A part that goes to resin (FDM or resin for your part) is modeled by other rules. You can draw details two to five times finer, supports hold up whatever hangs and the part is almost equally strong in every direction. In exchange, a closed cavity ruins it, holes and clearances shrink and the material snaps instead of bending. It all comes from four causes: light cures a little beyond where it shines, every layer peels off the film, cured resin is a brittle thermoset that shrinks, and trapped liquid never cures.

What changes from FDM

FDM against resin, rule by rule
Rule FDM Resin
Minimum wall ≈ 0.9 mm (2 beads) 0.2 mm minimum (Form 4); design ≥ 0.5–1 mm
Smallest text 3–4 mm characters 1–2 mm characters
Overhangs 45° chamfers, teardrops Supports hold them; without them, only short overhangs (≈ 5 mm at ≥ 10° on the Form 4). No islands
Horizontal hole Clean up to 6 mm; above 10 mm, teardrop or flat roof Comes out squashed in Z
Closed cavity No problem Forbidden: it must drain
Strength by direction Weak in Z Nearly the same
Heat-set inserts Yes No
Snap fits In PLA or PETG Tough resin only
Clearance From the FDM coupon From a resin coupon at your exposure

Why dimensions shift: light bleed and cure-through

In XY, the cured area is slightly larger than the lit pixels. Light arriving at an angle and light scattered inside the resin cure past the edge, and overexposure makes it worse. So every outline moves outwards by the same small amount. An outer wall grows, a pin gets fatter, a hole shrinks and the gap between two parts closes from both sides. Holes come out small, as in FDM, but for a different reason. In FDM the cause is the squashed bead and the polygon the hole is faceted into (Why holes print small); here it is the light. A gap narrows twice, once per face, and a small hole narrows all the way round. That is why small holes and tight clearances are the first things to close up.

In Z you get cure-through. The light that cures a layer does not stop there: it carries on into whatever lies behind. If that is liquid, as inside a horizontal hole at the moment the layer that closes it is exposed, it cures a skin of unwanted resin. So the side of a horizontal hole or channel that prints last grows inwards, and the hole comes out oval, squashed in Z. For reference, Carbon states that in its DLS process holes come out 0.05 to 0.2 mm smaller in Z because of this effect. That is a figure for an industrial machine. Clear resins suffer more, because light travels further into them.

Pixel size limits how crisp an edge is, not the smallest detail. As of late 2026, 10-inch machines such as the Elegoo Saturn 4 Ultra 16K have 14 × 19 µm pixels, and a 7-inch one such as the Mars 5 Ultra has 18 µm. The smallest reliable detail spans several pixels, plus the bleed, and it also has to survive the peel. Never design at the size of a pixel.

Exposure shifts every one of these dimensions. Too much, and features grow and holes close; too little, and features thin out and detail is lost. The exposure test is in How a resin printer works. Your clearances only hold for that resin and that exposure.

XY: one layer, seen from the screenSide sectionMachine viewPinHoleGapPixelsLit areaCured areaModel outlineBuild plateLightFilmSide printed lastModel outlineCure-through
Left: within one layer, the cured area spills past the lit pixels; the pin gets fatter and the hole and the gap narrow relative to the model outline. Right, in machine view (plate on top, film below): the light that closes a horizontal hole cures resin inside it, on the side that prints last, and the hole comes out squashed in Z.

Minimum figures: walls, details, holes and clearances

The most complete recent set of measured figures for a resin machine is Formlabs' design guide for the Form 4, with its Grey V5 resin at 50 µm. A supported wall is joined to the part on two or more sides; an unsupported one, on a single side. An embossed detail stands proud; an engraved one sinks in.

Formlabs minimums: Form 4, Grey V5, 50 µm layer
Feature Minimum
Supported wall 0.2 mm
Unsupported wall 0.2 mm
Embossed detail 0.1 mm
Engraved detail 0.15 mm
Clearance between parts 0.4 mm
Hole 0.5 mm
Vertical rod 0.3 mm (7 mm tall) / 0.6 mm (30 mm tall)
Unsupported overhang 5 mm long, at 10° or more from horizontal
Horizontal bridge 29 mm (5 × 3 mm beam)

These are absolute minimums: below them nothing prints, and designing right at them leaves no margin. They were measured on one specific machine, with its optics, its resin and its test pieces. The older Form 2 guide (Clear resin, 100 µm layer) gave 0.4 mm walls, 0.4 mm engraving, 0.5 mm clearance, 0.8 mm holes and 1.5 mm for a 30 mm tall rod. The Form 2 is a laser machine; the Form 4 now uses a screen, like your MSLA, but with different optics and a different pixel. Across its own machines, the same company's figures differ by a factor of up to two or three: that is how far the minimums can move, and only your coupon measures your machine's.

