Euro stacking boxes (Eurobox; KLT in the automotive trade) are boxes in polypropylene (PP) or high-density polyethylene (HDPE) whose outside footprint is a fraction of the 1200 × 800 mm Euro pallet: 600 × 400, 400 × 300 and 300 × 200. Nobody fixes the inside: two 600 × 400 boxes from different makers can differ inside by more than 25 mm, from 544 × 364 to 570 × 370. You size an insert from what you measure in your box, not from the footprint. KapyCAD is not affiliated with the manufacturers named or with Gridfinity.
What the standard fixes
| Item | Value |
|---|---|
| Nominal footprints | 600 × 400 · 400 × 300 · 300 × 200 (800 × 600 also exists) |
| Boxes per layer on a 1200 × 800 pallet | 4 of 600 × 400 or 8 of 400 × 300, and they can be mixed in the same layer |
| Actual outside on some boxes | ≈ 594 × 396 · 396 × 297 · 297 × 198 |
| Common heights | 147.5 and 280 overall; in a stack each adds 132.5 and 265 (15 overlap) |
| Heights in one commercial range (WERIT) | 120 / 170 / 220 / 270 / 320 |
| KLT heights (VDA 4500) | 120 / 147 / 174 / 213 / 280 |
Sources: the Wikipedia article "Euro container" and the WERIT catalog, checked in late 2026. The standards are DIN EN 13199 (small load carriers), DIN 30820 (Euro stacking containers) and VDA 4500 (KLT). They fix the footprint and the stacking interface; the inside dimensions and the rated load come from each maker's datasheet. Shops also sell 200 × 150 boxes, but none of these standards appears to include them. Two boxes of the same footprint from different brands usually stack, but it is not guaranteed: test a pair before you buy twenty.
| Box | Inside |
|---|---|
| 600 × 400 (Wikipedia table) | 544 × 364 |
| 600 × 400 × 125 (Transoplast) | 560 × 360 × 114 |
| 600 × 400 × 235 (Transoplast) | 555 × 355 × 220 |
| 600 × 400 × 330 (Rotom) | 569 × 366 × 310 |
| 600 × 400 × 220 (Auer EG 64/22) | 570 × 370 × 215; usable stacked height: 203 |
| 400 × 300 (Wikipedia) | 346 × 265 |
| 300 × 200 (Wikipedia) | 243 × 162 |
The inside varies this much because the stacking interface fixes only the outside and the rim. The rest is the maker's choice: wall thickness, ribs, draft angle (the walls taper toward the base so the box releases from the mold) and the radius between floor and wall. Datasheets usually quote the inside dimension at the rim, which is the largest; at the floor the box is narrower.
The four dimensions you measure yourself
- Inside length and width at the floor. Measure at both ends and in the middle; keep the smallest.
- The same dimensions at the height the insert reaches. Because of the draft, they will be larger.
- The floor-to-wall radius. Use a radius gauge, or set a coin or the shank of a drill bit in the corner and compare the curve.
- The usable stacked height. It is the distance from the floor to the lowest point of the box above, whose foot drops into the rim of the box below. Some datasheets give it: the Auer EG 64/22 has 215 mm of inside height and 203 of usable stacked height. The foot of the box above takes 12 mm.
Also note everything the insert has to clear: handles that protrude inwards, label holders, drain holes and ribs on the floor. Measure the box you own. If you change batch or maker, even for "the same" model, measure again. Measuring an undocumented standard covers measuring with callipers and repeating the reading; the box is a part someone else designed, and Designing for an ecosystem covers how to treat it as one.
Nothing printed rises above the usable stacked height. If it does, the box above rests on the insert and the whole load of the stack, which datasheets put at hundreds of kilos, goes through printed walls instead of the box's molded ones. That load, not what you store inside, is what crushes the insert or makes it creep.
