An accessory mounts on a bike in three places: the handlebar, the seatpost and the bottle-cage bolts, nearly always with a split clamp. A printed clamp only grips while its two halves are still apart: if they meet as you tighten, the bolt force stays in the ears and the light turns at the first bump. And one rule before you draw anything: print what hangs off the bike, never what holds up the rider. The stem, the handlebar, aero extensions, the seatpost clamp and the levers are bought ready-made, in metal.
Garmin and GoPro are trademarks of their respective owners; neither sponsors nor endorses this article.
The dimensions
| Mounting point | Diameter or thread | Where you find it |
|---|---|---|
| Handlebar, stem area | 25.4 mm | ISO size; older bars and many town bikes |
| Handlebar, stem area | 26.0 mm | Older road bikes (Italian size) |
| Handlebar, stem area | 31.8 mm | The usual size on road and mountain bikes |
| Handlebar, stem area | 35 mm | Current mountain bikes and some road bikes |
| Handlebar, grip area | 22.2 mm | Flat bars (mountain, town, BMX) |
| Handlebar, lever area | 23.8 mm | Road (drop) bars |
| Seatpost | 27.2 mm | Road, classic frames |
| Seatpost | 30.9 and 31.6 mm | Mountain, many dropper posts |
| Seatpost | 34.9 mm | Recent dropper posts, increasingly common |
| Bottle-cage bosses | Two M5 × 0.8 threads, 64 mm between centers | Down tube and seat tube |
Sources: Sheldon Brown's handlebar and seatpost tables; handlebar and stem guides from trade retailers and magazines (35 mm); Park Tool and Wolf Tooth's product sheets (bottle bosses at 64 mm); 2025 dropper-post guides from evo, BikeRadar and Singletracks (34.9 mm).
The handlebar only steps up to 31.8 or 35 mm in the center, where the stem clamps it and where the bending moment is highest; toward the grips and levers it narrows to 22.2 or 23.8. That thick section is short: measure the usable length left once the stem, the cables and the computer mount are on. On many road bars the tops are a flattened aero profile, and integrated cockpits (bar and stem in one piece, cables routed inside), widespread by late 2026, leave even less room.
Measure with callipers at the exact spot the clamp will sit, two readings at 90°: a painted tube does not come out at its nominal size, and you never measure or clamp over bar tape (Measuring an undocumented standard).
On the seatpost, the rear light and the saddlebag bracket go on the round section left visible between the seat clamp and the saddle. The D-shaped or proprietary posts of aero bikes take no round clamp: use the manufacturer's mount or the saddle rails. Fork legs, stays or a carbon top tube are not mounting points either unless the frame manual says so: a thin-walled carbon tube is not designed for the concentrated squeeze of a clamp.
The clamp that does not turn
Make two halves with two bolts. A one-piece 31.8 C would have to open so far to pass over the bar that the strain would be well beyond the 1–1.5 % PLA tolerates in repeated bending, and sliding it on from the end means stripping off grips and levers.
Draw the bore at the measured bar diameter, with no clearance: the halves must touch the tube before they touch each other. Apply your printer's hole compensation so the ring bears around the whole arc and not only on the edges next to the split (Why holes print small); if it still comes out a tenth under, you are on the safe side. Do not add a sliding-fit clearance: that is for parts that turn or slide.
Leave a gap g of 1.5–2 mm at each split. It is the reserve that absorbs the deviation of the real bar, the error of the printed hole and how much the liner compresses: as you tighten, the halves close by up to g along the bolts and, if the ring flexes, the diameter drops by 2g/π, about 1.3 mm with g = 2. If the gap disappears when you tighten, the clamp has bottomed out and is holding nothing.
The values in this section are practice, not a standard:
- Width: at least 15 mm along the bar, with a 0.5 mm chamfer on the bore edges. A narrow ring or a sharp edge concentrates the pressure on a line that bites into the paint and, on carbon, crushes the fibers; the width also stops the clamp rocking.
- Liner: a 1 mm TPU liner, or the rubber shim that comes with lights, grips better than bare plastic. Draw the bore two liner thicknesses larger: 33.8 mm for a 31.8 bar (TPU and flexible filaments).
- Shims: to make one clamp fit several bars, draw the bore for 35 or 31.8 and print shims of thickness (D_bore − D_tube)/2: from 31.8 to 25.4 that is 3.2 mm; from 31.8 to 22.2, 4.8 mm; from 35 to 31.8, 1.6 mm. Split them in two and key them in with a tab so they do not turn inside.
- Bolts: M4 or M5 through the ears, with a captive nut or heat-set insert in the other half and a washer under the head (Captive nuts and clearance holes). Between the hole and the edge of the ear, at least one bolt diameter of material.
Tighten until the clamp will not turn by hand, then stop: the gap must still be visible, and 0.5–1 N·m is enough. Leaning on the key gets you to 1–2 N·m, which crushes the plastic under the washer and closes the gap.
Print each half lying flat, with the bore axis vertical, so the beads run around the ring within each layer (Layer orientation for mechanisms). Cup-up, with the axis horizontal, the crown and the ears are built layer on layer and the first time you tighten hard the part splits along a layer. Lying flat, the bolt holes end up horizontal, and M4 and M5 clearance holes are below the 6 mm that print clean.
Worked example: does it turn over a bump?
This is an order-of-magnitude sum to see which way it falls; the bump acceleration, the torque coefficient and the friction are estimates, not datasheet values.
