kapy academy

Lamp holders and shades

16 min readUpdated Nov 2026

In a lamp you almost never print the part that holds the bulb. You buy the lamp holder certified, in ceramic or thermoset, with its own terminals. What you print is everything around it: the shade, the body, the arm or the spotlight housing. So three numbers matter: the outer thread of the lamp holder, which takes the ring that clamps the shade; the hole in the shade that this thread passes through; and the distance from the bulb to the plastic, which is 30 mm at least.

Cap dimensions

Shops say "socket" or "fitting" for the whole assembly. The names below are the IEC terms: the cap is the bulb's base (E27, E14, GU10; "lamp base" in North America) and the lamp holder is the bought part it goes into. The shade ring screws onto the outside of the lamp holder, and the threaded tube is the hollow M10×1 tube that holds it all up.

Lamp caps and shade rings (mm)
Cap Region Thread or pins Pitch Typical bulbs Lamp holder's shade ring
E27 (Edison) Europe round Edison thread, nominal Ø 27 3.629 (7 threads per inch) A60 (Ø 60), G95 and G125 globes Ø ≈ 38–40, pitch ≈ 2–2.4: measure it
E14 (small Edison) Europe round Edison thread, nominal Ø 14 2.822 (9 threads per inch) C35 candle, P45 golf ball Ø ≈ 28, pitch ≈ 2: measure it
GU10 Europe, 230 V mains two mushroom-headed pins, 10 between centers; push in and twist ≈ ¼ turn — PAR16: Ø 50, length 53–55 none: a clip holds the bulb by its rim

Sources: IEC 60061-1, sheets 7004-21 (E27), 7004-23 (E14) and 7004-121 (GU10), as summarized on Wikipedia ("Edison screw" and the bi-pin lamp base table); Ledvance PAR16 GU10 datasheets for the bulb size. The shade ring figures come from rings on sale and community-shared models, not from a standard.

In the bulb code, the number is the diameter in millimeters: an A60 is 60 mm across. The 27 and 14 diameters are nominal. You do not need the real diameter of the cap thread, because the printed part never takes the bulb.

The threaded tube sits below the lamp holder. In Europe it is M10×1 (10 mm, fine 1 mm pitch) with two nuts. In North America it is 1/8 IPS, 27 threads per inch and ≈ 10.3 mm outside diameter. They look alike, but they do not interchange.

The standard fixes the cap so that any bulb fits any lamp holder. The outer thread of the lamp holder only has to match the rings from the same maker, and two E27 rings from different brands can differ by 1–2 mm in diameter, and in pitch too. That is why the table says "measure it": with a thread gauge, or by measuring ten pitches with callipers, from crest 1 to crest 11 (Measuring an undocumented standard).

CapE27Ø27Pitch 3.6297 threads per inchE14Ø14Pitch 2.8229 threads per inchGU10Ø50 face (PAR16)10PinsPush and twist ¼ turnLamp holderIEC 60061Shade ringØ≈38–40 · pitch: measure itShoulderM10×1 threaded tube10 mm
The IEC standard fixes the bulb's thread; the shade ring's thread is up to each maker, so measure it.

What fits what

  • E26 (North America, 26 mm) has the same pitch as E27, 7 threads per inch: an E26 bulb goes into an E27 lamp holder, and the other way round. The real incompatibility is the voltage: 120 V in North America, 230 V in Europe. The American E12 candle cap is not an E14.
  • The B22 bayonet (UK, Ireland, France and much of the Commonwealth) has two side pins: you push and twist. Its lamp holders and rings are a different size, so measure them.
  • You can buy E27 to E14 shade reducers, and they are among the most printed parts (see "What to print").
  • GU5.3 (MR16) runs at 12 V and has thin, straight pins, with the same 50 mm face as GU10. A housing designed for one takes the other's bulb, but not its lamp holder.

How a shade is held

The shade has a flat plate with a hole at its center, the shade flange. The lamp holder's outer thread passes through the flange, which ends up clamped between the lamp holder's shoulder (or a lower ring) and the shade ring. In a pendant, the shade hangs from the ring, which carries its weight. In a table lamp, the shade rests on the lower ring or the shoulder, and the top ring stops it lifting.

The flange hole has to slide over the crests, not bite into them. Hole = measured crest Ø + 0.40 (sliding fit, on the diameter; Real printed clearances) + shrinkage × D. At Ø 40, shrinkage adds ≈ 0.12 mm in PLA and 0.12–0.2 in PETG, so a crest of 39.5 gives a hole of ≈ 40.0–40.1 mm. Fine-tune it with a 2 mm test ring (Test coupons). Compensate holes in one place, the model or the slicer, never both (Why holes print small).

The flange thickness is limited by the free thread. Measure that thread and leave the ring at least three full turns of it: at a 2.2 pitch that is ≈ 7 mm. E27 lamp holders with a ring usually take shades a few millimeters thick, so a printed flange of 2–4 mm fits almost all of them; check the free thread on yours.

