kapy academy

When your numbers drift

14 min readUpdated Nov 2026

In March, an 8 mm steel pin slid into your printed bracket with 0.20 mm of clearance per side and turned without rubbing. In June the same file, profile and printer give a pin that binds. The model has not changed, but the clearance does not belong to the design alone: it is a measurement of one printer, one nozzle and one filament as they were on the day you measured. Several things move it, each at its own pace and in its own direction: find which one before you touch the clearance.

Why no table can give you your clearance

Published values are ranges per class of machine, for a calibrated printer running PLA or PETG. Sliding fit: 0.20 mm per side (0.40 on the diameter) on a modern bedslinger and 0.15 on an enclosed CoreXY (Real printed clearances). The typical error of those same classes is on the same scale as the clearance itself (Accuracy, precision and repeatability). That is why a table cannot choose your value: all it tells you is where to put the middle step of your coupon.

Two "identical" printers do not give the same measurement either. The bias of a printed hole depends on flow, line width, that filament's shrinkage, the slicer's compensations and the mechanics; Parts that print the wrong size separates those kinds of error, and Why holes print small explains why holes shrink. A profile made for a printer model knows the model, not your particular machine, your spool or the wear on your nozzle.

The only value you can trust is the one you measured yourself, with the conditions written down next to it.

Measure your values and keep a reference

Calibrate the machine and the filament first (What to calibrate, and in what order), then scale, skew and XY compensation (Dimensional calibration), and only then the fit coupons (Test coupons). A clearance measured on an uncalibrated machine stops being valid the moment you calibrate it.

Write the conditions down with every value: printer, nozzle (diameter, material and which one exactly), filament brand and type, whether it was dry, profile, layer height and date. The full list is in Test coupons.

Keep the coupon with the chosen step marked and, with it, a steel reference: a ground dowel pin, the shank of an 8 mm drill bit or the bore of a 608 bearing (8 mm). They are physical gauges that do not drift.

One thing is still missing: a starting point, the baseline. On the day you calibrate, print a witness part: a fixed file that never changes and that you always print with the same profile, in the same orientation and in the same spot on the bed. One row of the fit coupon will do, or a ring with an 8 mm bore and a 50–100 mm bar. Measure two or three dimensions, at least one large one and one hole, and write them down. Without that baseline, you will have no way of telling later whether anything has moved.

Keep each value in one place only, and give the profile that holds it a name and a date (Printer, filament and process profiles). A profile is a dated calibration record, not a permanent template.

Drift or noise?

Scatter is the copy-to-copy variation when nothing changes: a few hundredths of a millimeter on a calibrated machine. Drift is a trend: several prints in a row moving in the same direction, or a step after a change. A single bad measurement is not drift. The statistics are in Accuracy, precision and repeatability.

Keep the noise floor in mind. Callipers carry an uncertainty of ±0.03–0.05 mm on an FDM part, so on a calibrated modern machine do not try to correct differences below about 0.05 mm. Measure two or three copies of the witness part, cold, at mid-height and along two axes. Mid-height because the first layer depends on the Z offset: if someone has re-leveled or changed the offset, the base comes out more or less squashed and throws the reading off. Iterate and measure covers the technique.

Rule out the instrument first. Zero the callipers, check them against the steel reference, replace the battery if it is low and measure at room temperature. A part that is still warm measures large. A nylon part that has spent days in damp air has grown, but that is a change in the part in service, not in the printer: it is covered in Shrinkage and dimensional stability.

Keep a log: date, spool, nozzle and the witness-part readings. On a chart, drift has a shape that gives its cause away: a step when you change spool, a dip that recovers after drying, a slow ramp over weeks, a jump after an update or after someone touched the belts. Scatter is a cloud around a flat line.

BaselineNoiseDampDriedNew nozzleNew spoolScatterWearTighterPrintClearance
Scatter is a cloud inside the noise band. Drift has a shape: a step that stays, a dip that recovers on drying, a ramp that only a new nozzle corrects.