A 150 g light on a forward arm, with its center of mass 80 mm ahead of the bar axis. A bump can give the bar an acceleration of about 10 g, the same as in GoPro-compatible mounts. The bump force is F_b = 0.15 × 9.81 × 10 ≈ 15 N, and the moment trying to turn the clamp is M = 15 N × 80 mm ≈ 1.2 N·m.
An M5 tightened with a short hex key until it will not turn by hand ends up at about 0.5 N·m. With T_a ≈ 0.2 · F · d (torque coefficient K ≈ 0.2, dry steel), each bolt clamps with F ≈ 0.5 / (0.2 × 0.005) = 500 N. Spread under an M5 washer (about 55 mm² of plastic), that is ≈ 9 MPa: the plastic takes it, but it is the stress that relaxes over a summer.
Two rigid halves clamped with F on each side resist turning up to T_d ≈ 2.5 · μ · F · D (cosine pressure distribution, total normal force ≈ 16F/π). There is no published friction value for plastic on paint or anodized aluminum: start from μ ≈ 0.25, the value for printed plastic on steel, and measure it (Friction and wear). T_d ≈ 2.5 × 0.25 × 500 × 0.0318 ≈ 10 N·m.
Ten against 1.2: a margin of about eight to one. Even if a summer's heat halves the clamp force, 5 N·m remain, four times the load. On a mountain bike or a fully rigid bike, allow for twice the bump: with full clamp force there is still plenty to spare; with the clamp force relaxed to half you are cutting it fine, and that decides the material.
So a printed clamp that turns is almost never short of bolt or of friction, but of contact. If the halves bottom out, the force reaching the tube drops to nearly zero, especially if you drew clearance, and the slip torque drops with it.
The moment grows in proportion to the arm: at 160 mm it doubles and there is still margin. With something heavy at the end of a long arm, a 400 g light or a phone, the problem becomes rocking and arm flex: widen the clamp and stiffen the arm (Ribs, gussets and fillets).
The bottle-cage bolts
They are two M5 × 0.8 threads at 64 mm: rivet nuts in aluminum frames, metal inserts bonded into carbon ones and brazed bosses in steel ones. They sit on the down tube and the seat tube, and many gravel and touring frames add more under the down tube, on the top tube and on the fork, nearly always at 64 mm between each pair; there is no written standard, so measure them. It is the firmest mounting point on the bike, a metal thread with nothing to slip: it takes pump, tool, lock or battery mounts, and adapters that move the bottle cage up or down.
Draw the M5 clearance holes at 5.5 mm (ISO 273 medium series) and add the hole compensation. Turn one into a slot of ±1.5 mm along the tube: frames stray from 64, which is why cage makers already slot one hole.
The adapter adds its thickness under the head: use an M5 that much longer, and check it does not hit bottom inside the tube, because then the head stops clamping and the adapter rattles. Here the frame's thread sets the limit: frame makers give 2–5 N·m for these bolts, and on carbon it is usually 2–3 N·m; check the manual. Overdo it and the insert spins in the frame, and the bike goes to the shop. Fit a washer and retighten after the first few rides.
Which material
Handlebar in the sun: ASA as the default and PC for the most demanding clamp; PETG only for parts in the shade or the turbo-trainer bike, and PLA for test-fitting. A clamp's squeeze is a sustained load, and in PLA or PETG in the sun it relaxes (Creep and fatigue, Heat, cold, sunlight and chemicals). For a long forward arm, PET-CF adds stiffness, but the ears and any tab that works in bending go in ASA or PC: fiber-filled filaments take less repeated strain than PLA.
When it fails
| Symptom | Cause | Fix |
|---|---|---|
| Turns at the first bump with the bolts tight | The halves bottom out; bore drawn with clearance | Bore = bar; 1.5–2 mm of gap visible after tightening |
| Turns after a few weeks or after a hot day | The clamp force has relaxed (PLA or PETG in the sun) | ASA or PC, washer, retighten after the first rides |
| Washer imprint, crushed ear | Too much torque | Wide washer; tighten until it will not turn by hand, then stop |
| Splits along a layer at the crown or ear when tightened | Printed with the bore axis horizontal | Flat, axis vertical |
| The ear breaks through the bolt hole | Hole too close to the edge, thin ear | One bolt diameter of wall; insert or captive nut |
| Marks or rings in the paint or carbon | Narrow ring, sharp edge, grit, slow slipping | ≥ 15 mm wide, 0.5 chamfer, TPU or rubber liner, clean tube |
| The bottle-cage adapter does not line up with the frame holes | Holes too small or frame not exactly 64 | 5.5 + compensation and a slot |
| The bottle-cage bolt spins without tightening | Insert loosened by over-torque | Stop tightening; take it to a bike shop |
| The bolt is home but the adapter rattles | The bolt bottoms out inside the tube | Shorter bolt, at the manual's torque (2–5 N·m) |
How to test it
Before the whole clamp, print a 10 mm slice of the ring in its final orientation and tighten it on the bar: the gap must still be there (Test coupons).
With the clamp fitted, draw a marker line across clamp and bar. On the workbench, hang a spring balance or a luggage scale from the end of the arm and pull to twice the bump moment: 2 × 1.2 N·m at 80 mm is ≈ 30 N, about 3 kg on the scale. The line must not move; repeat after 48 h, and look again after a ride and after a hot day. The method for sustained and stepped loads is in Estimating whether a part will hold.
See also
- Garmin-compatible quarter-turn mounts: the cradle that goes on the bike computer's clamp.
- Phone mounts: which phone system to print and which to buy for the handlebar.
- GoPro-compatible mounts: the action camera's fingers and their bolt.
- Creep and fatigue: why a clamp's squeeze relaxes in the sun.