kapy academy

Gluing and welding printed parts

15 min readUpdated Nov 2026

The part came out in pieces: it did not fit the printer, each half wanted a different orientation, or it broke. Joining it is mostly a materials question: what sticks depends on the plastic, and the joint can never be stronger than the walls it is bonded to. Every joint also needs sanded, clean faces, a planned bond gap, pressure while it sets and a full cure before you load it. This step comes after Support removal and cleanup and before Sanding and smoothing; where to cut and how the halves line up is covered in Splitting large parts.

Glue, dissolve or melt

Adhesive

A third material wets both faces and hardens between them. For that to work, the glue has to wet the plastic, which depends on the plastic's surface energy, and it has to fill the gap. It can also join dissimilar plastics. The bond is only as good as its adhesion to each face.

Solvent welding

A solvent softens both faces, polymer chains from each face tangle into the other, the solvent evaporates and you are left with one continuous piece of the same plastic. It only works if there is a solvent that attacks that plastic and is safe to use at home: in practice, acetone with ABS and ASA. It adds no material and fills no gaps unless you make a slurry.

Heat welding

Heat melts both faces and a filler bead of the same filament, and on cooling you have a single piece, the same way layers fuse during printing. It works on any thermoplastic, including the ones no common adhesive grips (PP, PE, TPU). But it only joins a plastic to itself or to its own family. ABS and ASA share a matrix and weld to each other, with acetone and with heat; PC welds to PC-ABS. PLA does not weld to PETG, which is exactly why each works as a support interface for the other.

In practice, between parts of the same plastic, welding raises no compatibility questions. Between plastics of different families, you are left with an adhesive or a mechanical joint. And if the joint will ever need to come apart, do not glue it: screws, inserts (Designing for heat-set inserts), captive nuts or snap fits (Print-friendly snap fits) hold without glue and come apart again.

Which glue for which plastic

Joining each plastic: first choice, alternative and what fails
Material First choice Alternative What fails
PLA CA Epoxy if there is load or a gap No safe household solvent
PETG / PCTG CA or epoxy on sanded faces Heat welding Acetone barely touches it
ABS / ASA Acetone welding ABS slurry for gaps; CA and epoxy also grip Too much acetone caves in thin walls
PC and blends CA or epoxy Heat welding Its solvents (dichloromethane, DCM) are not for home use; CA and accelerator can crack stressed PC
Nylon (PA) Epoxy or CA on a dry, sanded part Heat welding Damp nylon: the CA cures instantly and the bond line is weak
TPU Heat welding Polyurethane or flexible CA Rigid CA cracks when it flexes
PP / PE Heat welding Polyolefin primer + CA Ordinary CA and epoxy do not grip
Dissimilar plastics Epoxy CA if the gap is minimal Solvent and heat only join the same family (ABS to ASA yes, PLA to PETG no)

Cyanoacrylate

It cures in seconds from the moisture on the surfaces. Thin grades need near-total contact, a gap of 0.15 mm at most; gels reach 0.25 mm. It cures rigid and brittle: good in shear, poor in peel and impact. Accelerator (activator) sets a thick drop instantly but leaves it more brittle.

CA has one defect of its own: blooming, a white haze around the joint. It is monomer that evaporates before curing and settles next to the joint. Avoid it with less glue, ventilation, a low-bloom CA or a touch of activator, which cures it before it can evaporate. On visible faces of ABS, PC or painted surfaces, test the activator on an offcut first: the solvent carrier in some activators marks or cracks these plastics.

Two-part epoxy

It fills gaps, carries load, joins dissimilar materials and is tougher than CA. The resin-to-hardener ratio is set by the manufacturer. "5-minute" epoxies set fast but end up weaker and softer than slow ones. Full strength usually arrives after 24 h at room temperature; check the product datasheet, because the cure takes longer in the cold. Watch the pot life: a large mass heats up as it reacts, and that heat can soften PLA. Mix small batches and keep glue lines thin.

PP and PE

Their surface energy is low: liquids bead up instead of spreading, and a normal glue has nothing to hold on to. A polyolefin primer modifies the surface so CA can wet it. For systems such as Loctite 406 with 770 primer, the manufacturer quotes several N/mm² in shear on primed PP, but does not recommend it for joints loaded in peel. The material itself is covered in Polypropylene.