What moves your numbers

The filament. Every material shrinks by a different amount as it cools: roughly 0.2–0.5 % for PLA, 0.3–0.5 % for PETG, 0.5–0.8 % for ABS and 1–2 % for unfilled nylon (PA). On top of that, the filament's real diameter changes the volume per millimeter: ±0.02 mm on 1.75 mm means ±2.3 % flow, and cheap spools reach ±0.05 mm or do not state it at all (What comes on a spool of filament). The two leave different signatures. Shrinkage scales with size: the 100 mm dimension moves more than the 8 mm hole, and outsides and holes shrink together. A Ø20 hole that goes from PLA (0.3 %) to nylon (1.5 %) loses about 0.24 mm of diameter, 0.12 mm per side: nearly a whole sliding fit. A change in diameter or flow, on the other hand, is a fixed offset: outsides larger and holes smaller, whatever their size. Measure one large dimension and one hole on the witness part and you will know which you have. The change is abrupt and arrives with the spool; if you move to ABS or nylon you will also see warping and lifting corners. If you change family or brand, repeat the filament calibration from What to calibrate, and in what order and print a new coupon. The same filament in another color should not need recalibrating; if it is heavily filled or has additives (glow-in-the-dark, silk, matt), check it with the witness part.

Moisture. Absorbed water boils in the melt zone, the bead foams and comes out wider and uneven: walls grow and holes close up. It comes with popping at the nozzle, stringing and rough surfaces. The pace depends on the material: nylon or PVA shows it within hours out of its box; PETG, PC and TPU within days; PLA holds out for weeks. Fits get tighter, and unevenly; what gives it away is that it goes away when you dry the spool. Dry it (temperatures in Drying and storing filament), reprint the witness part and compare it with the baseline. Never re-tune the clearance with a damp spool.

The nozzle. The extruder meters volume, so a wider orifice does not lay down more plastic. What changes is the shape of the bead. As the nozzle wears, the orifice opens up and the flat face of the tip rounds over and shrinks: it squashes the bead less, so the bead comes out less well defined, with a ragged edge. The fit dimensions shift, often toward tighter, and the witness part tells you which way. The wider orifice also changes the pressure inside the nozzle, so the right pressure advance value shifts: bulging corners and uneven lines appear. The first visible warning is grooved top surfaces and worse ironing; after that, fits that slowly change. It is a slow ramp, over weeks or kilograms. With abrasive filaments (carbon or glass fiber, glow-in-the-dark, glitter, marble), a 0.4 mm brass nozzle opens up visibly within a few hundred grams; hardened steel wears too, on a scale of kilograms.

The opposite case is a partial clog or heat creep: too little material comes out, walls are thin and gappy, holes grow, fits loosen and the extruder often clicks. If hot air reaches the cold side of the hotend, PLA softens too early and jams (Hotends and how much they can melt). In an enclosed machine, the most common cause is printing PLA with a hot chamber, and an open door prevents it; in an open one, the heatsink fan. Check or replace the nozzle (Nozzle and hotend care) and then repeat what a new nozzle calls for in What to calibrate, and in what order: the Z offset if your probe does not sense with the nozzle itself (inductive, BLTouch, eddy current), because load-cell and nozzle-contact probes sort it out on their own, plus a flow and pressure advance check. Watch the stored values: a printer cannot tell two nozzles of the same diameter and type apart. After swapping a worn nozzle for an identical one, run the pressure advance calibration by hand (Flow Dynamics on Bambu printers, as of late 2026) rather than trusting the value it already had.

The machine. Belts lose tension after running in and with use. A reinforced GT2 belt barely stretches and it is the pulley teeth that set the travel, so a slack belt does not shrink or enlarge the part uniformly. What it causes is mechanical play: oval holes, a dimension that depends on which side the nozzle came from, ringing after corners and, on a CoreXY with its two belts at different tensions, skew (squares come out as rhombuses). A loose pulley grub screw shows up as layer shifts. Tension the belts until their measured frequency matches the manufacturer's value (Rails, belts and motors), repeat the resonance compensation (input shaping) and check the skew again with the frame from Dimensional calibration.