Nothing rests on the rim either: that is where the foot of the box above sits; a tray hanging from the rim on tabs lifts the stack. You can only hang a tray if your box has a molded ledge for it, inside and below the rim.
Leave 1 to 2 mm of clearance per side, taken from the smallest inside dimension at the floor. An insert is not a press fit: it has to go in and come out with the box full. When you lift the box by its handles, the floor sags and the long walls lean inwards, squeezing whatever sits between them. An insert jammed wall to wall takes that squeeze. PLA shrinkage (0.2–0.5 %) shifts the final length of a 550 mm insert by 1.1 to 2.8 mm (Shrinkage and dimensional stability); that is why the full-length test strip comes before the insert. If you lay several parts in a row, their errors add up (Assemblies and tolerance stackups). Chamfer the bottom edges with a chamfer no smaller than the floor radius: the insert then sits flat instead of riding up on the curve.
Example: a Gridfinity-compatible floor for a 600 × 400 box
Take the Auer from the table: 600 × 400 × 220, with 203 mm of usable stacked height. Assume the floor measures 556 × 356 and the radius about 3 mm.
- Available space, at 1.5 mm per side: 556 − 3 = 553 and 356 − 3 = 353.
- Cells: ⌊553 / 42⌋ = 13 cells (546 mm) and ⌊353 / 42⌋ = 8 cells (336 mm). That is 104 cells.
- Leftover: 5 mm at each end along the length and 10 on each side across the width.
Fill both directions down to 1.5 mm per side, like any insert: printed strips of about 8.5 mm along the long sides and about 3.5 mm along the short ones, or a border that wide on the end tiles. With that play, loose tiles would drift apart at the joints, the 42 mm pitch would break and a multi-cell bin straddling a joint would no longer seat: join the tiles to each other (Splitting large parts).
Run the same numbers on the box with the smallest inside in the table (544 × 364, and that at the rim): 13 cells no longer fit and the grid drops to 12 × 8. That is why you measure. The dimensions of the cell, the foot and the lip are in Gridfinity: the 42 mm grid.
A 546 × 336 grid does not fit a 256 × 256 bed, a common size. The largest tile that fits has ⌊256 / 42⌋ = 6 cells (252 mm). Split the 13 columns into 5 + 4 + 4 and the 8 rows into 4 + 4: that gives six tiles, two of 210 × 168 and four of 168 × 168, which also fit a 250 × 210 bed. Always cut along the line between cells so the sockets come out whole, and join the tiles with a dovetail or a clip at each joint.
In height, a bin of U units stands 7·U + 4.4 mm to the lip (7 mm per unit). On the baseplate its foot sits a few tenths above the underside of the plate, so the lip ends up about 7·U + 5 mm above the floor. Keep 2 mm of margin below the 203: 7·U + 5 ≤ 201, so U ≤ 28. In a box 120 tall, with about 100 mm of usable stacked height (measure it: no datasheet gives it), the maximum drops to 13 U.
By the same method, a 400 × 300 takes 8 × 6 cells (336 × 252) if its floor measures at least 339 × 255; with the datasheet's 346 × 265 measured at the rim, the margin is 5 mm per side and the draft can eat it. On a 256 bed that is two 4 × 6 tiles; on a 250 × 210, four of 4 × 3. A 300 × 200 takes 5 × 3 cells (210 × 126) if its floor measures at least 213 × 129, but over 30 mm is left in each direction: there a custom tray pays off better.
Half-lap dividers
If you store large, light, irregular things (cables, bags, tools), use a half-lap divider grid. If they are small parts you reach for often, use bins on a Gridfinity-compatible floor: the bins themselves act as dividers.
- Thickness t: 1.6 to 2.0 mm, that is 8–10 layers of 0.2 with the strip lying flat. With 4–5 solid layers top and bottom it prints solid with no infill (Walls, perimeters and infill). A squashed first layer changes it: measure the printed t before you fix the slot.