Preparing the joint

Sand

Take 120 to 240 grit paper over both faces to kill the shine and expose fresh plastic. The face that sat on the build plate, glossy if it was printed on smooth PEI or glass, is the worst one to bond. Sanding gives the adhesive more contact area and a mechanical key.

Clean

Wash glue-stick or release-agent residue off the face that sat on the bed with warm soapy water: it is there precisely so the part lets go (Bed prep for each material), and alcohol will not dissolve it. Dry, blow off the dust, wipe with 90 % or stronger isopropyl alcohol and let it flash off. On PVB, which alcohol attacks, clean with soap and water only. From then on, keep your fingers off the faces.

Design the gap

CA wants near-total contact. Epoxy works best with a gap of about 0.1–0.3 mm: it holds more, but a thick line is weaker and runs hotter as it cures. Solvent welding needs contact. The reasoning behind clearances, and values for pins and pockets, are in Choosing the fit: clearance, transition, interference and Splitting large parts.

Gap and cure time by method
Method Gap No load until
Thin CA ≤ ~0.15 mm minutes to handle, hours for full strength
Gel CA ≤ ~0.25 mm same as thin
Epoxy ~0.1–0.3 mm (design value) ~24 h at room temperature (longer in the cold)
Acetone (ABS / ASA) contact ~24 h
Heat welding V-groove, filler of the same plastic once cool

Load the joint in shear

A joint holds far more in shear than in peel or tension. A lap, a sleeve or a tab puts the glue line in shear over a large area. A butt joint works in tension over a small area, and if one edge opens it peels from that end. With the same glue, a lap multiplies the area and loads the joint in the direction it handles best.

butt (tension)loadglue linesmall areaweakpeelloadstress at the edgeweakestlap (shear)loadlarge areastrong
The same glue performs very differently depending on joint geometry. A butt joint works in tension over a small area; opened at one edge, it peels with all the stress at the end; a lap joint works in shear along its whole length.

Bond to walls, not infill

The glue grips the outer walls. If the face is backed by only two walls over sparse infill, the joint holds but the walls tear away from the infill right next to it. Print mating faces with more walls or solid infill behind them (Walls, perimeters and infill, Modifiers by region and height).

Orient the joint so the load does not pull in Z

The layers next to the joint are still the weak plane. For design, assume the part is half as strong in Z as in XY, or 30 % if the material is fiber-filled, and orient it so the main load runs along the beads (Layer adhesion and anisotropy).

Allow for heat

Gluing does not raise the maximum service temperature either: glued PLA still softens at around 57 °C (HDT at 0.45 MPa). Often the adhesive gives up before the plastic does. Many consumer epoxies and the 5-minute ones soften between 40 and 60 °C, and standard CA starts to lose strength around 80 °C; it depends on the product, so read its datasheet. For ASA, ABS or PC that works hot (a car's dashboard in the sun reaches 70–100 °C), choose a slow high-temperature epoxy or weld.

Clamp and wait

Apply light, even pressure with clamps, tape, rubber bands or the part's own pins. Wipe off squeeze-out before it hardens, and wait out the times in the table.

Welding ABS and ASA with acetone

Check that the faces sit flat against each other. Brush acetone on both, wait a few seconds for them to turn tacky, press them together and hold with light pressure. The softened surfaces fuse into each other and no glue line is left.

For gaps and open joints, make an ABS slurry: offcuts of the same filament dissolved in acetone to the consistency of cream. The slurry fills and welds at once, and if the offcuts are the same color the line disappears. The catch is that it shrinks as it dries, because almost all of its volume is acetone that evaporates. Fill in thin coats, let each one dry and overfill slightly before sanding. A thick fill needs more than a day.

Acetone leaves the joint slowly, and while solvent remains the bond is soft and weaker. For reference, 4 mm ABS bars that had been vapor-smoothed gained around 1 % in weight from the solvent and water they held. Do not load, sand or paint the part for about 24 h.

Set your expectations. A good solvent weld behaves like an interlayer bond in the same plastic, not like something "stronger than the part". Too much acetone caves in thin walls and erases the detail next to the joint.

Solvent cements for acrylic, PVC or styrene are a different chemistry with a different safety datasheet. Some well-known ones, such as Weld-On 16, contained 30 to 60 % DCM, and in 2025 they were reformulated without it. Vapor and chemical smoothing explains why DCM and THF are not for home use and why PLA has no safe solvent.

