kapy academy

Filament comparison table

16 min readUpdated Nov 2026

Once you know what would make your part fail (Choosing a filament), these two tables put the families side by side: what each material gives you and what it asks of the printer. The figures are manufacturer data for 1.75 mm filament, nearly all from one manufacturer's datasheets (Bambu Lab), so the columns compare like with like. Another brand may give different values, and a printed part falls short of the datasheet specimen. Use the tables to shortlist candidates; a test part makes the final call.

What each material gives you

Each family has its own article: PLA and its variants, PETG, PCTG and other copolyesters, ABS and ASA, Polycarbonate and its blends, Nylons and polyamides, Polypropylene, TPU and flexible filaments, Carbon and glass fiber filaments and PPS, PEEK, PEKK and PEI.

What each material gives you
Family HDT at 0.45 MPa (°C) Service under load (°C) Flexural modulus XY (GPa) Toughness Shrinkage (%)
PLA 57 (52–60) 40 2.8 brittle 0.2–0.5
PLA-HT 70 · ≈105 annealed ≈50 · ≈85 annealed ≈ PLA brittle 0.3 (+0.3–0.6 when annealed in Polymaker grades; measure it)
PETG / PETG-HF 69–71 50 1.8 medium-high 0.3–0.5
PCTG ≈65–75 ≈50 ≈1.6–1.9 high 0.3–0.5
ABS 87 70 1.9 medium 0.5–0.8
ASA 100 80 1.9 medium 0.4–0.7
PC 112–117 95 2.3 very high 0.5–0.8
PC-ABS ≈100–115 HDT − (15–20) ≈1.9–2.3 high 0.5–0.7
Unfilled nylon (PA6, PA12) 90–130 ≈50, lower when moist ≈1–2 (dry) very high 1–2
PP depends on grade no load when hot ≈0.4–0.6 very high 1.5–2.5
TPU (95A–85A) no HDT no HDT 0.01 does not break 0.5–1
PLA-CF / PETG-CF ≈ its base ≈ its base 2.9 (PETG-CF) brittle-medium 0.2–0.5*
PA-CF / PAHT-CF 186 / 194 ≈140 / ≈150 4.2 (PAHT-CF) medium 0.2–0.5*
PET-CF 205 ≈165 5.1–5.3 brittle-medium 0.2–0.4*
PPA-CF 227 ≈180 9.9 brittle-medium 0.2–0.4*
PPS-CF 264 ≈210, test it no verified value brittle-medium 0.2–0.4*
PEEK / PEI PEEK ≈140–160 · PEI depends on grade PEI 9085 ≈135 · PEEK, test it ≈2.2–4 high (PEI 9085) 1–1.5 / 0.5–0.7

* For fiber-filled compounds, the shrinkage given is along the bead; across it, shrinkage is higher. Values marked "≈" are estimates or ranges with no verified datasheet behind them: they rank the families, but to calculate anything you need your spool's datasheet. For TPU the table gives Young's modulus (about 9 MPa), because no flexural modulus is published. Expressed in GPa (0.01), it sits two orders of magnitude below everything else. Glass-filled nylon (PA-GF) behaves like the PA-CF row: a little less stiff, with a similar HDT. In the "under load" column, the "≈" rows of the semi-crystalline materials come from the HDT at 1.8 MPa (see "How to read each column").

Support materials (PVA, BVOH, HIPS) and specialty filaments are left out of the table: they are covered in Support materials, Functional specialty filaments, Decorative filaments and Metal filaments and sintering. Resistance to UV and chemicals has no column either: Heat, cold, sunlight and chemicals covers it.

What it asks of the printer

Same rows, same order. Bold marks the starting value where there is one.

What it asks of the printer
Family Nozzle (°C) Bed (°C) Surface Enclosure Nozzle material Drying Difficulty €/kg
PLA 190–230 (215) 35–65 (55–60) smooth or textured PEI no brass recommended 1 15–30
PLA-HT 200–230 50–60 PEI no brass recommended 1 > PLA
PETG / PETG-HF 230–270 (245) 60–80 (70) textured PEI no brass recommended 2 15–30
PCTG 240–270 70–80 textured PEI no brass recommended 2 25–40
ABS 240–280 90–110 PEI passive brass recommended 3 15–30
ASA 240–270 90–110 PEI passive brass recommended 3 25–40
PC 260–290 100–120 PEI + glue passive or heated brass required 4 35–60
PC-ABS 250–275 100–110 PEI + glue passive brass required 3 30–50
Unfilled nylon 250–290 90–120 glue on PEI or garolite passive or heated brass required 4 40–80
PP 220–250 80–100 PP sheet or packing tape passive brass rarely 4 30–50
TPU 200–250 (225) 30–45 textured PEI + glue no brass required 2 (95A) · 4 (85A) 30–50
PLA-CF / PETG-CF as its base as its base textured PEI no hardened recommended 2 30–50
PA-CF / PAHT-CF 260–300 80–120 glue on PEI heated (recommended) hardened required 3 55–110
PET-CF 260–300 80–120 glue on PEI heated (recommended) hardened required 3 60–100
PPA-CF 285–320 100–120 glue on PEI heated hardened required 4 150–210
PPS-CF 310–340 100–120 glue on PEI heated hardened required 5 ≈200–270
PEEK / PEI 380–440 / 340–390 120–160 Kapton / dedicated adhesive industrial the machine's own required 5 hundreds of €

