kapy academy

Bed prep for each material

15 min readUpdated Nov 2026

Every material asks the plate for two things that pull in opposite directions: grip while it prints, and let go when it is done. Nylon and PP slide on PEI and the part lifts halfway through the print; PETG and TPU bond so hard to smooth PEI that peeling them off rips chunks out of the coating. Bed prep means choosing the surface, the cleaning, the temperature and, when needed, a release film, so that the bond lands between those two limits. What each plate is, Beds and build surfaces explains.

Grip and release: the window for each pairing

Every pairing of material and plate has a window between gripping too little and gripping too much. The first bead holds through contact area and, in some pairings, through an almost chemical bond while it is hot. PETG, PC and PEI are all polar polymers, which is why PETG and PC wet PEI so well. When you peel the part off, the crack runs wherever the bond is weakest, and that decides whether the plate survives.

partcoatingsteelToo weakpartshrinkagebreakIn the windowpartflakebreakToo strongpartbreakglueWith release layer
Where the bond breaks on removal, in four cases: nylon or PP on PEI (too weak), PLA on PEI (in the window), PETG on smooth PEI (too strong) and PETG on a film of glue (release layer).
  • Too weak. Nylon or PP on bare PEI: the bead never wets the surface and the part lifts during the print.
  • In the window. PLA on PEI: it grips while hot and, as the plate cools, the part shrinks more than the steel sheet. The interface is loaded in shear and lets go.
  • Too strong. PETG on smooth PEI, or TPU on PEI: the bond to the plastic is stronger than the coating's bond to the steel. The crack dives into the coating and tears out a flake.
  • With a release layer. A film of glue between the two: the crack runs through the film, which washes off with water, and the plate stays intact.

Cooling releases the part because, as the plate drops from 60 °C to room temperature, the plastic shrinks several times more than the steel. The interface ends up in shear and, in a pairing that sits in the window, breaks there. Remove most parts once the plate is below about 40 °C; flexing the sheet pops them off. Prying with the plate still hot is how PEI usually gets scratched.

Gripping too hard is a failure too. A torn-out flake leaves a pit that marks the underside of every part that follows, and the plate no longer holds in that spot. The fix is a release layer.

Glue stick does two opposite jobs depending on the pairing. It is a water-soluble film of PVA or PVP. On a surface the plastic does not wet (nylon on PEI, PC on some plates) it acts as an adhesive. On one the plastic bonds to too strongly (PETG or TPU on PEI) it acts as a separator, or release agent.

Cleaning the plate

Skin oil is a release agent: a single fingerprint is enough to let a corner go. For a deep clean: warm water with a few drops of washing-up liquid (not hand soap, which leaves oils), rinse, and dry with a lint-free cloth. After that, keep your fingers off the print area.

Prusa recommends isopropyl alcohol (IPA) at 90 % or higher for the quick wipe between prints. When parts start letting go even after an IPA wipe, it is time for water and washing-up liquid: IPA dissolves skin grease poorly and ends up smearing it around. Prusa's PP plate is cleaned this way, with IPA before every print and soap if that is not enough.

Clean it cold and with the sheet off the printer: no splashes on the electronics, no thermal shock, and access to the edges. If you printed with glue, wash it off with warm water afterwards. Glue built up over several sessions forms a relief, and that relief is copied into the next first layer.

Do not put the sheet in the freezer to release parts. Prusa forbids it on its textured, satin, nylon and PP plates: condensation and the sudden temperature change punish the coating. A coating that no longer holds when clean is worn: if the sheet is double-sided, flip it; if not, replace it (Bed and motion upkeep).

Glue and release layers: how much and how

With the plate cold or warm, never hot, spread the glue stick in crossing passes until you have a thin, even film over the area the part will cover. Let it dry until it is no longer tacky. A thick, lumpy film is copied into the first layer and holds no better. Renew it every two or three prints, or after washing.

Liquid glues and dedicated agents work the same way but leave a more even film, and some are designed for a specific bed temperature. Printer makers sell their own, alongside the Magigoo range (with PRO versions for PC, PA, PP and flexibles, and a general one for PLA, PETG and ABS) and Vision Miner's Nano. A stick is easier to put exactly where it is needed; a liquid gives a more regular first layer. Before using any of them, check what your plate accepts: Bambu, for example, recommends its own glue stick or liquid glue for its plates.

Hairspray also lays down a thin film on glass and PEI, but do not use it: in an enclosed machine the mist ends up on the rods and rails, and glue stick does the same job without that risk.

