You load the part into the resin slicer and it sits flat on the plate, the way you would print it in FDM. In resin, that is usually the orientation most likely to fail. A resin part prints tilted, held up by a forest of thin supports, and often hollowed out. All three are decided before the first layer cures. The part hangs from the plate, and every layer is torn off the film at the bottom of the vat: what breaks a resin print is almost always that pull, not gravity.

Every layer peels off the film

Throughout this article the figures show the machine: build plate at the top, film at the bottom. The slicer shows you the same scene upside down, with the plate at the bottom. To avoid confusion, this article says "toward the plate" and "toward the film"; where "up" or "down" appears, it says which view it means.

The full mechanism is in How a resin printer works; here you only need its consequence. The layer cures between the film and the part. The plate rises. The film has to let go of the whole freshly cured area at once. The force is roughly proportional to that area: a 50 × 50 mm layer leaves 2,500 mm² stuck to the film. The pull acts on the newest, softest layer and on every joint between the part and the plate.

That pull breaks the weakest link first. In order: the thin supports, the joint between the part and its supports and, last, the raft on the plate. The classic symptom is a sheet of cured resin stuck to the film and nothing else on the plate.

A tilting vat, low-adhesion films and warm resin reduce the pull on each layer (How a resin printer works).

On any machine you also have a slicer setting: lift speed. The suction holding the layer grows with the area and with how fast the plate rises. A slow lift for the first layers and for large cross-sections lowers the pull without touching the geometry. None of this removes islands or suction cups: there, orientation still rules.

flattilted 45°filmfilmbuild platecurrent layerpeel forcesupportsheightbuild platecurrent layerpeel forcesupportsheight
The same tile, in machine view. Lying flat, each layer cures its full width at once and the peel pulls on all of that area. Tilted, each layer is a narrow strip and the pull is small; the price is extra height.

Tilt the part: small layers, gentle peel

An example with numbers. A 50 × 50 × 3 mm tile lying flat on the plate cures 2,500 mm² in a single layer. Tilt it 45° onto one edge and each layer is a 50 × 4.2 mm strip (3 / sin 45°): about 212 mm², nearly twelve times smaller. The cost is height. Flat, it stands 3 mm tall; tilted, about 37 mm. Since resin print time depends only on height (FDM or resin for your part), that part takes longer, but a plate full of tilted parts takes no longer than a single one.

Starting points for resin orientation
Decision Starting value Why
Tilt 30–45° to the plate, on two axes (the first layer is a corner) No layer cures a long straight edge in one go
Large faces Tilted, except a reference face placed directly on the plate A large face parallel to the plate is a maximum-area peel
Small faces Parallel to the plate or clearly tilted A nearly parallel face leaves wide steps
Show face Toward the film (up in the slicer) Supports go on the faces that look toward the plate
Long parts Held at both ends, or close to vertical A long part sags while it is green (not yet post-cured)

These values are community and slicer practice, not rules. More tilt is not always better: a taller part means more layers, more peels and longer supports that can sway.

A face parallel to the plate and looking toward the film is the last layer of that region and comes out smooth. The same face looking toward the plate comes out free of steps but covered in support marks. Faces a few degrees off horizontal show the layers most, because each 0.05 mm layer turns into a wide terrace. The terrace width is the layer height divided by the tangent of the angle: at 45°, 0.05 mm; at 5°, 0.57 mm, steps you can see and feel.

Supports rest on the faces looking toward the plate (down in the slicer): turn the show face toward the film and leave the marks where nobody sees them.

There is one exception. A functional part with a large face that must come out flat and true can go directly on the plate, with no tilt and no supports. The cost: the first layers get a much longer exposure to grip the plate, that face grows slightly (resin's elephant's foot) and it is hard to pry off. Add a small chamfer at the base of the model or compensate by a few tenths of a millimeter there; the exact rules are in Designing for resin.

Islands: a layer cannot cure on thin air

An island is a region of a layer that rests on nothing cured in the previous layer. The part grows from the plate toward the film, so every new feature starts at its point closest to the plate. In machine view: the tip of a finger pointing at the plate, the edge of an overhanging lip closest to the plate, the crown of an arch that opens toward the film. Every point that sticks out toward the plate (a local minimum in the slicer, where it appears at the bottom) starts life as an island.