Start from these values and confirm them with a test coupon.

Starting points on desktop MSLA, against FDM
Feature Resin: design value FDM, 0.4 mm nozzle
Decorative wall ≥ 0.5 mm 2 beads, ≈ 0.9 mm
Wall that is handled or carries load ≥ 1 mm 3–4 beads or more
Embossed detail ≥ 0.2 mm high and wide ≥ 0.5 mm stroke
Engraved detail ≥ 0.3 mm wide and deep ≥ 0.6 mm stroke
Round hole ≥ 1 mm Prints small; see Why holes print small
Short vertical pin ≥ 0.5 mm, thicker the taller it is ≥ 2 beads
Character height 1–2 mm 3–4 mm

Thin walls have an extra problem: left too long in the wash, they soak up alcohol and distort, and thin rods lose strength. Keep their wash short. For pins and rods, slenderness rules: the taller and thinner they are, the more they wobble on every peel. The FDM figures come from Minimum features and text.

Text in resin stays legible at sizes FDM cannot reach. Emboss it rather than engrave it, and keep it on faces without supports. Use engraved text only if resin can drain out of the grooves, meaning they open to an edge or are at least 0.3 mm wide.

A long, thin, free-standing feature, such as a sword blade or a spear, flexes on every peel and comes out bent or wavy. Make it short, give it a fillet at the root, or tie it to the part with a sacrificial bridge you cut off afterwards, as miniature designers do.

Clearances and fits: measure them, do not copy them

Do not reuse your FDM clearances. There, they are set by the squashed bead and the machine's motion; here, by bleed, exposure and cure shrinkage. The numbers are different, and they change from one resin to the next.

There are two kinds of clearance, with different minimums. The first is a gap that only has to stay open during the print: two parts printed together, a hinge printed in place. Its published minimum is Formlabs' 0.4 mm. On a Form 3, that 0.4 mm gap measured 0.15 mm once printed: the bleed ate the rest. The second is the clearance between parts printed separately and assembled afterwards. It can be much smaller, because nothing has to stay open during the print. On your test coupon, include a clearance ladder from 0.05 to 0.30 mm per side, in 0.05 mm steps (per-side clearance is counted as in Real printed clearances).

A precision horizontal hole comes out squashed in Z because of cure-through. Print precise bores vertically, with the axis perpendicular to the plate, or leave 0.1 to 0.2 mm extra in that direction and open it up with a drill. You do not need a teardrop: supports and the following layers hold up the roof. It does no harm either.

A press fit that works in PLA cracks a standard resin bushing: the material does not give. If you need interference, use a tough or ABS-like resin, keep the interference small and test it first. Better still, glue the pin (Gluing and welding printed parts). Heat-set inserts do not work because resin does not melt (Designing for heat-set inserts): glue in knurled inserts or use a captive nut (Captive nuts and clearance holes). Self-tapping screws split standard resin (Self-tapping screws in plastic). Fine threads close up with bleed: model threads of M4 or larger with the clearance from your coupon, or drill and tap afterwards. Cured resin machines well, although threads cut in standard resin are brittle (Modeling threads).

Brittle, isotropic and shrinking: shapes that hold up

A properly cured resin part is roughly as strong in every direction, unlike an FDM one (Layer adhesion and anisotropy). Orientation is decided by the peel, the supports and the finish, not by strength.

Standard resin is brittle: Elegoo Standard has an elongation at break of 8.8 % (Types of resin). A sharp inside corner concentrates stress and is where the crack starts. Fillet every inside corner that carries load: on small parts, 0.5–1 mm is enough. Do not put cantilever snap fits in standard resin (Print-friendly snap fits). Keep living hinges and flexures to tough or flexible resin, and to a low cycle count (Living hinges and flexures).

Resin shrinks as it cures, and again during post-cure. A thick section next to a thin one cures and shrinks differently: the thin one warps or the transition cracks. Keep wall thickness uniform and hollow out thick bosses. Avoid large, thin flat sheets, which also flex on every peel and warp after post-cure. If you need a flat panel, stiffen it with ribs and print it tilted (Orienting and supporting resin prints). Manufacturers publish few shrinkage figures and they do not agree with each other: measure it on your coupon.

Post-curing also embrittles: overdo it and the part becomes more brittle and may yellow. Times and procedure are in Washing and curing resin parts.

Hollow parts and drain holes

This rule is resin's alone: no closed cavities. In FDM a sealed cavity causes no trouble and needs no vent (Lightweighting). In resin, the liquid inside never cures, oozes out for weeks and, with the heat of post-cure, can crack the part. During the print, a cavity closed toward the plate and open only toward the film acts as a suction cup; the mechanism is in Orienting and supporting resin prints.