Leave the glue off in three cases:

  • PLA on clean smooth or textured PEI: it adds a step and nothing else.
  • Plates designed to print without adhesive, such as Prusa's nylon and PP plates.
  • SuperTack-type cool plates, which grip on their own.

Material by material

Bed prep by material
Material Bed (°C) Surface Glue or agent Typical failure
PLA 35–65 (55–60) smooth or textured PEI, cool plate none dirty plate; bed too hot
PETG, PETG-HF 60–80 (70) textured PEI release layer if the plate is smooth or the part large tears flakes out of the PEI
PCTG 70–80 textured PEI release layer on smooth PEI same as PETG
ABS, ASA 90–110 PEI optional, adhesive on large footprints corners lifted by shrinkage
PC and blends 100–120 PEI or engineering plate yes: adhesive and release layer wet filament; tears out on cooling
Unfilled PA 90–120 garolite (G10), PA plate or PEI adhesive on PEI wet filament; slides off bare PEI
PA-CF/GF 80–120 PEI or engineering plate adhesive wet filament
TPU 30–45 textured PEI release layer breaks the coating on removal
PP 80–100 polypropylene, PP plate PP agents only will not stick to PEI

Manufacturers change their plates, and their rules, from one revision to the next. What follows holds for Bambu and Prusa plates as of late 2026; when in doubt, your plate's documentation wins.

PLA and its variants

Smooth or textured PEI, or a cool plate with a lower bed temperature; in every case, nothing on top. It fails on a dirty plate or a bed that is too hot: above about 65 °C the base softens and you get elephant's foot (The first layer and bed adhesion). Cool plates with a tacky coating, such as Bambu's Cool Plate SuperTack, hold PLA at a lower temperature; use the value the profile carries for that plate. Bambu warns that its PLA Silk bonds so strongly to the original SuperTack that the part can be damaged on removal. A cool plate without that coating, such as Bambu's basic Cool Plate, is for PLA only and needs glue.

PETG, PETG-HF and PCTG

Textured PEI is the first choice. On smooth PEI, or on the glass of older machines, only with a film of glue as a release layer, because PETG can tear flakes out of the coating. Textured PEI copes better, but with too low a Z offset it chips too, and the same release layer fixes it. Bed at 70 °C. Raising the Z offset a little compared with PLA also helps (The first layer and bed adhesion). Remove it with the plate fully cold.

Smooth PEI plate with two pits where the coating has been torn out and the gray steel shows, next to an upside-down blue PETG part with gold flakes of coating stuck to its base
Smooth PEI plate with two pits where the coating has been torn out and the gray steel shows, next to an upside-down blue PETG part with gold flakes of coating stuck to its base

ABS and ASA

PEI holds them at 90–110 °C. Glue is optional and helps on parts with a large footprint and on smooth PEI. The bed is rarely the problem: shrinkage pulls the corners up, and the fix is an enclosed machine plus a brim or mouse ears (Warping and lifting corners, Enclosures and heated chambers). Do not lower the bed temperature to make removal easier: that is exactly how corners lift.

PC and its blends

Bed at 100–120 °C, enclosed machine. Hot, it bonds strongly to smooth PEI and, cold, it shrinks a lot, so use glue on PEI or on an engineering plate; Bambu calls for glue on its Engineering Plate with any filament. Here the glue is adhesive and release layer at once. Dry PC first: wet, it foams in the nozzle and the first layer comes out rough and weak (Drying and storing filament).

Nylon (PA6, PA12, PA11, PA-CF)

It sticks poorly to bare PEI. In order of preference: a sheet of garolite (G10), which nylon grips while hot and lets go of as it cools; a dedicated PA plate, such as Prusa's Special PA Nylon, which runs without adhesive and is cleaned with water only; or glue stick or a PA agent on PEI. Bed at 90–120 °C for unfilled PA, with the machine enclosed. Always dry it: wet nylon bubbles, leaves a porous, weak first layer and looks as if it will not stick even on the right surface. Unfilled PA shrinks in the order of 1–2 %, and a large, flat part warps even on a perfect bed. Fiber-filled grades (PA-CF) shrink far less along the bead and are the best place to start.

TPU

Low bed, 30–45 °C. TPU grips PEI too hard, smooth PEI above all, and harder the hotter the bed. Use textured PEI with glue as a release layer and peel it slowly from one corner, with the plate cold. On SuperTack-type plates, check the plate's documentation first. Dry it too: wet TPU comes out full of bubbles and the first layer never lies flat.