Notes on the table:

  • "No" under enclosure does not mean you need an open printer. On an enclosed printer, open the door or lid once the bed goes above about 45 °C with PLA or TPU, or about 70 °C with PETG. Otherwise heat travels up the heatsink (heat creep) and clogs the hotend. "Passive" means an unheated enclosure; "heated", an active chamber at 50–65 °C; "industrial", 90 °C or more. The details are in Enclosures and heated chambers.
  • Maximum hotend temperature. The stock hotend on current machines reaches 290–300 °C, enough for PC, nylon, PA-CF and PET-CF. PPA-CF and PPS-CF need a hotend in the 320–350 °C class, like the one on the Bambu X1E (320 °C, in the lower part of PPS-CF's 310–340 °C range) or the H2 series. PEEK and PEI need 400–500 °C: industrial equipment. A hotend with a PTFE liner down to the nozzle runs at 240 °C at most, because beyond that the PTFE starts to degrade: it suits PLA and TPU, and PETG only at the bottom of its range, 230–240 °C.
  • Hardened nozzle (or harder: carbide, ruby) for anything with fiber in it. Preferably 0.6 mm, 0.4 mm if you must, never 0.2 mm, and never brass or stainless steel. The same rule applies to abrasive decorative filaments: glow-in-the-dark, marble, glitter. Nozzles: size and material explains why.
  • Surface. PETG bonds so hard to smooth PEI that it can tear flakes out of it: on smooth PEI, always put down a layer of glue as a release agent. Every other combination is in Bed prep for each material.
  • Drying. The table only says whether it is needed. Temperatures and times are in Drying and storing filament.
  • Price is a rough guide for late 2026, per net kilo. Engineering filaments often come on 500–750 g spools, so always compare in €/kg (What comes on a spool of filament).
  • ABS, ASA, PC and nylon give off ultrafine particles and VOCs you should not breathe. Print them in a filtered enclosure or with extraction to the outside (Emissions and ventilation).

These are starting points. The real number comes from your slicer profile and a temperature tower (Test coupons).

How to read each column

  • HDT at 0.45 MPa. Heat deflection temperature, measured at a low stress: it ranks materials, but it is not the temperature a loaded part survives. Always check the stress it was measured at: at 1.8 MPa the figure comes out lower and the two cannot be compared (on the same datasheet, PLA gives 57 and 54 °C; PAHT-CF, 194 and 170 °C). The "under load" column applies the book's rule: under load, design 15–20 °C below the HDT at 0.45 MPa if the plastic is amorphous (PLA, PETG, ABS, ASA, PC), and 15–20 °C below the HDT at 1.8 MPa if it is semi-crystalline, with or without fiber (nylon, PP, PA-CF, PET-CF, PPA-CF, PPS-CF). Why is in Heat, cold, sunlight and chemicals, and what to put in a car is in Choosing a filament.
  • Flexural modulus. It measures how stiffly the part resists bending: it sets how far brackets, arms and housings deflect. It does not tell you when the part breaks. The table uses the flexural modulus because a printed bracket is loaded in bending, and because the tensile modulus on these datasheets is unreliable: the same ABS datasheet gives 3.8 GPa in tension and 1.9 in bending. It is an XY value, along the bead; between layers it is lower (PAHT-CF drops from 4.2 to 1.8 GPa in Z). The orientation rule in Layer adhesion and anisotropy applies to stiffness too. This is the datasheet column: to calculate deflections and forces, use 90 % of it (PLA 2.5 GPa, PETG 1.6), because a real part has seams and joins that the test bar does not.
  • Toughness. How much energy the part absorbs before it breaks. It is given in words because printed-specimen numbers rank the materials poorly. The notched Charpy test depends so much on the notch, the orientation and the bond between layers that the same manufacturer's datasheets give PC 7.5 kJ/m², against 21.6 for PETG and 21.5 for ABS. Drop a part, though, and the order flips: PC is the one that survives. Elongation at break tells a similar story: printed PC manages only 3.8 %, although the bulk polymer stretches far more. So the column ranks the materials by how parts behave when dropped or knocked, not by the test-bar figure. The physics is in Stiffness, strength and toughness.
  • Shrinkage. It hits you twice: it lifts the part off the bed and it throws your fits out. If both halves of a fit are the same material, they shrink by almost the same amount and the clearance barely changes. The trouble starts when the part mates with metal, with a bought-in part or with another material, and on long dimensions: 0.5 % over 100 mm is 0.5 mm, more than the clearance of a sliding fit (0.15–0.20 mm per side on a modern machine). Correct it once, in the slicer's filament profile: OrcaSlicer ("Shrinkage (XY)") and Bambu Studio ("Shrinkage") compensate it per filament. Note that you enter the measured size as a percentage of nominal (99.6 %), not the shrinkage (0.4 %). More in Shrinkage and dimensional stability; what to do with your clearances when you change family is in Choosing a filament.
  • Difficulty. Our own 1–5 scale, combining three things: the tendency to lift (shrinkage and the need for an enclosure), the need for drying, and how narrow the tuning window is. It depends on the machine: ABS is a 3 on an enclosed CoreXY and a 5 on an open legacy bedslinger.
  • Price. Per net kilo. Material is usually a small share of a part's cost next to machine time and failed prints (What a printed part costs).