The slicer hollows decorative parts well. Hollow in the model when you want to decide where the holes go (on a hidden face, away from a datum face, sized for your plug) or when the hollow has to follow the outer shape.

Hollow part on desktop MSLA
Decision Starting value Why
Wall 2–3 mm Any thinner and it flexes on every peel and cracks later
Number of holes ≥ 2 per cavity One lets air in, the other lets liquid out
Position One at the end nearest the plate, one at the opposite end, both on hidden faces The first also vents the cavity during the print
Diameter 3–5 mm Viscous resin and alcohol have to be able to flow
Formlabs reference ≥ 2.5 mm (Form 3 / 3L), ≥ 0.75 mm (Form 4) Valid for those machines only; 0.75 mm does not work in a desktop vat

Check every enclosed volume: a blind hole, a deep pocket closed by a lid in your design, the inside of a hollow handle. A blind hole too narrow to wash holds liquid resin at the bottom.

To seal a drain, design a stepped plug: a shoulder slightly larger than the hole and a spigot the hole's diameter minus the clearance from your coupon. Print it on the same plate. Once the cavity is washed and dry, glue it in with a drop of resin and cure it. Make the hole round and on a flat or gently curved face, so the plug seats.

There is no infill in resin: the inside is solid, hollow or a lattice the slicer generates, and the lattice has to drain too.

Toward the plateTrapped liquidSealedToward the plateDrainedWallAir inLiquid outHidden faceDrain holePlug
Two sections of the same hollow part, in model view. In the sealed one, liquid stays inside and eventually cracks the wall. In the drained one, the wall is uniform and there are two holes on hidden faces: one at the end facing the plate and one at the opposite end, so air gets in and liquid gets out; the stepped plug closes the second.

Where the supports and the bed face go

Every support leaves a mark on the face it touches (Support removal and cleanup). Decide while modeling which face takes them (the hidden underside or the inside of a shell), keep fine detail and text off it, and give it a smooth surface. A small flat landing on a curved face turned toward the plate gives the supports a clean place to sit. And even though supports hold up almost everything, leave no islands: every feature should grow from something already printed or from a planned support.

A functional part with a flat datum face can print straight on the plate, without supports. The base layers get several times the normal exposure to grip the plate (How a resin printer works), and the base flares out: resin's elephant's foot, the equivalent of FDM's (The face on the bed). In the model, put a 0.3–0.5 mm 45° chamfer on the base edge, more if your base flares a lot, and keep fit surfaces out of the first millimeter. Think about how you will release it too: a large flat face grips hard, and a lip or a chamfer gives the scraper somewhere to get in.

Sharp edgeChamferedBuild plateFlareBase layersModel outlineBuild plateNo fits hereChamferFilmMachine view
Machine view: plate on top, film below. With a sharp edge, the overexposed base layers spill past the model outline. With a 45° chamfer, that flare fills the chamfer and does not stick out past the side wall. Fit surfaces go above the first millimeter.

If the part does not fit the build volume, split it. A 10-inch machine such as the Saturn 4 Ultra 16K gives you about 212 × 118 × 220 mm. Design locating pins with your resin's clearance and glue the halves (Splitting large parts, Gluing and welding printed parts). Splitting has another advantage: each half gets its own orientation.

When it fails

Symptom → cause → fix
Symptom Cause Fix
Engraved text comes out flush 0.2 mm grooves filled by bleed and by resin that never drained and cured in place Grooves at least 0.3 mm wide and a little deeper, or embossed text
A print-in-place hinge comes out fused Designed with FDM's 0.3 mm gap Start at 0.4 mm and check it on a coupon with that resin and that exposure
A snap fit breaks the first time you assemble it Thin arm in standard resin, which does not give Tough resin with a longer, thicker arm, or a screw
A press fit cracks the bushing Standard resin does not give Tough resin with little interference, or glue the pin
A horizontal hole comes out oval, squashed in Z Cure-through on the side printed last Print it vertically, or leave 0.1–0.2 mm extra in Z and open it up with a drill
A hollow part oozes for weeks or cracks during post-cure Cavity with no drain, or with only one hole Two 3–5 mm holes at opposite ends; wash and dry the cavity before curing
A flared base stops the part from fitting Overexposed base layers 0.3–0.5 mm × 45° chamfer on the base and no fit surface in the first millimeter
A flat sheet warps after post-cure Uneven thickness, or a large thin panel that flexes on every peel Uniform wall, ribs and the panel printed tilted

How to test it

Before you trust any figure, print one coupon per resin, at your exposure: walls, embossed and engraved lines, holes and pins from 0.3 mm, a clearance ladder and a horizontal hole. The method is in Test coupons.

See also

Design it in KapyCAD

Design parts sized for your printer and your nozzle.

Free plan, no card. Runs in your browser, nothing to install.