kapy academy

Designing for an ecosystem

14 min readUpdated Nov 2026

You are about to print one half of a joint whose other half someone else designed: a bin for the Gridfinity baseplate you downloaded from another maker, a hook for the IKEA Skådis board, a part that has to fit an injection-molded plastic brick. You cannot change their half. Three questions decide whether yours fits and whether you may share it: who made the other half, how far apart the features are, and what the license and the trademark allow. On top of that, every hook or wall mount follows four shared rules.

Who made the other half

Clearance exists to absorb error. Where it goes depends on how many printed parts are in the joint and who printed them.

  • You printed both halves. Your bin in your baseplate, on the same machine and in the same material. The standard's author already designed the gap for two printed parts. Print at nominal size on a calibrated machine.
  • A bought part: molded, punched or machined. The Skådis board, a pegboard, a jar, a 2020 extrusion. Its feature is at nominal size and carries no printer error. All the clearance goes on your part.
  • One half printed by someone else, on a machine you will never see. The two errors add up. That is why ecosystems build the gap into the design itself instead of publishing a tolerance, and that gap is only enough if both machines are calibrated.
Printed + printed by you, same standardPitch 42Bin 41.5The gap is in the standard: 0.25 per sideCalibrate and print at nominal sizePrinted + bought partTab 4.6NominalSlot 5Board at nominal size: all the clearance onyour part (−0.4)Printed + printed by someone elseThe two errors add up: it only fits if bothmachines are calibrated
Who made the other half decides where the clearance goes: in the standard, on your part, or shared between two calibrated machines.

So the rule is: an ecosystem of downloadable designs is printed at its nominal dimensions on a calibrated machine. If it does not fit, calibrate the machine, not the standard.

The standard already carries its clearance

Gridfinity shows it in numbers. The grid pitch is 42 mm and the footprint of a one-cell bin is 41.5 mm; an N-cell bin measures N × 42 − 0.5. That is 0.5 mm of gap across the width, 0.25 per side, whatever the size, and it is already in the specification. That is the free-running fit of a modern machine (0.25–0.30 mm per side). There is nothing to add.

Check it against real error. A modern bedslinger holds ±0.1–0.15 mm per part in XY. If the bin comes out 0.15 wider and the socket 0.15 narrower, they eat 0.30 of the 0.50 mm gap across the width and the bin still goes in. A legacy bedslinger, at ±0.2–0.3 per part, adds up to 0.4–0.6: it eats nearly all of the gap or more.

Add 0.3–0.4 mm per side "in case" and your bins rattle in other people's baseplates and theirs in yours. What a standard gives you is compatibility, and extra clearance breaks it.

When a downloaded part goes in too tight, print the ecosystem's own test piece or a clearance coupon and measure. Find out whether it is a scale error (long dimensions are off by a percentage) or a constant error (every edge is off by the same amount), correct it in the slicer profile and print again. The procedure is in Dimensional calibration, how to tell the two errors apart in Parts that print the wrong size, and the sequence in What to calibrate, and in what order.

Ecosystem holes are no exception: a small vertical hole prints 0.1–0.3 mm tight on the diameter because of facets, the bead bulging into the curve and shrinkage (Why holes print small).

Against a bought part, all the clearance goes on yours

A punched, drilled or molded hole is at nominal size. Only your part carries error, and printed pegs come out at size or slightly fat. So the whole fit clearance comes off your part.

Your printed part against a bought part
Bought part What you print Why
5 mm slot (Skådis) or 5 mm hole (System 32) 4.6 mm peg (hole − 0.4) sliding fit: goes in and out by hand
The same hole, a peg that must stay put 4.8 mm friction fit
1/4″ pegboard (6.35) 5.95 mm peg hole − 0.4
3/16″ pegboard (4.76) 4.35 mm peg hole − 0.4
Jar, PET bottle or hose thread, Ø ≥ 30 mm internal thread diameter + 0.3 mm + shrinkage × D PLA ≈ 0.3 %: Ø70 → +0.5
Metal screw or nut 0.2–0.3 mm less on your screw, or more on your nut's bore only the printed part shrinks

Picking the type of fit is covered in Choosing the fit: clearance, transition, interference, and threads in Modeling threads.

