the under-extrusion described in Extrusion problems. Untangle it by hand or cut out the crossed section and reload, free the end before the spool runs out and seat refills properly.

Cardboard spools. They shed fiber and slip on the rollers: the rollers turn and the spool does not. Many units struggle with them. Rewind the filament onto a plastic spool or fit a printed adapter ring.

Brittle filament. Old or damp PLA, some silks and several fiber-filled filaments snap at a tight bend in the tube or under the cutter. The broken piece stays in the tube or at the merge point, and every slot that runs through it stops loading. Filament breaks more often in a switcher than on a single spool: the filament goes up and down the same bends hundreds of times, and every trip is a bending test. Pull it out from behind: on Bambu Lab machines, release the tube at the unit's outlet and draw the piece backwards; their wiki has a page for broken filament at any point on the path. Then dry the spool or take it out (Drying and storing filament). If a short length snaps when you bend it by hand, it will snap in the switcher.

Soft filament that buckles. A TPU softer than the unit accepts folds inside the tube and wraps around the feeder gears. No setting fixes it: feed it from an external spool or print it with its own tool on a toolchanger. Bambu Lab does not support generic TPU or TPE in the AMS 2 Pro; its TPU for AMS has a Shore hardness of 68D. More in TPU and flexible filaments.

Worn PTFE tubes. Every change drags the filament through the tube in both directions. At the bends it cuts a groove, friction rises and loads do not finish in time. Abrasives (carbon fiber, glass fiber, glow-in-the-dark) wear them much faster, and Bambu Lab treats the AMS tubes as consumables. The typical symptom is a load that fails now and then on one slot and works on a retry. A tube with a tight bend, or longer than it needs to be, adds the same resistance: Bambu Lab lists both as causes of a tangle alarm with no tangle. Replace the tube; the procedure is in Filament switcher upkeep.

Damp PVA and BVOH. A switcher prints PVA without trouble; what fails is damp PVA, which softens, swells and sticks to the tube. Bambu Lab does not support damp PVA or BVOH in the AMS 2 Pro. Keep them sealed. Recovering damp PVA takes 75–85 °C for 8–12 hours (BVOH, 60–80 °C), in an AMS HT (up to 85 °C) or a separate dryer; the AMS 2 Pro, which tops out at 65 °C, keeps them dry but will not dry them.

End of spool and auto refill. Auto refill only switches to another spool if the unit recognizes it as identical: same material and same color, from its RFID or from what you set for that slot. A slot with another color or another type is no backup, and the print pauses. If the spool runs out with no backup, a half-loaded end is left in the path: pull it out before loading the new spool.

At the toolhead: cutter, tip and extruder

The shapes of the filament end (flat cut, good tip, blob, string) are drawn in Filament switchers: AMS, MMU, CFS and ACE; here is the fault each badly formed end causes.

The cutter does not cut cleanly. A blunt cutter, or a lever that does not travel its full stroke, leaves the filament crushed and only partly severed. When the unit retracts, the two pieces stay attached, or a crushed end snags in the buffer or the tube. The symptom is "Failed to pull back" or a jam in the buffer with a flat, frayed end. Clean the area and replace the cutter if the cut keeps coming out badly: a print with 150 changes is 150 cuts.

The cutter lever does not return. Bambu Lab printers expect the lever to spring back after each cut, and raise an error if it has not returned after two minutes. The causes their wiki gives include a clogged hotend (the filament under the cutter cannot move out and the lever stays loaded), the toolhead fan cable caught on the lever, the lever spring out of place and friction between the cutter and the extruder wall. In that order: look for the clog, check the cable routing, refit the spring and, if it persists, replace the cutter.

The tip comes out badly formed. This is the failure specific to the MMU3 and to cutterless systems. A tip with a blob jams on its way up the tube or in the extruder. A long, thin string snaps off in the selector and fools the sensor; the "FINDA filament stuck" error (#04102) on unload belongs to this family. Tip forming depends on the material, the nozzle temperature and the ramming and cooling moves in the filament profile: PLA forms clean tips; PETG and stringy filaments form far worse ones. Tune that profile's ramming and cooling, drop the unload temperature a few degrees if the profile allows it, and dry the filament.

The load reaches the extruder and stops. The toolhead sensor does not see the filament in time, or the extruder does not grip it. On MMU3 firmware as of late 2026, the errors "Load to extruder failed" (#04108) and #04103, the filament sensor that did not trigger, point first to the calibration of the toolhead filament sensor and then to the extruder's idler lever; recalibrate and run the "Loading Test". On any machine, the same message can come from a cut-off scrap or dirt at the extruder inlet, a worn gear or a tube not fully seated in the toolhead.

The hotend will not take the new filament. A partial clog or heat creep softens the filament above the melt zone. The unload pulls out a fat, mushroom-shaped end, and the next load stops at the heatbreak. On enclosed machines the typical cause is printing PLA, PVA or TPU with the door shut and the bed hot: with those materials, open the door once the bed is above about 45 °C (Enclosures and heated chambers). Clear the clog first (Extrusion problems for heat creep, Nozzle and hotend care for cleaning); the switcher error is only the consequence.

