The face that sits on the plate is the flattest face of an FDM part and its best Z reference, and its edge is the worst-printed one. The first layer is squashed on purpose so that it grips, which makes its outline grow. At the design stage you decide three things: what the bottom edge looks like, how much of that face actually bonds, and which dimensions near the base you can trust. The rule: a 0.5 × 45° chamfer on the edges that touch the plate, the slicer's compensation at its default, and no fillet on the bottom edge.

Why the base comes out wide

With a 0.4 mm nozzle, the first layer is laid 0.20 mm thick and 0.50 mm wide, pressed against the plate. The displaced plastic has nowhere to go but sideways, so it spills past the nominal outline. The heated bed keeps the lowest layers soft, so the second and third layers spread a little too. The result is a lip of one or two tenths of a millimeter per side over the first 0.2 to 0.6 mm of height. The first layer and bed adhesion covers the full mechanism.

You notice it at assembly. The part will not sit flush in its pocket or slot. A lid rubs only along its bottom edge. A vertical hole is tight at the mouth and loose further up. Measured with callipers at the base, the part reads oversize.

Before you touch the design, look at the first layer. A first layer that is translucent with ridges between the lines is squashed too hard: the problem is the Z offset, not the model (Bed probing and Z offset). For PLA the bed runs at 35 to 65 °C, usually 55–60 °C. Above about 65 °C the base grows as well, because PLA passes its glass transition at around 60 °C and the low layers give under the nozzle's pressure. Once the first layer is set correctly, the lip that remains is normal, and the slicer's compensation and the chamfer deal with it.

Compensation and chamfer, both at once

The slicer's compensation pulls the first layer's outline inwards by a fixed amount. At the end of 2026, the stock profiles ship with 0.2 mm on the Prusa MK4S, 0.15 mm on the Bambu Lab X1C and 0.075 mm on the A1. The setting is called "Elephant foot compensation" in PrusaSlicer, Bambu Studio and OrcaSlicer; in Cura the equivalent is a negative "Initial Layer Horizontal Expansion". In PrusaSlicer, Bambu Studio and Cura it only touches the first layer. OrcaSlicer can spread it, tapering off, over several layers ("Elephant foot compensation layers"). In every case it is a fixed estimate.

The chamfer gives the displaced plastic somewhere to sit during the first two or three layers and hides the compensation's error. It also removes the sharp edge, the one that snags and chips. Leave the compensation at its default and model the chamfer as well.

Yes, they add up. With a 0.5 mm chamfer and 0.2 mm of compensation, the first layer ends up about 0.6 mm inside nominal. That bottom half-millimeter mates with nothing, so you lose nothing: from the third layer up, the wall is on size. You will sometimes read that the two should not be combined because they shrink the base. The shrinkage is real, but it falls inside the chamfer.

Do not push the compensation far above its default to get rid of the lip. You shrink exactly the outline that holds the part down, and you leave a visible step in the first layer.

On a raft there is no elephant's foot, because the part's first layer sits on the raft interface, not on the plate. There the chamfer is optional.

Chamfer, not fillet: what the slicer sees

Mainstream slicers slice the model at the mid-height of each layer: with 0.20 mm layers, at z = 0.1, 0.3 and 0.5 mm. The bottom edge becomes a staircase of 0.2 mm treads, and the shape of that staircase decides where the squashed plastic goes.

sharp edgeelephant's footnominal outline0.20 mmplatechamfer 0.5 × 45°recessfillet r 0.5elephant's footfillet r 3overhang > 45°contact lost
The same bottom edge sliced into 0.20 mm layers. The sharp edge spreads into a lip; the 0.5 mm chamfer leaves a recess of 0.4 and 0.2 mm, bigger than the lip, which stays hidden inside the nominal outline; the 0.5 mm fillet leaves half the recess and almost nothing on the second layer; the 3 mm fillet overhangs by more than 45° at its lowest part and loses contact width.

0.5 mm × 45° chamfer. The outline sits 0.4 mm inside nominal on layer 1, 0.2 mm on layer 2 and on nominal by layer 3. The recess is exactly where the squashed plastic goes, and each tread steps out at exactly 45°, so it prints without support.

0.5 mm fillet. It sits 0.2 mm inside on layer 1 and 0.04 mm on layer 2: half the recess on the first layer and almost nothing on the second, right where the heat of the bed is still spreading the plastic. A small lip shows on layer 2. It does a worse job than a chamfer of the same size, but it does not fail.

3 mm fillet, the one that goes on every edge out of habit. It sits 2.2 mm inside on layer 1, 1.7 on layer 2, 1.3 on layer 3 and 1.1 on layer 4. The outline steps outwards by 0.54, 0.35 and 0.27 mm per 0.2 mm layer: overhangs of 70°, 60° and 54°. A fillet of radius r on the bottom edge overhangs by more than 45° over its lowest stretch, which is r(1 − 1/√2) ≈ 0.29·r tall. With r = 3 mm that is 0.9 mm: about four layers printed into thin air on the very edge that has to hold the part down. Those layers curl upwards, the edge comes out ragged and the part grips less.

At the same leg length, a chamfer and a fillet take the same width off the footprint. The difference is how big each one has to be to do its job. A 40 × 40 mm box with a 3 mm fillet underneath keeps a flat face of about 34 × 34 mm: 1156 of its 1600 mm², 72 %. With a 0.5 mm chamfer the flat face is about 39 × 39 mm: 1521 mm², 95 %. Those are the model's figures; the real first layer, sliced at 0.1 mm and minus the compensation, comes out close.