Pitch error grows with length

Grids are pitch standards: Gridfinity 42 mm, openGrid 28, Multiboard 25, Skådis 40, HSW 40.88. Shrinkage is an error proportional to length, independent of each feature's own ±, and it grows along a long part.

Take a Skådis accessory with tabs in five slots of one row: it spans 4 × 40 = 160 mm. PLA shrinks by 0.2 to 0.5 %. At an uncalibrated 0.3 %, the distance between the end tabs comes out 0.48 mm shorter than between their slots, because the board does not shrink. A sliding tab has 0.2 mm per side, so the two end tabs together tolerate 0.40 mm of offset. 0.48 is more than that: the end tabs rub on their inner sides and the accessory will not go in. At 0.5 % it is 0.80 mm, twice what fits.

A five-tab accessory on a 40 mm pitch, seen from the front in its board's slots, shrinking toward its middle tab. Top, the board is printed too and shrinks with it: the slots follow the tabs. Bottom, the board does not shrink: at 0.3 % the end tabs are 0.48 mm off against 0.40 of play and rub on the inside; at 0.5 %, 0.80 mm
Shrinkage and play drawn ten times larger. Two printed parts shrink together and their features stay aligned; against a board that does not shrink, the whole pitch error lands on the joint and grows with length: over 160 mm, 0.3 % is 0.48 mm, more than the 0.40 of play in the end tabs. The fix: one feature sets the position and the rest have play along the row.

The fix follows an order, explained in Assemblies and tolerance stackups. First calibrate each filament's shrinkage in the slicer profile, never by scaling the model. Then let a single feature set the position and give the others play in the direction of the pattern: slots, or tabs made narrower along the row.

Between parts printed in the same material and the same orientation, both grids shrink together and the error almost cancels. Mix materials and that cancellation is lost. PETG shrinks around 0.3–0.5 % and ABS 0.5–0.8 %: about 0.3 percentage points apart. What counts is the distance between the feet, because each one seats in its own socket: the end feet of a four-cell bin are 3 × 42 = 126 mm apart, and 0.3 points is 0.38 mm, 0.19 at each end, three quarters of Gridfinity's 0.25 per side before either machine's error is added. The same happens with a large baseplate printed in sections on different printers.

Rules shared by hooks and wall mounts

These hold for any hook, bracket or wall accessory.

  • Material. At room temperature, PLA holds a light sustained load about as well as PETG: no reliable data on printed parts says which creeps more. PETG only wins when the part gets warm. For a sustained load, use PC or ASA, or a fiber-filled filament if the part is not a spring (Creep and fatigue). Under load, an amorphous plastic works up to about 15–20 °C below its HDT at 0.45 MPa: PLA about 40 °C, PETG 50, ASA 80–85 (Heat, cold, sunlight and chemicals).
  • Orienting whatever flexes. A tab, a clip or a hook's lip prints with its length in the layer plane, lying flat (stance A) or on edge (stance B), never standing up (stance C) (Layer orientation for mechanisms).
  • Loads across layers. For design, assume the part is half as strong in Z as in XY, or 30 % if the material is fiber-filled, and orient it so the main load runs along the beads (Layer adhesion and anisotropy). A hook printed standing up loads its lip across the layers; print it on its side, with the hook's profile in the layer plane.
  • Threads. Vertical axis and a pitch of 1 mm or more. Where the standard calls for a metal thread (a tripod's 1/4″-20, a VESA mount's M4), fit a heat-set insert, not a printed thread. The pocket dimensions are in Designing for heat-set inserts.

Licenses: what you may do with what you download

Keep two things apart. The interface is the dimensions that guarantee the fit: the pitch, the slot width, the thread. The files are the STL, the STEP, the drawings and the generator's code. A dimension read from a published specification, or taken with callipers, is a fact; drawing your own geometry from it is not remixing anyone's file. Files, on the other hand, are someone's work and carry a license: before you remix or sell, read the license of every file you start from on the page where you downloaded it.

