kapy academy

What a printed part costs

13 min readUpdated Nov 2026

The slicer says "120 g, €2.40" and you take that as the cost of the part. That figure is the material alone, and once you count failures and your minutes at the machine, it stops being the biggest item. The real cost comes from this formula: cost = (material + energy + machine wear) × failure factor + your time. Each section works out one term on the same example: a 120 g PLA bracket, 6 h on an enclosed CoreXY such as a P1S or a CORE One, 0.20 mm layers and a single color.

what the slicer says2.402.40running cost4.012.401.08full cost9.012.401.08materialmachineenergyfailures0.130.40your time5.00the slicer ≈ a quarter0246810€
The same part costed three ways: the slicer's figure is only the base, and once failures and time are added, material is little more than a quarter of the total.

Material: the grams the slicer reports and the ones it misses

It is one multiplication: grams / 1000 × price per kilo. As of late 2026, PLA costs between €15 and €30/kg in Europe. At €20/kg, the bracket's 120 g come to €2.40.

The slicer's grams are reliable because they are the extruded volume times the density (about 1.24 g/cm³ for PLA). They include walls, infill, supports, brim and prime tower, as long as the breakdown picks them up. Check that supports and purge count toward the total instead of sitting on a separate line, where they are easy to miss.

What it misses is the filament that never reaches the plate: the end of the spool the filament switcher cannot feed, the initial purge line, the test prints you run before the good one. A gram of PLA is about 33 cm of 1.75 mm filament, so a couple of leftover meters is already 6 g. A spool is not 1000 g of usable part.

On a single-nozzle filament switcher (AMS, MMU, CFS), the purge often weighs more than the part. A four-color cube at 0.20 mm needs 153 changes and throws away about 83 g: a little over half a gram per change. You pay for those grams in the same way as for the part's. A toolchanger brings this item close to zero: on the CORE One's INDX each change purges about 13 mg. Where those grams come from and how to cut them is covered in Purge and multicolor waste.

Engineering materials push this item up. PETG-CF and PLA-CF cost a little more than PLA; PA, PC, PA-CF and PPA cost two to four times as much per kilo, or more.

Enter the price per kilo once in each filament profile: OrcaSlicer, Bambu Studio and PrusaSlicer all accept it and show the cost next to the grams. Of the five items, it is the only one the slicer works out for you.

Energy: less than you think

Energy = average power in watts × hours / 1000 × price per kWh. What matters is the average. The rating plate sets the ceiling, not the consumption: from about 240–360 W on machines with a 24 V bed to around 1000 W on those that heat the bed at mains voltage, such as the P1S in Europe. The heaters run at full power only while heating up; after that they cycle on and off to hold temperature.

With PLA, a modern desktop printer draws 80 to 120 W on average. Prusa states an average of 80 W for its MK-series bedslingers, and an independent measurement of an enclosed P1S gives about 120 W. While heating up it draws from about 200 W to around 1 kW for a minute or two, depending on the machine; idle, it draws 5 to 15 W.

ABS, ASA and PC use more because the bed runs at 90–120 °C instead of 55–60 °C. According to Prusa, the MK series goes from 80 W with PLA to about 120 W with ABS. On an enclosed CoreXY without a chamber heater, the chamber warms from the bed itself; a machine with an active chamber heater draws considerably more while it is on. The heated bed takes most of the power, not the motors.

The price that matters is that of each extra kWh: the energy charge on your bill, including network charges and taxes, not the whole bill divided by the kWh, because you pay the standing charge even with the printer switched off. In Spain that price runs from about €0.15 to €0.25/kWh depending on tariff and month; check yours. At 110 W and €0.20/kWh: 0.11 kW × 6 h = 0.66 kWh, and 0.66 kWh × €0.20/kWh = €0.13.

For your exact figure, measure a long print with a smart plug that meters power. You will also see the idle draw: many enclosed printers keep using a few watts all night, so unplug yours if it will sit unused for days.

In the example, energy is under 6 % of the material. It only matters on long engineering prints, in a farm or when you dry filament: a dryer drawing a few tens of watts for several hours can use as much as the print itself, and that energy belongs on the bill of the PA or PC parts that need it. When to dry and for how long is in Drying and storing filament.

Machine: depreciation and wear per hour

This item has two parts: depreciation (the purchase price spread over the hours of service life) and consumables: nozzles, plates, PTFE tubes, belts, filters and the odd hotend.

Depreciation per hour is the price divided by the print hours you expect to get out of the machine. A €700 printer over 5000 print hours comes to €0.14/h. But 5000 h is about three years at 4.5 h a day. A hobby machine that prints a few hours a week never gets there, and its hour costs more, not less. Be honest about the hours.

electricitydepreciationconsumableshobby: ~4 h/week for 3 yearsheavy use: ~4.5 h/day for 3 years€700 printer50010002500500000.51.01.5€/hprint hours
The machine's cost per hour falls with the hours you actually print: the printer that barely gets used is the expensive one; electricity stays well below both curves.

For consumables, set a yearly budget and divide it by the same hours you used for depreciation: €60 a year over about 1700 h is about €0.04/h. Abrasive filaments move this item. A 0.4 mm brass nozzle widens noticeably after a few hundred grams of carbon fiber or glow-in-the-dark filament; a hardened steel one lasts kilos, but not for ever. Charge that wear to the parts printed in those filaments, not to everything else. Which nozzle suits each material is in Nozzles: size and material; what to replace and how often, in A maintenance schedule.

In the example: 6 h × (0.14 + 0.04) €/h = €1.08, nearly half the material.