Where the flange sits relative to the bulb is what gets forgotten. On many lamp holders the outer thread is only at the mouth, on the bulb side, and the neck of an A60 sticks out a few millimeters from there. A flange clamped at the mouth will usually be less than 30 mm from the bulb, which is the distance the standard asks for (next section). You have two ways out:

  • A lamp holder with outer thread along the whole sleeve: the flange goes at the top, next to the shoulder, and you check that it is 30 mm or more from the bulb.
  • A bought metal flange or bracket (a brass or steel shade washer, or a wire shade carrier) that the ring clamps and that holds the printed shade 30 mm or more from the bulb.

If the printed flange still lands inside that band, you no longer meet the 30 mm rule. At the very least make it in ASA or PC, and the risk is yours.

The clamped flange gives way unless you protect it. In a pendant, the ring clamps it in the hottest spot: above the bulb, where the hot air rises. A clamped, warm plastic relaxes, and under load PLA works up to about 40 °C and PETG up to 50 (Creep and fatigue). Use PETG with low-power LEDs, and ASA or PC otherwise (ABS and ASA, Polycarbonate and its blends). Print the flange flat on the bed, so that the clamped face is a top or bottom layer. Tighten the ring by hand, never with a tool. Tie the flange to the wall with 3–4 radial ribs, so the weight does not hang from a single wall.

A printed shade ring, as a spare or a reducer, is an internal thread that screws onto a bought part of ≈ 28–40 mm. Open its diameter by 0.3 mm + shrinkage × D, which gives +0.4 at both Ø 40 and Ø 28. Print it with its axis vertical and flat on the bed, with 30° flanks (Modeling threads). Take the pitch from your lamp holder: get it wrong by 0.2 mm and the ring jams on the first turn.

Distance from the bulb and choice of plastic

The rule is 30 mm. The luminaire standard, in its 2015 edition with the 2018 amendment (EN 60598-1, clause 4.15), requires shades and covers that do not pass the 650 °C glow-wire test to be at least 30 mm from any hot part. The 2019 ETICS interpretation (DSH 0867A) counts every light source as a hot part, whatever its power. Assume your printed part has not passed that test, because nobody has tested it: leave 30 mm to the bulb surface all the way round. The IEC published edition 10.0 in November 2024, and the clause may carry a different number there.

The 30 mm keeps the material from burning, not from softening. The second check is temperature. Measure the hottest point of the shade after the lamp has been on for an hour, with a cheap thermocouple or an infrared thermometer on a matt patch (the method is in Heat, cold, sunlight and chemicals). A part near the bulb usually settles between 40 and 65 °C. Measure at the highest room temperature the lamp will see, or add the difference: in summer or close to the ceiling, the air can be 10–15 °C warmer than in your workshop. Under load, an unfilled part works up to about 15–20 °C below its HDT at 0.45 MPa (Heat, cold, sunlight and chemicals):

Service limit under load (°C)
Material HDT 0.45 MPa Service limit
PLA 57 ~40
PETG 69–71 ~50
ASA 100 ~80
PC 112–117 ~95

A shade that only carries its own weight works at very low load; the clamped flange does not.

Hot air rises, and that decides where to measure. In a pendant, with the bulb pointing down, it climbs toward the lamp holder and the flange: the top of the shade is the hottest part. In a table lamp, with the bulb pointing up, it escapes through the top opening; the lamp holder and the flange, below, stay cooler, and the top rim is what you measure. In both, leave the top open or vented: a closed shade traps the heat.

HottestMeasure herePendantOpenHot air30 mmMeasure hereTable lampOpenHot air30 mm
Hot air rises: in a pendant the flange heats up; in a table lamp, the top rim. Measure there after an hour with the bulb on.

By bulb, these figures are orders of magnitude; measure yours. LED efficiency keeps improving, so go by lumens, not watts:

  • LED A60, 806–1055 lm (≈ 4–11 W depending on efficiency, as of late 2026): the hottest part is the plastic or aluminum neck next to the cap, at ≈ 50–80 °C, and the globe is lukewarm. A PLA shade at 30 mm usually copes, but check the flange of a pendant.
  • GU10 LED: the whole body is a heat sink. Keep every printed part off it, and make the housing in ASA or PC.
  • 60 W incandescent: the glass goes above 100 °C. Capsule or reflector halogen: several hundred degrees; an A60-shaped halogen behaves like an incandescent. They are no longer sold in the EU, but they still turn up in drawers and second-hand lamps. With them, a PLA or PETG shade at 30 mm will not do; only a PC or flame-retardant one will, and even then the risk is yours.

A UL 94 V-0 rated filament gives margin, but UL 94 rates a specimen of a given thickness, not your shade, and it is not the glow-wire test (PPS, PEEK, PEKK and PEI): use it to gain margin, never to go below 30 mm.

For the light, PETG and PCTG let more through than PLA; a natural or milky grade, a textured wall or a single vase-mode wall diffuses it (Decorative filaments).