What the tables teach

Fiber adds stiffness and heat resistance, but not toughness. PET-CF and PPA-CF are roughly 3 to 5.5 times stiffer than PETG and have an HDT 135 to 160 °C higher. Short fibers carry the stress along the bead and restrain the matrix: less creep, less shrinkage. But every fiber is also a place where a crack can start, and that shows in drops and knocks. A part that has to survive being dropped calls for PC or nylon. Within the fiber-filled group, the most forgiving is PAHT-CF, with 8.4 % elongation against 3–4.5 % for PET-CF, PA6-GF and PPA-CF.

PC and nylon win on toughness and temperature, but hardly on stiffness: PC (2.3 GPa) barely beats PETG (1.8), and unfilled nylon matches it or falls below, more so once it absorbs moisture. Among unfilled materials the stiffest is PLA (2.8), and PETG-CF barely beats it. What adds real stiffness is fiber in an engineering matrix: PA, PET, PPA.

EnclosureHeated chamber125104080120160200240280Flexural modulus XY (GPa, log scale)HDT at 0.45 MPa (°C)TPU · 0.01 GPa · no HDTfiber-filled: stiffer, more heat-resistant, less toughUnfilled nylonPLAPETGABSASAPCPETG-CFPA6-GFPAHT-CFPET-CFPPA-CF
Stiffness against temperature, from manufacturer datasheets (XY flexural modulus, HDT at 0.45 MPa). The unfilled families cluster at the bottom left; PC and nylon move to the right without climbing much. Only fiber in an engineering matrix (PA, PET, PPA) gains on both axes; PETG-CF stays next to PLA. Glass-filled PA6-GF lands next to the carbon-filled nylons. TPU is off the chart.

Each step up in temperature needs a different class of machine. Above PETG (HDT ≈ 70 °C), the unfilled families that follow (ABS, ASA, PC, nylon) need an enclosure; the exception is annealed PLA-HT. Above about 180 °C, where the fiber-filled engineering materials begin with PA-CF, you need a heated chamber and a hardened nozzle, and from PPA-CF on, a high-temperature hotend. PEEK and PEI need an industrial machine; if your part needs them, the usual answer is to have it made (When to order the part instead). Difficulty and price rise with each step. Pick the cheapest family that resists your part's failure mode.

PriceDifficultyOpen printerstart here≤ 75 °CPLA · PETGPCTGEnclosure87–130 °CABS · ASAPC · NylonChamber and hardenednozzle186–205 °CPA-CF · PET-CFHigh-temperaturehotend227–264 °CPPA-CF · PPS-CFIndustrialPEEK · PEI
Each step up in heat resistance raises the price, the difficulty and the machine you need, all at once. A rough guide: 15–40 €/kg for PLA, PETG and PCTG; 15–80 with an enclosure; 55–110 with a chamber; 150–270 with a high-temperature hotend; hundreds of euros per kilo on the industrial step.

PP and TPU are in a class of their own. Neither is stiff, but PP has the best fatigue resistance and TPU does not break at all. Each makes bed adhesion hard in its own way: almost nothing sticks to PP, and TPU sticks too well. If your part is a hinge or a bumper, this table will not settle it: go to Living hinges and flexures and TPU and flexible filaments.

One column is missing on purpose: sustained load, because the margin below the HDT does not cover creep. At room temperature, PLA holds a light sustained load about as well as PETG: no reliable data on printed parts says which creeps more. PETG only wins when the part gets warm. For a sustained load, use PC or ASA, or a fiber-filled filament if the part is not a spring (Creep and fatigue).

When it fails

Symptom, cause and fix
Symptom Cause Fix
Two brands, two HDTs that do not match One measured at 1.8 MPa and the other at 0.45 MPa Only compare at the same stress; see Reading a material datasheet
You chose the material with the highest tensile strength and the part broke when dropped Strength is not toughness Check the toughness column
A CF bracket sized with the XY modulus deflects or cracks between layers XY values only hold along the bead; in Z, strength drops to ~30 % of XY and stiffness to ~40–50 % Align the load with the bead
You compared prices per spool A 500 g spool at the same price costs twice as much per kilo Compare in €/kg
A fit that worked in PLA is tight in nylon Nylon shrinks 1–2 % and swells as it absorbs water Print the coupon with dry filament, leave it a few days at the humidity it will live in before measuring, and set the clearance for that state (Test coupons)

See also

Design it in KapyCAD

Size the walls, the clearances and the orientation for the material you chose.

Free plan, no card. Runs in your browser, nothing to install.

Open the editor