You have a shelf bracket, a wall hook or the arm of a clamp, and you want to know whether it will hold before you spend an afternoon and 40 g of filament finding out. There are three tools, in this order: a five-minute hand calculation with printed-part numbers, which settles most cases; an external finite element analysis (FEA) when the geometry has no formula, which shows where the part will fail but not how much it will take; and a test of the printed part, which has the last word.

The load comes first

Most estimates that go wrong get the load wrong, not the formula. Before you calculate anything, write down four things:

  • How much. In newtons. A 1 kg hanging mass weighs about 9.8 N; round it to 10 N.
  • Where it acts. At the tip of an arm, spread along a shelf or concentrated on a pin.
  • Which way relative to the layers. That decides how much strength you really have, as you will see below.
  • How it acts. Static (you set it down and it stays put), sustained (it hangs for months), repeated (cycles) or impact.

Dynamic loads and impacts multiply the force. A weight that drops a few centimeters, or a door that slams against its stop, loads the part with several times its static value. Do not try to calculate that number precisely: it goes inside the safety factor.

Four formulas that cover almost everything

Tension or compression. σ = F / A. The force spreads over the cross-section perpendicular to it. A 10 × 4 mm bar (40 mm²) pulled with 200 N carries 5 MPa. Compression has one exception. A long, slender bar never gets as far as crushing: it buckles at a far lower load. If the part is much longer than it is thick, F/A does not protect you; that case needs an FEA or a test.

Cantilever bending, fixed at one end and loaded at the tip. This is the hook, the bracket and the clip:

  • Bending moment at the root: M = F·L.
  • Maximum stress: σ = M / W, with section modulus W = b·h²/6.
  • Tip deflection: δ = F·L³ / (3·E·I), with second moment of area I = b·h³/12.
fixed rootFδLh (depth)b (width)
The depth h is measured in the direction the part bends. Stress σ = M/W and deflection δ = F·L³/(3·E·I) come from this section, and the maximum sits at the root: that is where it breaks.

The root (where the arm meets its support) is the critical point for a geometric reason: the moment grows with distance from the load, so the fixed end carries the maximum moment. That is where the part breaks, and that is where a sharp corner does the most damage.

The exponents are your design levers. Strength grows with h², stiffness with h³, but both grow only linearly with b. Double the length and you double the stress at the root and multiply the deflection by eight. The cube law is worked through in Ribs, gussets and fillets.

Shear on a pin. τ = F / A, with A the pin's cross-section. If the pin is supported on both sides (double shear), the stress is shared between two sections and halves. Compare it with a shear strength of half the tensile strength, which is the conservative estimate. A pin printed upright has its shear plane parallel to the layers and shears along a layer line: use the interlayer value there, or print it lying down, or fit a metal pin. In practice a printed pin usually gives way in bending, or by crushing its hole (σ = F / (d·t), with d the diameter and t the thickness of the wall that holds it), before it fails in pure shear.

A beam supported at both ends with a central load, like a shelf between two brackets: M = F·L/4 and δ = F·L³ / (48·E·I).

The formulas assume plain sections. A hole or a sharp inside corner multiplies σ (a round hole in a plate under tension triples it, Kt ≈ 3): if the critical point is a corner, round it with a radius of half the wall thickness or apply the factor (Ribs, gussets and fillets).

There is a weightier assumption: the formulas treat the part as a homogeneous, isotropic, linear elastic material. A printed part is none of those. The formula is only the starting point, and the next two sections correct it.

Which numbers to use for a printed part

Strength. Start from the tensile strength along the bead (XY) on the datasheet. Datasheet specimens are printed from dry filament under ideal conditions and are often annealed, so that value is an upper bound. This is covered in Reading a material datasheet. Values from current filament datasheets:

Tensile strength along the bead and across layers (MPa)
Material XY (along the bead) Z (across layers, per datasheet) Design Z
PLA 35 31 17.5 (50 %)
PETG 51 35 25.5 (50 %)
ASA 52 35 26 (50 %)
PC 62 56 31 (50 %)
PAHT-CF 92 47 27.6 (30 %)

For polyamides (PA and PA-CF), the datasheet values are dry. A part in service absorbs moisture from the air and ends up below them, in both strength and stiffness. If the datasheet gives conditioned values, use those.