The printer skips a change. If the sensors miss a failed load, or you resume a pause without loading, the printer lays a band of the wrong color or extrudes into thin air until the filament arrives, leaving a gap or a nest of spaghetti on top. On current machines it is rare, but it happens: the sensors detect presence, not color. The nest and what to do about it are in Layer shifts and spaghetti. If you resume after a failed change, check that the right filament has reached the nozzle and purge by hand before you carry on.

Colors that bleed

White part printed on top of a black section: the first white layers above the joint have a gray haze and dark streaks fading upwards; higher up, on the white face, a few loose black specks and a black hair of plastic
White part printed on top of a black section: the first white layers above the joint have a gray haze and dark streaks fading upwards; higher up, on the white face, a few loose black specks and a black hair of plastic

Tell the symptoms apart first: two different causes give similar defects.

  • A gray haze or a streak at the start of the new color, in the first walls after the change and in the same place on every layer with a change: the purge for that color pair is too short. Purge and multicolor waste covers it, along with the shadow that appears when you purge into infill on a part with few walls.
  • A speck, smudge or hair of the old color in random places on the new color: ooze or debris carried by the nozzle, not the purge.

Ooze and strings at the change. After the change, the nozzle travels from the tower or the chute to the part. Residual pressure, plus damp filament, leaves a string or a blob of the purged mix where it rejoins the part. Dry the filament and keep the prime tower: it stabilizes the pressure and wipes the nozzle, and without it the nozzle arrives oozing. Check that filament's retraction too, in Stringing and blobs.

Plastic stuck to the outside of the nozzle. A lump of purge or a string wrapped round the tip carries old color and drops it on the new one, almost always as dark specks on light faces. Machines with a chute wipe the nozzle on a wiper after purging; if the wiper is worn or dirty, it stops cleaning. Clean the outside of the nozzle while hot, check the wiper and the chute (Filament switcher upkeep) and fit a silicone sock on the heater block: plastic does not stick to silicone.

Purge builds up. With the chute full, the next purge stays on the nozzle or drops onto the plate, and the nozzle ends up dragging it across the part. A long multicolor print can fill it: empty it before long jobs.

Two defects that are not the switcher's fault: a dark color showing through a light one with thin walls (too few walls or too little painted depth, Designing for multicolor) and colors with the right shape in the wrong place (wrong slot mapping, Assigning colors in the slicer).

Towers that fall over

Tower design is in Purge and multicolor waste. The tower is fragile by design: tall, narrow, printed fast and with a different filament on almost every layer, and every line starts with a nozzle that may be oozing. A blob from a change or a curled corner sticks up, the nozzle hits it on the next pass and the tower topples or tears off the plate. It is the same collision that causes layer shifts (Layer shifts and spaghetti).

A fallen tower almost always ends the print. The machine keeps purging into thin air, drags strings over to the part, and the debris can build a ball of plastic round the heater block. Cancel early.

The causes, from most to least likely:

  • Poor first-layer adhesion on the tower. Its footprint is smaller than almost any part's. Use a brim and clean the plate.
  • Blobs sticking up. Dry the filament and check the wiper.
  • PETG or TPU curling at the tower's corners under the part-cooling fan. Widen the tower and add a brim.
  • Materials that do not bond to each other. PLA and PETG do not fuse (which is why each is used as a support interface for the other), and a tower that alternates them splits along those layers. Widen the tower or purge the support material into the supports.
  • Bad position. A curled corner of the part or a toolhead travel sweeps it: move it.
  • Rigid material on TPU. Prusa warns that a rigid material printed on top of a few layers of TPU can push them sideways.
  • Speed. On a fast machine, the tower prints faster than a thin column can stand: cap its speed.

With "No sparse layers", the tower only grows on layers with a change, and the nozzle drops to the tower's height on its way there. If the part is taller than the tower along that path, the nozzle hits it. If you see knocks or dragged strings on those layers, turn the option off.

Multi-nozzle machines

Toolchangers, IDEX machines, dual-nozzle heads and hotend swappers do not purge at every change, so they fail differently. Why they ooze on standby and why they drift out of offset is explained in Toolchangers, IDEX and dual nozzles.