Chamfers below, fillets above. A fillet is fine on vertical edges (the corners seen in plan) and on top edges. On the edge against the plate, a chamfer or nothing.

How big a chamfer

The reference value is 0.5 mm × 45°, within 0.4 to 0.6 mm, for a 0.4 mm nozzle and 0.20 mm layers. It has to be taller than the zone that spreads (the first two or three layers, 0.4 to 0.6 mm) and wider than the lip and the compensation together. And small enough to cost almost no contact and not read as a bevel.

With another nozzle or layer height, make it at least two to three times the first-layer height. With a 0.6 mm nozzle and 0.30 mm layers that gives 0.6 to 0.9 mm.

Keep it at 45°. A shallower one, at 30° from horizontal, overhangs at 60°, curls and uses up more contact. A steeper one prints fine, but for the same height it leaves less room for the squashed plastic. At 45° the recess is the largest you can get without an overhang.

Large chamfers do another job: the lead-in on a part that is pushed into a pocket, or keeping the part from digging into your hand. They follow the 45° rule, but they cost contact: check how much you have left.

Where it goes and where it does not

The 0.5 mm chamfer goes on every outside edge resting on the plate. Also on the mouth of every vertical hole or slot that starts at the plate: a 0.5 mm internal chamfer, like a countersink, opens the tight mouth and guides the screw or pin in. And on bosses and pins printed standing on the plate that go into another part.

Thin walls do not take two chamfers. A 0.9 mm wall (two beads) chamfered 0.5 mm on both sides leaves about 0.1 mm on the first layer: nothing to bond. Below about 2 mm, chamfer only the outside edge and leave the inside one square; minimum wall thicknesses are in Minimum features and text.

Some edges are meant to stay sharp: the edge of a scraper, a part that must sit flush against a wall along its base, a sealing line. Orient them so that they do not touch the plate (Orientation and overhangs), or rely on the compensation alone and run a test.

The first thing the squashed plastic closes up is text or a logo engraved into the bottom face. Make the strokes a little wider than the usual engraving minimum.

This face copies the surface of the plate: the grain of textured PEI, the gloss of smooth PEI or the pattern of an embossed plate (Beds and build surfaces).

Edges that peel

Peeling starts where the first layer is thin or ends in a point. The design sets three traps.

tangent contactcontact1 mm flat cutacute angletruncated tip0.9 mm wallchamfer outside onlyplate
Three contacts that peel and their fix: a cylinder lying down touches along a line, and a 1 mm deep flat cut gives it a band; a wedge meeting the plate at an acute angle prints a fringe of loose lines, and truncating it gives it a footing; a thin wall chamfered on both sides barely touches the plate, and chamfering only the outside is enough.

Tangent contact. A cylinder lying on its side, a sphere or a curved base touch the plate along a line or at a point, and the first layer is a strip a few tenths wide. Model a flat: a 1 mm deep flat cut along a horizontal cylinder gives a band that grips, and stops it rolling, too.

Acute edges. A wedge or a blade that meets the plate at an acute angle prints its first layers as a fringe of loose lines, which lifts at the first bit of shrinkage. Trim the tip with a flat at least two line widths across (line width is around 0.45 mm; 0.42 in Bambu Studio), or stand the wedge on its flat face.

Sharp corners of the footprint in plan. That is where warping starts. Rounding them as seen from above moves the peeling front inwards; Warping and lifting corners gives the radii per material. Rounding the corner in plan helps; rounding the bottom edge in section hurts. And the chamfer does not fix warping. It deals with the lip and the edge; warping is shrinkage, and you fight it with radii in plan, an enclosure and a plate that grips.

If the contact has to be small, the next step is a brim or modeled mouse ears (Brims, rafts and mouse ears).

Dimensions at the base

The bottom face is the part's best Z reference: flat against a flat plate, at Z = 0. Measure heights from it and put the faces whose flatness matters there, unless warping distorts it.

Its edge is the worst XY reference. The first half-millimeter is distorted by the lip and by the chamfer you added. Do not dimension a fit against the bottom edge: place whatever has to mate above the chamfer height, and measure 2 or 3 mm up from the base when you check a part. Parts that print the wrong size explains how to measure and tell the lip from a scale error; Iterate and measure covers the test loop.

When a part locates in a pocket by its base (a lid in a frame, a box on a base plate, a cartridge in a slot), it is the base outline that binds. Chamfer it and give it the clearance you would give it anywhere else (Real printed clearances).

A vertical hole that is only tight at the mouth is elephant's foot. If it is tight along its whole length, it is a different mechanism: Why holes print small.

When it fails

Bottom face problems
Symptom Cause Fix
The base does not sit flush, the lid rubs at the bottom Elephant's foot Default compensation + 0.5 mm × 45° chamfer
The lip is still large with a chamfer First layer squashed too hard or bed too hot Z offset; bed temperature within range
Bottom edge lifted on a filleted base Large fillet overhanging by more than 45° A chamfer instead
Peels at a thin edge or a curved base Tangent or acute contact Flat cut, truncated tip or another stance
The corners of a large base lift Warping Radius in plan, enclosure, brim
Hole tight only at the mouth Elephant's foot 0.5 mm internal chamfer at the mouth

See also

Design it in KapyCAD

Draw the part with these clearances and walls, and change any dimension later without redrawing it.

Free plan, no card. Runs in your browser, nothing to install.

Open the editor

Still have a question?