Welding with heat and filament

A length of the same filament is your filler rod. The heat melts the rod and also the walls of the groove, and the filler fuses with both sides. If only the rod melts and lands on a cold surface, you get a bead that pulls off in one go: without penetration there is no weld.

fusedV-groove, ~90°filler (same plastic)melted zonedepth: 1/2 to 2/3 of thicknesscold surfaceunfused linepeels offV-groove, ~90°
The weld holds when the filler fuses with the melted walls of the groove. On a cold surface you get a bead with an unfused line beneath it, and it peels off in one piece.

Prepare the joint before you heat anything. On a butt joint, cut a V-groove of about 90° along the line, between half and two-thirds of the wall thickness deep. Better still, model a chamfer on both edges so the halves form the V when they meet. The filler needs room to reach the bottom and a large melted surface to bond to.

Soldering iron

Use a dedicated tip or a cheap iron kept for plastic only: molten plastic ruins an electronics tip. The temperature is the same as for setting heat-set inserts, 10 to 20 °C above the print temperature. For materials not in the table, such as TPU or PP, apply the same rule to their print temperature. Dry nylon and PC before welding: the moisture boils and leaves bubbles in the bead.

Tip temperature for welding plastic (the same as for inserts)
Material Tip
PLA 220–240 °C
PETG 250–260 °C
ABS / ASA 260–270 °C
PC / PA 280–300 °C
Others (TPU, PP…) 10–20 °C above their print temperature

Lay the rod in the groove and push it in with the tip while you melt the walls. Move slowly and smooth it off at the end. The same method repairs cracks and holes. With the tip too hot or the travel too slow, the plastic scorches, bubbles and loses strength.

Friction welding

Clamp a short piece of filament in the chuck of a rotary tool and spin it against the groove: friction melts filler and part at the same time. It is fast, penetrates deep and works with PLA, PETG and ABS. Leave little filament sticking out of the chuck, because a long piece whips and snaps. Keep a steady pace and trim the excess flush. Lab tests on printed PLA show that joint strength depends on spindle speed and stays below that of solid PLA. It is good for repairs and closing seams; it does not bring back the strength of the original material.

Rotary tool with a short piece of blue filament in the chuck, melting into the V-groove between two PETG halves; ahead of it the groove is still open and behind it the groove is filled with a rippled bead of filler (generated illustration)
Rotary tool with a short piece of blue filament in the chuck, melting into the V-groove between two PETG halves; ahead of it the groove is still open and behind it the groove is filled with a rippled bead of filler (generated illustration)

Hot air with welding rods

This is how bumper repair shops work and how PP and PE are joined, since no common glue bonds them. A 3D pen also lays down filler, but on a cold surface it only adds a bead on top. Melt the groove first with the iron, or use the pen only to add material.

When it fails

The broken faces tell you what happened.

Glued and welded joints: symptom, cause and fix
Symptom Cause Fix
The glue stays whole on one face and the other comes away clean and shiny (adhesive failure) The face was not prepared, was dirty, or the glue does not wet that plastic (PP, PE, release-agent residue) Sand, clean, use a primer or switch to welding
The glue splits through its own thickness (cohesive failure) Wrong glue for the load or the gap: brittle CA in peel, too wide a gap for CA, badly mixed or uncured epoxy Switch to epoxy, redesign as a lap and wait out the full cure
The plastic tears out with the glue still attached (substrate failure) The joint outlasted the part Strengthen the part with more walls or a better orientation; the glue is no longer the problem
A white haze surrounds the CA joint Evaporated monomer that has settled Less glue, more ventilation, a low-bloom CA or a touch of activator
The glued joint gives way on a part that gets hot The adhesive softened before the plastic High-temperature epoxy or welding
The welded bead peels off in a single strip No penetration: the groove was too shallow or its walls never melted Cut a deeper V and melt the walls before adding filler
The welded bead comes out full of bubbles Tip too hot, travel too slow or damp material Lower the temperature, move faster and dry nylon and PC first

See also

Design it in KapyCAD

Many of these problems are cheaper to fix in the model than in the slicer: wall thickness, overhangs, the face the part stands on.

Free plan, no card. Runs in your browser, nothing to install.

Open the editor

Still have a question?