PP

It sticks to very few surfaces. Its surface energy is so low that almost nothing wets it, for the same reason glue will not stick to a PP food tub. What does work: polypropylene (packing tape, whose backing is PP, stretched taut over the plate), coatings made for PP, such as Prusa's powder-coated PP plate (which also takes PLA, PETG and TPU), or a dedicated agent such as Magigoo PRO PP. Neither more glue nor more temperature will hold it on any other surface. Bed at 80–100 °C on a PP plate or agent; with tape, check what temperature it tolerates, because its adhesive gives way with heat and the tape wrinkles or lifts. PP shrinks in the order of 1.5–2.5 %, the most of any material in the table: a brim and rounded corners are mandatory, and if the part warps, the tape lifts with it.

Everything else

PVA or BVOH supports go on whatever surface the main material asks for (Support materials). Fiber-filled grades follow their base polymer, but wear textured PEI faster over time. PEEK, PEI and other high-temperature polymers belong on industrial machines: PEI filament welds itself to a PEI plate and needs a different surface (PPS, PEEK, PEKK and PEI).

Bed temperature: what it does and what it does not

In PETG, ABS and PC, which are amorphous, and in printed PLA, which comes out almost amorphous, the bed keeps the base close to its glass transition: the bead stays soft enough not to peel and the part's outline shrinks less. Far above it, the base sags; far below it, the outline shrinks unchecked and lifts. In semi-crystalline plastics (PP, nylon) the bed does a different job: it slows the cooling and crystallization of the base, which is what shrinks most, and so reduces warping. TPU, flexible at room temperature, barely needs a heated bed.

Start from the profile. Bambu Studio and OrcaSlicer store a different bed temperature for each plate type in the filament profile. If you change the plate on the printer, change it in the slicer too, or the temperature will be the one for another plate.

Correct in 5 °C steps. Go up if, on a clean and suitable plate, the material does not hold. Go down if it holds too hard or the base sags. More temperature never fixes the wrong surface: nylon on bare PEI and PP on anything not made for PP still will not stick at 120 °C.

In an enclosed printer, open the door for PLA, PVA or TPU once the bed is above about 45 °C, and for PETG above about 70 °C (Enclosures and heated chambers). ABS, ASA, PC and nylon want the door closed.

Removing a part that will not come off

Work through this order:

  1. Wait until the plate is below about 40 °C.
  2. Flex the sheet.
  3. If it is PLA, or the plate is SuperTack-type, and the part is still stuck: put the sheet back, heat the bed to about 50 °C and flex it again. Near its glass transition PLA softens and the interface gives. With PETG or PC that temperature changes almost nothing.
  4. Go in from the edge with a thin plastic or brass-edged scraper, held very flat. Never dig the tip of a craft knife into the coating.

If there was glue, a stream of warm water under the edge dissolves the film and the part comes away on its own. The freezer is out for Prusa's textured, satin, nylon and PP plates; on the others, use it only as a last resort and with the sheet off the printer.

When it fails

Bed prep failures
Symptom Cause Fix
A PLA corner lets go mid-print skin oil on the plate wash with water and washing-up liquid, and keep your fingers off the print area
Nylon or PP lifts even with a hotter bed the surface does not wet it garolite, a PA plate or glue (nylon); tape, a plate or an agent made for PP
PETG or TPU tears flakes out of the PEI the bond is stronger than the coating's bond to the steel release film, a little more Z offset and a few degrees off the bed
PC tears out with pieces of coating as it cools it bonds hot and shrinks a lot a film of glue, bed temperature unchanged
Wide, sagging base on PLA bed above about 65 °C drop the bed to 55–60 °C
ABS or ASA corners lift on a good bed shrinkage enclosed machine plus a brim or mouse ears (Brims, rafts and mouse ears)
ABS or ASA tears out coating on a large footprint strong bond on smooth PEI a release film on those parts
Rough or bubbly first layer (PC, nylon, TPU) wet filament dry it before printing
The first layer copies a relief glue built up over several sessions wash the sheet with warm water
A clean plate no longer holds worn coating flip the sheet or replace it

See also

Design it in KapyCAD

Many of these problems are cheaper to fix in the model than in the slicer: wall thickness, overhangs, the face the part stands on.

Free plan, no card. Runs in your browser, nothing to install.

Open the editor

Still have a question?