The miniature itself is usually resin. What you print in FDM around it is a different job: the base, the magnet that holds it in the case and the tray that moves twenty of them at once. In almost every tabletop wargame the base is part of the rules: distances and contact are measured from its edge, so its footprint is set by the game's publisher. No rulebook sets the height, the bevel or the underside: you copy those from a bought base or choose them yourself.
Base sizes
| Shape | Sizes (mm) | Where they are used | Note |
|---|---|---|---|
| Round | 25, 28.5, 32, 40, 50, 60, 80, 90, 100, 130, 160 | Games Workshop games (Warhammer 40,000, Age of Sigmar) | 32 replaced 25 for much of the infantry; 28.5 is old but still in use |
| Oval | 60 × 35, 75 × 42, 90 × 52, 105 × 70, 120 × 92, 150 × 95, 170 × 105 | The same games | Some shops also sell 75 × 46 and 170 × 109: check the box |
| Square and rectangular | 25, 30, 40, 50; cavalry 25 × 50 and 30 × 60 | Warhammer: The Old World (2024) | Infantry moved from 20 to 25 mm |
| Square | 20, 25, 40, 50 | Kings of War | What counts is the footprint of the whole unit, not of each base |
| Round | 27, 50, 70, 100 | Star Wars: Legion | Some variants have notches |
| Role-playing grid | 25.4 square (5 feet in game); bases 25, 50, 75, 100 | Dungeons & Dragons and most role-playing games | Small and Medium 25, Large 50, Huge 75, Gargantuan 100 |
Sources: the size guide on spikeybits.com (Warhammer 40,000 and Age of Sigmar), the table on themagnetbaron.com, the litko.net guides for The Old World, Kings of War and Star Wars: Legion, and the warhammer.com page for the 25 × 50 base pack (2024). They are compiled from each publisher's datasheets: your unit's datasheet in the current edition is what counts, and any new edition can change sizes.
The role-playing grid has some slack: a 25 mm base in a 25.4 square leaves 0.4 mm, 0.2 per side. Large creatures take several squares (Huge, 3 × 3 = 76.2; Gargantuan, 4 × 4 = 101.6), so the 75 and 100 bases fit with even more margin (0.6 and 0.8 mm per side). If you print map tiles, draw the square at 25.4 and the bases will fit.
The table has no heights or undersides because no publisher gives them. Bought round bases are around 4 mm tall, with a beveled side and a hollow underside; for some of The Old World squares, thicknesses of 2.2 and 2.6 mm circulate, measured by players, not published. Take a bought base from your army and measure its height, the diameter at the top of the bevel and the depth of the hollow with callipers. The method is in Measuring an undocumented standard, and why it pays to follow someone else's system rather than invent your own, in Designing for an ecosystem.
Printing a base that passes for a bought one
Two things have to come out right: the footprint, because that is what the rules measure and what goes into the tray, and the flatness of the underside. Nobody looks at the bevel or the hollow.
Print it underside down on the bed. That is exactly the face elephant's foot spreads past nominal: a 32 that comes out at 32.3 at the bottom jams in the tray and measures large against a template. Compensate it in the slicer and also chamfer the bottom edge 0.5 mm at 45° (The face on the bed). With that chamfer, the edge touching the table measures Ø31, but seen from above the base still measures 32, and that is what counts.
Do not copy the hollow of the bought base. Make it solid, with the magnet pocket open on the underside. Because it opens onto the bed, the pocket needs no bridge and no support; the hollow, on the other hand, forces you to print upside down or to bridge more than 25 mm. Printed solid (100 % infill), a Ø32 × 4 mm base in PLA weighs up to about 4 g (3.2 cm³ × 1.24 g/cm³); with normal infill it stays at 2.5–3 g. Resin miniatures tend to tip over, and that ballast lowers their center of mass, at the cost of a few more grams for the magnet to hold.
Make it as tall as the bought bases in your army (3 to 4 mm) so the figures stand level.
On the top face, relief is built from layers: a 0.4 mm texture prints as two steps (Fuzzy skin and textures). Flagstones, brick or deck plating look good in FDM. Gravel, roots and grass belong to resin or to basing material (sand, static grass) glued on top.