Without a support, the first layer of that island cures against the film and stays there. The following layers can print on top of that flake and damage the film or even the screen, or the flake ends up floating in the vat. That forgotten flake is the most common reason the following print fails too: check the vat after every failure.

Chitubox, Lychee and each manufacturer's own slicer include an island detector; PrusaSlicer in SLA mode supports islands when it generates its automatic points. UVtools checks them on the already sliced file. Also scroll through the layer view around every tip, because a one-layer island is easy to miss.

Not all islands matter equally. Since Lychee 7.5 (November 2025), the slicer sorts them by size and lets you ignore the tiny ones, which the following layers absorb like any overhang. A support on a 0.1 mm speck does more harm than good.

After islands come overhangs. A tilted face looking toward the plate (down in the slicer) cures each layer slightly beyond the previous one, and if it gets too close to horizontal it needs supports at intervals. That angle depends on the resin and the machine, and the slicer lets you set it; there is no universal number. Under long faces parallel to the plate and looking toward it, space the supports out, closer together near the edges.

machine view (the slicer shows it upside down)islandsuction cupfilmfilmbuild plateflake stuck to the filmsupportbuild platesuctiontrapped liquidvent
Machine view. Left: the lip starts at a point with nothing between it and the plate; its first layer cures against the film and stays there. A support gives it somewhere to cure. Right: a cavity closed toward the plate and open toward the film creates a vacuum on every lift; a vent in the closed end lets the liquid in.

Anatomy of a resin support

From the part to the plate, a support has five parts. The contact tip is a cone that narrows to the point where it touches the part. Contact depth is how far that tip sinks into the part. Then come the shaft, the bracing that ties shafts together, and the base or raft on the plate.

The light, medium and heavy presets in slicers mainly change the tip diameter. A thin tip leaves a small mark and can snap during the peel; a thick one holds and leaves a crater. Size the tip to the load: thick where a large section peels, thin on fine detail.

Starting points for supports
Parameter Starting value When
Tip diameter 0.3–0.4 mm Fine detail, visible faces
Tip diameter 0.5–0.6 mm Large surfaces, the region near the plate
Contact depth 0.1–0.2 mm General
Raft On Any part larger than a miniature

These are starting values from community guides, not from any manufacturer; the guides themselves disagree on the shape of the contact. Tune them to your resin: tough and especially flexible resins come off the printer soft and need thicker tips (Types of resin).

Place supports in this order: first one on every island, then along the overhanging edges, then a grid under the large faces that look toward the plate. The supports at the end of the part closest to the plate, the first to print, carry the peel of the whole part: make them thicker.

The raft is a cured slab on the plate that spreads the pull and lets you lift the whole thing off with the scraper without bending the supports. Many slicers add one by default.

Generate the automatic supports, go through the island list and the layer view, add by hand whatever was missed and remove any that land on the show face. Lychee 7.5, for example, keeps manual supports when you re-run the automatic ones. How to remove them and clean up the marks is in Support removal and cleanup.

Resin part printed tilted on a raft, held up by thin supports that only touch the face looking toward the plate
Resin part printed tilted on a raft, held up by thin supports that only touch the face looking toward the plate

Suction cups: the vacuum that tears the part off

A suction cup is a cavity closed toward the plate and open toward the film. In machine view, as the walls grow, their rim seals against the film. Every lift tries to enlarge a sealed volume full of liquid, and the vacuum pulls on the whole part. In the slicer it looks like a bowl facing up, with the opening away from the plate. Helmets, mugs, boxes and any hollowed part suffer from it most. Formlabs warns that a cavity like this can trap resin or air and blow the part apart during the print.

A suction cup and a sealed cavity are different problems. The suction cup creates a vacuum during the print, while the cavity is still open against the film. The sealed cavity traps liquid afterwards, once the part is closed. The first tears the part off; the second can crack it days later.

The symptoms of a suction cup: the part breaks away from its supports right at the height where the cavity begins, thin walls burst, or the whole part rips off the plate.