- Slot: t + 2 × your sliding clearance, about 0.2 mm per side on a current printer (Real printed clearances gives the value for each class of machine). It goes together and comes apart by hand. Depth: half the strip height.
- Strip height: at most the usable stacked height less 2 mm.
- Length: the floor dimension in that direction, less 1–2 mm per side, never the rim dimension. A strip that touches both walls at the rim does not reach the floor. One cut to the floor leaves a few millimeters of gap at the top, with no consequence: the crossed strips lock each other and the walls only stop the grid from shifting. If things slip through that gap, bevel the ends at the draft angle you measured.
A 556 mm strip does not fit a 256 bed. Split it at a crossing so the joint hides in the half lap, or join two lengths with a dovetail (Printed dovetails and joinery). Print the strips lying flat, never on edge. Flat, the whole strip flexes along the extrusion lines and the slots come out accurate in XY. On edge, the tongues on either side of a slot flex across the layers when the crossing strip pushes them, and they snap along a layer line (Layer orientation for mechanisms). And a 2 mm wall 200 mm tall prints badly anyway.
Do not glue anything to the box: almost no adhesive holds on PP or HDPE (Polypropylene). Locate by shape instead: stops, interlocks or the wall itself.
How much the base will hold
According to the datasheets of several retailers (toom, Mercateo and 1a-topstore), each box is rated for 40 to 70 kg, and the stack, static, for 200 kg in the standard range up to 700 kg with a reinforced base. Trust only the datasheet for your exact part number.
Before you fill a box, do the math. A 600 × 400 × 120 filled with screws to 100 mm holds about 20 L (560 × 360 × 100 mm). Loose screws weigh about 3–4 kg per liter (steel at 7.85 g/cm³ with a 40–50 % packing fraction): 60–80 kg. That exceeds what almost all of these boxes are rated for, and it is 2.4 to 3.2 times the 25 kg that ISO 11228-1 takes as the reference for manual lifting. Keep hardware in low boxes or small footprints (400 × 300, 300 × 200) and leave the tall 600 × 400s for bulky, light things.
A grid floor or a tray spreads the load; legs concentrate it. An insert on four legs puts the whole contents on four points of a floor designed for distributed load: give each leg a wide pad or let the insert sit flat.
If the insert carries weight continuously somewhere hot (a van, a loft in summer), it creeps: under a sustained load, PLA is only comfortable below about 30 °C and its limit under load is around 40 °C; PETG's is around 50 °C (Creep and fatigue). Above that, use ASA or PC.
When it fails
| Symptom | Cause | Fix |
|---|---|---|
| The insert rocks or sits high on one side | It rests on the floor radius | Bottom chamfer ≥ measured radius |
| It goes in at the rim and jams before the bottom | Sized from the datasheet dimension (at the rim) | Resize it from the floor dimension |
| The box above rocks or does not seat | Insert or bins above the usable height, or tabs on the rim | Cut it down to 2 mm below the usable height and remove the tabs |
| The grid slides or opens at the joints | Leftover not filled in one direction | Filler strips in both directions and tiles joined to each other |
| Parts that fitted rattle in another box | Different maker or batch | Measure that box |
| The insert cracks or bows after weeks loaded in the heat | Creep and flexing of the box | A base that rests on the whole floor, ASA or PC if it is hot (PETG only up to about 50 °C), 1–2 mm per side |
How to test it
Before you spend 2 kg of filament, print a test corner of the insert, about 60 × 60 mm, with the full base height, the bottom chamfer and the radius. Try it in every corner of the box: it has to sit flat and leave the intended gap against both walls. Then print the filler strip or the longest divider at its real length and lay it in the box. That checks shrinkage and shows whether the box narrows in the middle (Test coupons).
See also
- Gridfinity: the 42 mm grid: the dimensions of the foot, the socket and the lip the example uses.
- Accessories for IKEA Trofast: if your boxes are the tubs from that unit rather than Euro boxes.
- Modular tool cases: inserts for branded stackable cases.