Magnets: design with the shear force
Shops that specialize in magnets for bases recommend Ø4.5 × 2.2 mm in round 25 and 28.5 bases, and Ø6 × 2.6 from 32 mm up. Large bases take two to four magnets, or one per corner. The other half is a steel sheet in the case or the tray, or a magnetic sheet in the case with a steel disc in the base.
The magnet has to fit with material over it. Leave at least three layers (0.6 mm) between the floor of the pocket and the top face of the base; with the pocket 0.2 deeper than the magnet, the magnet can be at most the base height minus 0.8. A 4 mm base takes the Ø6 × 2.6; a 3 mm base, the Ø6 × 2; in the thin The Old World squares not even the Ø4.5 × 2.2 fits, and you need a 1–1.5 mm magnet or magnetic sheet.
The catalog force is measured by pulling the magnet straight off a thick steel plate. But when the case tilts, is carried by hand or takes a knock, the miniature is pushed sideways, and sideways the magnet only holds by friction. For a Ø6 × 2 N45 disc, Supermagnete gives about 740 g of adhesive force and about 150 g of shear force (what its catalog calls displacement force): a fifth. Design with the shear figure. The example uses the Ø6 × 2 because that is the size with a published shear figure; with the × 2.6 the pocket becomes Ø6.3–6.4 × 2.8.
The example is a heavy miniature (metal or a large figure) of 25 g on a solid 32 mm base: 29 g in total.
| Ø6 × 2 mounting | Shear force | Margin over the weight |
|---|---|---|
| Flush, against thick plate (catalog figure) | ≈ 150 g | 150 / 29 ≈ 5× |
| 0.2 mm inside the underside | ≈ 130 g | ≈ 4.5× |
| Under a 0.6 mm printed roof (3 layers of 0.20) | ≈ 100 g | ≈ 3.5× |
| On thin sheet (tinplate, adhesive steel sheet) | much less | measure it |
The distance losses are estimates: a Ø6 × 3 keeps roughly 70 % of its force at 0.5 mm and 45 % at 1 mm, and a Ø6 × 2 loses a little more; check with the supplier's calculator. A typical resin infantry model weighs a good deal less, so the margin grows. The catalog also assumes thick steel. As a rough guide for a Ø6, steel 1 mm or thicker gets close to the catalog figure, while 0.2–0.5 mm sheet saturates and holds much less. The reliable number comes from the test at the end.
Because force falls off very quickly with distance, the magnet sits flush with the underside, 0.2 mm inside at most, never buried under several layers. The pocket stays open and the magnet is glued. Make the pocket diameter the magnet's plus 0.3 mm on an enclosed CoreXY, or plus 0.4 on a modern bedslinger: Ø6.3–6.4 for a Ø6 and Ø4.8–4.9 for a Ø4.5. The reason for that margin is in Why holes print small. Make it 0.2 deeper than the magnet, so the base does not rock on a magnet that sticks out. Since the mouth of the pocket is on the bed face, elephant's foot closes it too: give it a 0.3–0.5 × 45° chamfer, or check that the slicer's compensation opens holes as well.
Glue it with cyanoacrylate or epoxy. Pressed in without adhesive, it either splits the pocket or chips its nickel plating. If you would rather seal it inside the part, the procedure and the minimum roof are in Embedding magnets and nuts mid-print.
With a magnet in the base and steel in the case there is no polarity to watch, and any base goes in any slot. Magnets on both sides hold harder, but every base in the army must have the same pole facing down: before gluing, find the outward face with a reference magnet and mark it, because a magnet fitted the wrong way round repels. How force falls off with distance, and pocket design in depth, are in Magnets in mechanisms.
Movement trays
A movement tray holds a unit's bases in formation so you can move it in one go. There are two designs. In a pocket tray, the bases sit in a recess and the lip keeps them in. A flat magnetic tray has no lip: it has a steel plate or sheet glued on, and the magnets in the bases do the rest.
You do not size the pocket like a single base: it is a tolerance chain. N bases in a row add up their deviations, and the printed pocket comes out small, like every cavity. The method is in Assemblies and tolerance stackups, and the difference between a locating fit and a sliding fit, in Clearances for moving parts.
| Step | Frontage | Depth |
|---|---|---|
| Nominal (do not use it) | 5 × 25 = 125 | 4 × 25 = 100 |
| Row measured with callipers, bases pushed together (example) | 125.3 | 100.2 |
| Sliding fit, 0.20 per side (0.15 on an enclosed CoreXY) | + 0.4 | + 0.4 |
| PLA shrinkage, ≈ 0.3 % | + 0.4 | + 0.3 |
| 126.1 → 126 | 100.9 → 101 |
The measured figures are an example: measure your own row, because bought bases do not measure exactly 25 mm either.