  • A blob or string where a tool comes in: standby ooze. The idle tool oozes and the blob arrives with it; on a dual-nozzle head with a flow blocker (such as the H2D), it comes out on the first line when the nozzle drops again. Dry the filament, lower the standby temperature, turn on preheating and keep a small tower or the wiper.
  • A thin, gappy first bead after a change: the tool arrived without pressure after waiting. Prime more, or let the first lines go to the tower.
  • A pause before each change while it waits for temperature: the standby temperature drops too far and there is no preheat. It is not a fault; use the preheat time ("Preheat time" in OrcaSlicer).
  • Color boundary offset from the shape, with a gap on one side and an overlap on the other: the tool's XY offset has changed. If one color comes out squashed or barely stuck to the other, it is the Z offset. Repeat the offset calibration after changing a nozzle or a hotend, after a crash and whenever a boundary looks shifted. A calibrated machine holds a few hundredths (Snapmaker specifies 0.04 mm or less for the U1), so a visible gap is a calibration problem.
  • A tool the head cannot pick up or park: if it does not seat in its dock or on the carriage, the print stops with a coupling error or the machine crashes. The causes: plastic on the dock or the guides (ooze, a string), a tool knocked out of place, or the XY reference lost after a crash. Clean the dock and the contact faces, reseat the tool and repeat the calibration. A hotend swapper (such as the H2C's) that will not couple or release a hotend has this same failure.
  • In IDEX copy mode, one copy sticks and the other does not: the two nozzles do not lay the first layer at the same height; Toolchangers, IDEX and dual nozzles covers it.
  • Each nozzle with its own filament switcher (such as the H2D with two AMS units): the failures in the previous sections apply to each nozzle, and one nozzle cannot use filament from a unit connected to the other. If the slicer asks you to move spools from one unit to the other, this is why (Assigning colors in the slicer).

Cracks and weak layers in long prints

On a filament switcher, the part gets no plastic for much of each change, and a four-color layer needs three changes, because it starts with the color the previous one finished on. Meanwhile the part cools. In PLA the layers still bond. In large ABS, ASA or PC parts, the cooled layer bonds poorly to the next, and shrinkage opens a crack at one particular height. The physics of the bond is in Layers splitting apart, and that of shrinkage in Warping and lifting corners.

At print time you have three ways out: a closed, warm chamber for those materials, fewer layers with several colors (the design levers in Designing for multicolor), or a toolchanger, which changes without purging and leaves the part idle for far less time.

What makes a switcher reliable

Almost everything above is prevented the same way: dry filament, an empty chute before a long job, every slot set to its real material and color (so auto refill and the flush table work), and consumables replaced when the manufacturer says so, because a worn tube, cutter or wiper causes random failures that look like software bugs (Filament switcher upkeep). Before a 20-hour job, test every new brand or material with a short two-color print, especially on units that form a tip, where each filament needs its own tuning.

A camera with failure detection recognizes printing in mid-air and spaghetti, but not a color in the wrong place; Sensors, cameras and failure detection explains why.

When it fails

Multi-material failures: symptom, cause and fix
Symptom Cause Fix
One slot will not feed; motor-overload or tangle alarm Tangle, end clipped to the spool, off-center refill, kinked tube Untangle, free the end, seat the spool, straighten the tube
No slot loads Broken piece in the shared tube or at the merge point Pull it out from behind; dry or remove the spool (Drying and storing filament)
One slot fails now and then and works on a retry Worn or kinked PTFE tube, cardboard spool slipping Replace the tube; adapter ring for cardboard spools (Filament switcher upkeep)
"Failed to pull back", crushed or frayed end Blunt cutter or lever not traveling its full stroke Clean and replace the cutter
Cutter lever does not return Clog under the cutter, cable over the lever, spring out of place, cutter friction Clear the clog, reroute the cable and refit the spring, replace the cutter
Tip with a blob or string; unload jams (cutterless) Tip forming Tune the ramming and cooling, dry the filament
Load stops at the toolhead Sensor calibration, extruder idler lever, dirt, tube not seated Recalibrate, "Loading Test", clean the inlet
Load stops at the hotend; mushroomed end Partial clog, heat creep, door shut with PLA Extrusion problems
A soft TPU never arrives Buckling in the tube External spool or its own tool (TPU and flexible filaments)
Band of the wrong color or printing in mid-air after a change Failed or undetected load Check the loaded filament and purge by hand before resuming (Layer shifts and spaghetti)
Streak or gray haze at the start of each new color Purge too short for that pair Purge and multicolor waste
Loose specks or hairs of the old color Ooze, dirty nozzle exterior, worn wiper, full chute Dry, clean the nozzle, check the wiper, empty the chute, keep the tower
Prime tower topples Blob on the tower, small first-layer footprint, curling, materials that do not bond, bad position Brim, dry filament, wider tower, move it, cancel early
Blob from the parked tool or the incoming one Standby ooze Standby temperature and preheat, dry filament, tower or wiper (Toolchangers, IDEX and dual nozzles)
Color boundary shifted, gap on one side and overlap on the other Tool offset Repeat the offset calibration
Crack at one height in a large multicolor ABS, ASA or PC part The part cools during changes Warm chamber, fewer layers with several colors (Layers splitting apart)

See also

Design it in KapyCAD

Many of these problems are cheaper to fix in the model than in the slicer: wall thickness, overhangs, the face the part stands on.

Free plan, no card. Runs in your browser, nothing to install.

Open the editor

Still have a question?