Orientation factor. Datasheets put interlayer strength at 50–90 % of XY in unfilled materials and 25–55 % in fiber-filled ones. For design, take Z = 50 % of XY unfilled and 30 % fiber-filled, and apply it only when the critical tension crosses the layers. In that direction the load pulls on the weld between layers, which is weaker than the bead. The why, and the settings that improve it, are in Layer adhesion and anisotropy.

Do not use the flexural strength. Datasheets list it too (ISO 178), and it is higher than the tensile figure: on the PLA Basic datasheet, about 76 MPa in bending against 35 in tension. That number comes from applying σ = M/W to a bar that is no longer elastic: the core yields and redistributes the load, and the resulting figure exceeds the material's real strength. In the more ductile plastics many specimens do not even break, and the test stops at a fixed deflection. For a printed part, put the tensile strength into σ = M / W: it is conservative and it describes the face that actually cracks.

Stiffness. Deflection needs the elastic modulus E. The design E is the datasheet's flexural modulus, measured along the bead on a printed coupon, multiplied by 0.9 to cover what the coupon does not have: seams, the wall-to-infill transition and the creep of the first hour under load.

Design elastic modulus for hand calculations (GPa)
Material Design E, along the bead Across layers (indicative)
PLA 2.5 ≈ 2.1
PETG 1.6 ≈ 1.4
ASA 1.7 ≈ 1.4
PC 2.1 ≈ 1.8
PAHT-CF (dry) 3.8 ≈ 1.7

Across the layers, an unfilled material keeps about 0.85 of its E; a fiber-filled one, about 0.45. Do not use the 3.3–3.6 GPa often quoted for PLA: that is the injection-molded resin, not a printed part.

The section is not solid. The skin (walls plus top and bottom layers) carries the bending; sparse infill barely works. The reason is in Walls, perimeters and infill. The conservative rule: calculate I and W from the skin alone and ignore the infill. In narrow sections, 10 mm or less, with three or four walls (1.2 or about 1.6 mm with a 0.4 mm nozzle), the part is nearly solid and the difference is small. In large sections, the second moment of area of the skin alone can be half that of the solid section.

Elongation at break drops more than strength across the layers: PLA goes from 12 % to 7.5 %, PETG from 9.5 % to 5.2 %. An interlayer failure is brittle: the part snaps without deforming first. That justifies a higher safety factor; it is not a second reduction.

Worked example: the arm of a wall hook

A wall hook in PLA. The arm is 60 mm long and 10 mm wide (b), and you have to choose the depth h. It must hold 2 kg at the tip, about 20 N. The load is static and light, and nothing serious happens if it fails: you are aiming for a safety factor of 2.

Moment at the root: M = 20 N × 60 mm = 1,200 N·mm.

With h = 8 mm, printed lying flat. The tension runs along the arm without crossing layers. W = 10·8²/6 ≈ 107 mm³, so σ ≈ 11.3 MPa. Allowable: 35 / 2 = 17.5 MPa. Actual factor: 35 / 11.3 ≈ 3.1. It passes.

The same arm printed upright. Now the tension face crosses the layers. Design strength: 0.5 × 35 = 17.5 MPa; allowable: 8.75 MPa. The stress is still 11.3 MPa, so the actual factor is 17.5 / 11.3 ≈ 1.6. It falls short of 2.

The fix is more depth. To pass upright, σ has to come down to 8.75 MPa: W ≥ 137 mm³, which means h ≥ 9.1 mm. With h = 10 mm, W ≈ 167 mm³, σ ≈ 7.2 MPa and the actual factor is 2.4: it passes, and that is the depth you choose. Printing upright costs about 2 mm of depth here, 25 % more plastic in the arm. With h = 12 mm, W = 240 mm³, σ = 5.0 MPa and the factor rises to 3.5: the option with plenty in hand that the figure shows, in case the load grows. More infill fixes nothing: the stress is on the outer face.