Example: pendant shade for an E27 lamp holder

The goal is a pendant shade 200 mm across at the mouth and 150 mm tall, for a bought thermoset E27 lamp holder with outer thread along the whole sleeve and two rings, and an 806 lm LED A60 bulb.

  1. Measure the lamp holder. Crest Ø of the outer thread: 39.5. Ten pitches (crest 1 to crest 11): 22 mm, so the pitch is 2.2. Threaded length, shoulder to mouth: 40 mm.
  2. Flange. The hole is 39.5 + 0.40 + 0.12 ≈ 40.0 mm; in PETG shrinkage can reach 0.2, and the test ring decides. The flange goes at the top, under the shoulder, 3 mm thick and Ø 80 outside, and the ring clamps it from below with ≈ 4 turns (9 mm of thread). Four radial ribs, 2 mm wide, tie it to the wall.
  3. Distance. The flange comes first: it sits ≈ 37 mm above the mouth, where the bulb's neck sticks out, so it clears the 30 mm. With thread only at the mouth, you would have needed a metal flange here. The A60 is Ø 60 and ≈ 105–110 mm long. With 30 mm all round, the shade's inside diameter at the bulb's widest point has to be ≥ 60 + 2 × 30 = 120 mm; this profile gives ≈ 150. Nor can the wall come closer than 30 mm to the neck as it narrows up toward the flange: here it stays at ≈ 35. The wall starts at the edge of the flange: with Ø 60 instead of 80, that start would sit closer than 30 mm to the neck. Check it in section, in the sketch (Revolve), not by eye.
  4. The wall. Revolve the profile and shell it (Revolve, Shell) with a 1.2 mm wall (3 lines) in PETG. Print the shade upside down, with the flange flat on the bed: the profile flares about 22° from vertical and prints without supports. Print it with the wide rim on the bed and the flange becomes an unsupported ceiling. The shade weighs about 110 g at 1.2 mm, or about 40 g in vase mode with the flange printed separately: the ring carries 0.4 to 1.1 N.
  5. A measurement decides the material. Print a PLA prototype, hang it with the bulb on for an hour and measure the flange and the hottest point of the wall. Correct the reading for the highest room temperature the lamp will see. Up to 35–40 °C, PLA will do; up to 50 °C, PETG; above that, ASA or PC. Write the reading down: fit a brighter bulb and you will have to repeat it.
Ø40.0 = 39.5 + 0.40 + 0.12Lamp holderFlange 3Shade ringRibThread 40 · ≥ 3 turns for the ringWall 1.2A60 Ø6030 mm bandBed
The thread passes through the flange without biting it and the ring clamps it; the wall and the flange stay outside the 30 mm band around the bulb.
Thermoset E27 lamp holder with its fine outer thread, two shade rings, a flange printed in translucent PETG and a threaded tube with its nut
Thermoset E27 lamp holder with its fine outer thread, two shade rings, a flange printed in translucent PETG and a threaded tube with its nut

What to print

  • Pendant and table lamp shades, like the one in the example.
  • E27 to E14 shade reducer: on the outside, the diameter of an E27 shade's hole; on the inside, a hole or a thread for the E14 lamp holder. The thread is internal and screws onto a bought part, so open it by +0.4.
  • Spare shade rings: thread opened by +0.4 and knurled on the outside for grip (Knobs, handles and grips).
  • Bodies and arms the M10×1 tube runs through: a through hole and two bought nuts. Do not print the M10×1 thread: 1 mm is the minimum printable pitch with a 0.4 nozzle (Modeling threads), right at the limit, and the nut carries the lamp. Buy the tube and the nuts. For switches and push buttons in the body, read Panel components.
  • GU10 spotlight housings: Ø 50 front opening plus clearance, a bought spring clip, ASA or PC and ventilation above the bulb.

When it fails

Symptom, cause and fix
Symptom Cause Fix
The ring will not start or jams on the first turn Its pitch is not the lamp holder's (there is no standard) Measure 10 pitches (11 crests) and remake it at that pitch; open +0.4 on Ø
The shade will not go over the thread or threads itself on Flange hole drawn at the nominal size Crest Ø + 0.4 + shrinkage; test ring
The shade turns or drops after a few weeks The clamped flange relaxes in the heat PETG or ASA, flange flat on the bed, ribs; retighten by hand
Soft, glossy or yellowed patch above the bulb Under 30 mm, or material above its limit More distance, an opening at the top, ASA or PC, or a lower-lumen LED
The shade cracks next to the flange The weight pulls on a single wall, across layers Radial ribs and 3 perimeters around the flange

How to test it

The ring goes on by hand and runs its 4 turns with no tight spots. Leave the lamp on for a week: the shade should not turn when you touch it, because the clamp has not relaxed, and there should be no soft or discolored patch at the top.

See also

Design it in KapyCAD

Draw the part to the standard's dimensions and keep them as values you can edit.

Free plan, no card. Runs in your browser, nothing to install.

Open the editor

Still have a question?