Hours drive both this item and energy. Anything that shortens the print cuts both at once: fewer walls than you add out of habit, less infill where strength allows, thicker layers on hidden parts, an orientation that removes supports. The settings that decide grams and hours are explained in Walls, perimeters and infill.

The failure factor, which makes every good part cost more

A failed print costs the material, energy and hours up to the failure, plus the reprint. Spread over all your prints, it works as a factor: if you lose a fraction f of your prints, real cost = cost / (1 − f). At 10 % failures, ×1.11; at 25 %, ×1.33. With a material or printer you have not mastered yet, a rate in that range is not unusual.

The factor counts each failure as a whole print: it is the worst case. If nearly all your failures happen in the first layers, the real factor is lower. But the real rate is usually higher than people admit. Long prints fail more: more layers and more time for a clog, a lifting corner or a support coming loose. And late failures are the expensive ones, because the hours are already spent. The minutes you spend cleaning up and restarting are not in the factor; add them to your time.

Stop guessing: for a month, log every print, good or failed, and, if it failed, at what height.

Lowering the rate is cheaper than paying for it. Dry filament, a clean first layer and a test part before a batch give the best return; diagnosis is in Reading a failed print. Camera failure detection (the "spaghetti" kind) does not lower the rate, but it stops the print as soon as something goes wrong and makes each failure cheaper; how it works is in Sensors, cameras and failure detection.

In the example: €(2.40 + 0.13 + 1.08) = €3.61; × 1.11 = €4.01.

Your time: nearly always the biggest item

Machine hours are not your hours. Count the minutes you actually spend: slicing and preparing, changing and cleaning the plate, removing supports, finishing, packing. On a small part that is 10 to 30 minutes.

In the example, 15 minutes at €20/h is €5.00, more than everything before it put together. The bracket costs €9.01 in total, and the slicer's €2.40 is little more than a quarter of it.

Even if you print as a hobby, this item helps you decide: when to batch parts, when a finish is worth it, and when ordering the part from a service is cheaper than spending your afternoon on it. That last decision is covered in When to order the part instead.

Batching does not make everything cheaper. Ten brackets on one plate use about ten times the material and nearly ten times the hours: that cost does not fall per part. Preparation does: if the ten take 20 minutes in total, that is 2 minutes a part, €0.67 instead of €5.00. The trade-off: a full plate is riskier, because a part that comes loose can knock over its neighbors, and the failure takes the whole batch. That is why you print one first. How to fill a bed well is in Many parts on one plate.

Design is separate. A custom design is charged once and spread over the units you will make, or you write it off as a hobby. Decide which, and say so; do not hide it inside the price per part.

Pricing a part you sell

Start from the full cost, never from "material × 3" or any other rule of thumb. A multiplier on grams undercharges light parts with long print times and overcharges heavy parts that print fast, because time does not follow weight.

Price = full cost + margin. On top come the costs of selling: platform and payment fees, which are charged on the price and so eat into the margin too; packaging and shipping; and VAT if you are VAT-registered (21 % in Spain). Tax obligations depend on your country and circumstances, and are not covered here.

Most platforms take their fee on what the buyer pays, VAT included. The table works it out that way.

The bracket, priced (margin and fee are examples, not recommendations)
Item Calculation Amount
Full cost (material + energy + machine) × 1.11 + time €9.01
Margin 30 % on cost (your choice) €2.70
What you want to receive (net) 9.01 + 2.70 €11.71
Price excluding VAT 10 % fee on the VAT-inclusive price (use your platform's): 11.71 / (1 − 0.10 × 1.21) €13.32
Price including VAT 13.32 × 1.21 €16.12
Payment fee percentage + fixed per order, depending on your payment provider treat it like the platform fee: divide by (1 − % × 1.21) and add the fixed part
Packaging and shipping separate, depending on the carrier —

Compare the result with a quote from an online print service for the same file and material. If yours comes out well above it, look at your process: the failure rate and the minutes per part. And before you set a price, check the model's license: if it is non-commercial (CC BY-NC, for example), its prints cannot be sold.

The cost sheet: five items and where each figure comes from

For resin the formula holds and the items change: resin by the liter, alcohol or wash fluid, vat film and gloves.

The cost sheet, ready to copy into a spreadsheet
Item Formula Where the figure comes from
Material grams / 1000 × €/kg slicer grams (with purge and supports), the price of your spool
Energy average W × h / 1000 × €/kWh metering plug, energy charge on your bill
Machine h × (price / service hours + consumables/h) purchase price, your real hours, yearly consumables budget
Failures subtotal / (1 − f) your one-month log
Your time minutes / 60 × €/h a stopwatch, at every step

When it fails

Cost per part: symptom, cause and fix
Symptom Cause Fix
Parts cost more than you worked out You trusted the slicer's cost, which is only the material item Work out the other four at least once to see how much they weigh
Energy looks huge on the sheet You took the rating-plate power as consumption Meter a print with a smart plug: expect 80 to 120 W on average with PLA
The machine looks almost free per hour You depreciated it over 10,000 imaginary hours Count the hours you really print in a week and multiply by the years you will keep it
A multicolor job costs double the estimate You forgot the purge Add the purge and prime tower grams to the material; with a filament switcher they often double the bill
The margin vanishes and you cannot see why You count neither failures nor finishing minutes Log a month of prints and time the finishing once

See also

Design it in KapyCAD

Many of these problems are cheaper to fix in the model than in the slicer: wall thickness, overhangs, the face the part stands on.

Free plan, no card. Runs in your browser, nothing to install.

Open the editor

Still have a question?