The lip sits lower than the base: roughly half its measured height. With 4 mm bases, a 1.2 mm floor (6 layers) and a lip 2 mm above the floor leave the base standing proud enough to lift out with a fingertip. If your squares measure 2.2–2.6, drop the lip to 1.2. The wall is 1.8 mm, about four lines with a 0.4 nozzle. The tray adds two walls plus the clearance to the unit's footprint, and some gaming groups measure from the tray edge: keep the wall thin.
With those figures, the tray measures about 130 × 105 × 3.2 mm. It fits the bed of any current printer, but it is a large, thin, flat part: in PETG or ABS it tends to lift at the corners unless you take precautions (Warping and lifting corners). Put the same 0.5 × 45° chamfer on the edge that sits on the bed.
An adapter lets you rank up round-based miniatures on a larger footprint: a round 25 on a 30 square, or on a round 32, with a wall of about (32 − 25.4) / 2 ≈ 3.3 mm. At the same size it does not work: a round 25 in a 25 square would leave zero wall at the four contact points, so there the round base is glued or magnetized on top of a flat square, with no pocket. The round pocket takes the same clearance as the magnet pocket (+0.3/+0.4 on the diameter over the bought base).
It is a hole and, like every hole, it prints small, but at 25–32 mm shrinkage and the elephant's foot at the pocket's mouth dominate, so check it with a coupon rather than stacking another compensation blind.

When it fails
| Symptom | Cause | Fix |
|---|---|---|
| The base rocks on the table | Magnet sticking out, or an elephant's foot flare on the bottom edge | Pocket 0.2 deeper than the magnet; chamfer on the bed edge |
| The magnet will not go into the pocket | Elephant's foot at the mouth, or a pocket with no margin | Chamfer at the mouth; magnet diameter + 0.3/0.4 |
| Bases jam in the tray | Pocket drawn at N × nominal, with no clearance or shrinkage | Measure the row and add 0.4 and the shrinkage |
| Bases rattle and fall out when the tray tilts | Pocket too loose or lip too low | Pocket 0.2 smaller, or steel in the tray floor |
| A base cannot be lifted out | Lip as tall as the base | Lip at half the measured base height |
| The miniature slides on the steel in the case | Designed with the adhesive force, not the shear force; magnet buried; thin sheet | Magnet flush, larger or two of them; sheet of 1 mm or more |
| The magnet falls out | Pressed in without adhesive, or a tight pocket | Margin in the pocket and cyanoacrylate or epoxy |
| The base repels its slot | Reversed polarity (magnet against magnet) | Mark the faces with a reference magnet before gluing |
| The top texture comes out stepped | On the top face, relief is built in layers | Relief several layers deep, or texture in resin or basing material |
| The tray corners lift | Large, thin, flat part | Brim and chamfer; see Warping and lifting corners |
How to test it
Print one base with its pocket and a tray corner for 2 × 2 bases (two walls). In about 15 minutes you will know whether the footprint matches the bought one and whether the pocket fits (Test coupons).
For the magnet, start with the shake test: glue the magnet in, put the miniature in its case on the steel sheet, stand the case on end, then turn it upside down, and give it a sharp knock. To put a number on it, stand the steel sheet vertical and add ballast to the miniature (coins stuck on with putty) until it slides, or pull it sideways with a luggage scale. The margin is the force at which it slides divided by the weight of miniature and base; for transport, aim for 3× or more. Holding on a vertical sheet only proves 1×.
See also
- FDM or resin for your part: why the miniature goes in resin and the base and tray in FDM.
- Magnets in mechanisms: how a magnet's pull falls with distance.
- Painting and priming: finishing bases and miniatures.
- Board-game inserts: storing it all in the game box.
Warhammer and Citadel are trademarks of Games Workshop; Kings of War of Mantic Games; Star Wars: Legion of Lucasfilm and Atomic Mass Games; Dungeons & Dragons of Wizards of the Coast. None of them sponsors or endorses this article.