This is guidance, not legal advice. Some interfaces are also covered by other rights: in the EU, the connecting parts of a modular system can be protected as a design (Art. 8(3) of the EU Design Regulation, as amended by Regulation (EU) 2024/2822).

What the most common licenses allow
License Print for yourself Share a modified file Sell prints
CC0 (public domain) yes yes, no conditions yes, no conditions
CC BY yes yes, crediting the author yes, crediting the author
CC BY-SA yes yes, under the same license yes, crediting the author
CC BY-NC / BY-NC-SA yes yes (NC-SA: under the same license), no commercial use no
CC BY-ND yes no yes, unmodified
MIT yes yes, keeping the notice yes

ND allows modifying for your own use, not sharing the modified version.

This is where the licenses of these ecosystems stand as of November 2026. openGrid is published under CC BY 4.0. For Gridfinity, the specification drawing on gridfinity.xyz carries CC BY-NC-SA, but each remix and each generator carries its own, so what counts is the license of the file you downloaded. Multiboard is a Keep Making design with its own license, free for personal use; for any other use, read its terms at multibuild.io/community-promise and in Multiboard: the wall of anchor points.

Platforms add licenses of their own. Many MakerWorld models carry MakerWorld's standard digital file license, meant for printing for yourself and not allowing remixes; others carry a Creative Commons one. Printables offers Creative Commons variants and a few other licenses. On both, what counts is the license shown on the model's page.

What you draw in KapyCAD from published dimensions is yours. If you started from someone else's STL or STEP, your file inherits its license.

For power-tool batteries, stay with holders and wall mounts: a printed electrical adapter between batteries and tools is a safety and liability risk. The holders are in Power-tool battery mounts.

diagram
Before you share or sell, ask where your geometry comes from: from dimensions or from someone else's file.

How to name the brands

The brand qualifies the product's generic name; it never replaces it. Write "LEGO-compatible parts", "accessories for the IKEA Skådis", "GoPro-compatible mount"; never "a LEGO" or "a skadis". Their owners ask for it, and it makes clear the use is purely descriptive.

Say what fits, not who approves it. Put "compatible with" or "for" in the title and once in the text, and add a non-affiliation line:

X is a trademark of Y. This part is not made, sponsored or endorsed by Y.

In Spanish: «X es una marca de Y. Esta pieza no está fabricada, patrocinada ni aprobada por Y.»

No logos, no brand typefaces, no product names embossed on the part, and do not call your file "official". Gridfinity and openGrid are community projects; Multiboard is a Keep Making product. All three have authors: credit them as their license asks.

When it fails

Symptom, cause and fix
Symptom Cause Fix
A downloaded bin jams in a downloaded baseplate uncalibrated machine or over-extrusion: fat parts, narrow sockets calibrate flow and shrinkage, print the standard's test piece; do not edit the file
The bin rattles one half scaled or given extra clearance, or materials with different shrinkage both halves at nominal size, in the same material or with shrinkage calibrated
The bin rocks or does not seat in every cell warped baseplate that does not sit flat improve bed adhesion or print the baseplate in sections
The peg will not go into a bought board you drew it at the hole's nominal size peg = hole − 0.4
The end tabs clash while the middle ones go in scale error along the pitch calibrate shrinkage; give every tab but one play
A hook opens up over the weeks PLA or PETG under sustained load, or warm PC, ASA or fiber-filled, thicker root
A clip snaps at the root on first use printed standing up, length in Z reprint it lying flat or on edge

How to test it

Before printing the full assembly, test a single grid cell or one tab in its slot: in ten minutes you will learn what the assembly would tell you in ten hours. Test coupons shows how to design that minimal piece.

See also

Design it in KapyCAD

Draw the part to the standard's dimensions and keep them as values you can edit.

Free plan, no card. Runs in your browser, nothing to install.

Open the editor

Still have a question?