There are two more causes, with no part that wears: software and the environment. A firmware update can wipe stored values, and a slicer update or a cloud-synced profile can change defaults (line width, compensations) without you noticing. Compare the profile with the one you saved (Firmware: Marlin, Klipper and closed systems). As for the environment, printing ABS or ASA with the door open, or in a cold room in winter, changes shrinkage and warping.

Causes of drift
Cause Pace Effect on fits What else you see First check
Filament change When you change spool Every dimension in the same direction; shrinkage if it scales with size, flow if it is a fixed offset Warping if you move to ABS or nylon The witness part: one large dimension and one hole
Moisture Hours (nylon) to days Tighter, uneven Popping, stringing, rough surfaces Dry and reprint
Worn nozzle Weeks or kilograms Slow change, often tighter; confirm with the witness part Grooved top surfaces, worse ironing, bulging corners Inspect the tip
Partial clog or heat creep Days Looser, with gaps Thin walls, clicking extruder Cold pull; door open with PLA in an enclosed printer
Belts Weeks, or after shipping Oval holes, X differs from Y, skew Ringing, size that depends on direction Belt frequency
Update or profile With the update A step in one parameter Nothing else Compare the profile

Find the cause before you touch the number

Work through this in order, from the most likely and cheapest to check to the least likely: the measurement; whatever your log says has changed since the baseline (spool, brand, update, profile, work on the belts); the spool (dry it and reprint the witness part); the nozzle (top surfaces, a look at the tip); and the mechanics (ovality and skew point to the belts). Only if all of that is fine and the change is permanent do you recalibrate and write down the new value.

There is a physical reason for the order. Reading the log costs nothing; drying takes hours. Moisture and a spool change move a fit overnight and are the most common causes. The mechanics drift slowly and leave their own signature, ovality or skew, which a fit coupon alone cannot tell apart.

diagram
The order of checks when a proven fit stops fitting the way it did, whether it has got tighter or looser. Each branch fixes one cause; recalibrating is the last resort.

Never correct a passing fault by changing the clearance. If you widen it to live with a damp spool or a worn nozzle, you have stored a fault as if it were a constant. The day you dry the spool or replace the nozzle, every part comes out loose. Recalibrate only when the change is permanent: a new brand or family, a nozzle of a different diameter or material, a new printer.

If you run several printers, print the same witness part on all of them and compare each with its own baseline, not with the others: two identical machines already started from different values. The one that moves away from its own by more than the noise explains is the one that has drifted, not the design (Print queues and print farms).

When to check without waiting for a failure

What to repeat after each specific change is in the change table in What to calibrate, and in what order. Between changes, the witness part catches what no change announces: moisture, wear and belts. A sensible rhythm is to print it with every spool of a new brand or a heavily filled color, after any nozzle change and, on a machine that prints daily, once a month or every few kilograms. If you print abrasive filaments with a brass nozzle, after every spool. A maintenance schedule sets how often to do the upkeep itself.

When it fails

Symptom, cause and fix
Symptom Cause Fix
After drying the spool, everything is loose You calibrated with damp filament Repeat the coupon with dry filament
Fits change week by week and top surfaces get worse Worn nozzle Inspect or replace it before you touch the clearance
The pin slides one way round and binds the other, or holes come out oval Slack belts Tension the belts; leave the clearance alone
Everything changed at once after an update The profile or firmware went back to defaults Compare it with the profile you saved
You clean the nozzle and the fits loosen again a few days later Heat creep with PLA in an enclosed printer Print with the door open (Enclosures and heated chambers)

See also

Design it in KapyCAD

Design parts sized for your printer and your nozzle.

Free plan, no card. Runs in your browser, nothing to install.

Open the editor

Still have a question?