You have three fixes:

  • Flip it so the opening faces the plate. Liquid flows in through the opening as the cavity grows, and it never seals against the film.
  • Tilt it so the rim reaches the film progressively and the cavity is never closed off by a flat ring. It helps, but it is not always enough.
  • Open a vent in the closed end, the end of the cavity closest to the plate, so liquid can flow in as the volume grows.

Since Lychee 7.6 (January 2026), its voxel hollowing includes a suction-cup detector with an option to fill the interior beneath them; UVtools also flags them in the sliced file.

Hollow the part and drain it

A solid part more than 10 mm thick wastes resin and peels huge areas on every layer. Hollowing turns each layer into a ring and cuts both. Small parts and parts that must take compression stay solid.

Every major resin slicer hollows parts, with an optional internal lattice.

For home-sized parts, start with 2–3 mm walls. Any thinner and they flex on every peel and crack later.

Liquid only comes out if air can get in, so add at least two holes. Put one as close as possible to the end of the part nearest the plate; it also vents the suction cup while you print. Put the other far from it. Both go on faces nobody sees, plus one more wherever the slicer detects a suction cup.

Drain holes
Source Diameter Context
Formlabs, Form 3 / 3L guide ≥ 2.5 mm Enclosed cavities on that generation of machines
Formlabs, Form 4 guide ≥ 0.75 mm Tied to that machine and its process; do not carry it over to a home MSLA
Home MSLA practice 3–5 mm Starting point so viscous resin and isopropyl alcohol can flow
Count ≥ 2 per cavity One lets air in, the other lets liquid out

Resin sealed inside never cures, because light cannot reach it. It seeps out through micro-cracks for weeks. On top of that, trapped liquid, whether resin or alcohol from the wash, expands with the heat of post-curing and with temperature swings; together with the stresses in the cured shell, it cracks the part days later. Anyone who prints resin runs into it sooner or later, and it is the reason a closed cavity that causes no trouble in FDM (Lightweighting) ruins a resin part.

After printing, flush the cavity through the holes and let it dry completely before curing: alcohol left inside whitens and cracks the part during the cure. The procedure is in Washing and curing resin parts. If you want to plug the holes, print a short plug alongside the part and, with the cavity washed and dry, glue it in with a drop of resin and cure it. Wear nitrile gloves when you take the green part off the plate and off its supports; the rest is in Handling resin safely.

platesuctiontrapped liquidno holesplatedrain holesdrainedfilm
Machine view, halfway through printing a hollowed part; dashed, what has not printed yet. Without holes, the cavity open against the film traps liquid and pulls on the part with every lift. A hole at the end closest to the plate lets liquid in while you print; another at the opposite end lets you empty the cavity when washing.

Before you slice

Run through this with the part already oriented:

  • The show face looks toward the film, not the plate.
  • No large face sits parallel to the film (maximum peel) or nearly parallel (steps), except a reference face placed deliberately on the plate.
  • A 30–45° tilt on two axes, or a deliberate decision to print on the plate.
  • The island detector is clean, or every unsupported island has a reason.
  • Every cavity closed toward the plate is flipped or vented.
  • Hollowed part: walls of 2 mm or more and at least two drain holes on hidden faces.
  • Raft on, and thicker supports at the end closest to the plate.

When it fails

Orientation and support failures
Symptom Cause Fix
Nothing on the plate, a sheet on the film First layers or plate adhesion, not orientation Check the initial exposure and the leveling (How a resin printer works)
The part prints but a detail is missing, and there is a flake on the film Unsupported island Put a support on that tip; clean the vat before reprinting
The part breaks away from its supports mid-print Peel force Tilt more, thicken the supports, lower the lift speed, look for a suction cup
Burst wall or crater in a hollow part Suction cup Flip it, open a vent, add drain holes
Heavy layer lines on one face Face nearly parallel to the plate Make it parallel or clearly tilted
Cracks or seeping days later Trapped resin or alcohol, missing drains Open two holes per cavity, wash the inside and dry before curing

See also

Design it in KapyCAD

Design parts sized for your printer and your nozzle.

Free plan, no card. Runs in your browser, nothing to install.

Open the editor

Still have a question?