Datasheet (XY) 35Flat, h = 8: 11.3 vs 17.5passesUpright, h = 8: 11.3 vs 8.75Orientation ×0.5failsUpright, h = 12: 5.0 vs 8.75passes010203040Stress (MPa)Design strengthAllowable (÷2)Calculated stress
Same load, same material. Printing upright takes half the arm's strength away before the safety factor is applied: at 8 mm it fails; at 10 mm it already passes, and at 12 mm with plenty in hand.

A caveat about "flat". With the arm lying on the bed, the most heavily stressed faces are the top and bottom skins, and those skins are solid infill with lines at ±45°, not beads running along the arm. Only the side walls run the right way. The best stance for a cantilever is on its edge, with the bending plane in XY: then the tension and compression faces are walls that follow the arm. If you print it flat, add top and bottom layers or assume a little less than XY in the skin. How to weigh that stance against supports and finish is covered in Orientation and overhangs.

Skin-only check. Flat, h = 8 mm, with three walls (1.2 mm per side), 1 mm of skin top and bottom and the infill ignored: I drops from about 427 to about 290 mm⁴, or 68 %. The stress rises to about 16.6 MPa and the factor falls to 2.1. It still passes, with a lot less margin. That is why you should always run it.

Deflection. With h = 8 and E = 2.5 GPa, the tip drops about 1.35 mm with a solid section and about 2.0 mm with the skin alone. In PETG (E = 1.6 GPa) it drops about 2.1 mm with a solid section: tougher than PLA, but it bends more than one and a half times as much. A part can pass on strength and fail on stiffness. The difference between the two properties is explained in Stiffness, strength and toughness.

How much margin to leave

These are two separate corrections, and you must not stack them by accident:

  1. The orientation factor (0.5 unfilled, 0.3 filled), only when the critical tension crosses the layers. It corrects something you know: the weld between layers is weaker.
  2. The safety factor, for everything you do not know.

If you raise the safety factor "because the load crosses the layers" after applying the orientation factor, you count the anisotropy twice and oversize for no reason.

Indicative safety factors for printed parts
Situation Factor
Static, known load along the bead; nothing serious happens if it fails 2
Uncertain load, knocks, or a failure that damages something else 3
Load sustained for months, cyclic load, hot environment or risk of injury 4 or more

If you need more than 4 or 5, the answer is another material, a metal insert or not printing it: When to order the part instead.

For metal machine parts, with well-known material and load, factors of 1.5–2 are common. Here they are higher because of the scatter between prints (moisture, cooling, a layer that went cold), the voids between beads and at the seam, because you do not know the real Z value in your part, and because the datasheet describes an ideal specimen. In a large part, with long layers, heavy part cooling or damp filament, interlayer strength can fall to 20–40 % of XY.

Sustained loads. Under constant stress, plastic creeps, and the more so the warmer it gets. Under load, an unfilled part works up to about 15–20 °C below its heat deflection temperature (HDT) at 0.45 MPa: PLA about 40 °C, PETG 50, ASA 80–85 and PC 95 (Heat, cold, sunlight and chemicals). A PLA hook by a sunny window gives way within days at a stress it would carry for years at 20 °C. In summer, a car's dashboard in the sun reaches 70–100 °C. A loaded part there needs a fiber-filled compound: PA-CF, PET-CF or PPA-CF. Unloaded or in the shade, in the console or the glovebox, ASA, PC or annealed PLA-HT will do, and PC wherever it takes knocks. Inside a car, never PLA or PETG. How the deflection grows over the months is in Creep and fatigue.

Cyclic loads. Fatigue starts at the weakest defect, almost always a layer line, the seam or a corner, at loads far below the static breaking load. A static calculation cannot see it. Use a factor of 4 or more, put the cyclic tension along the beads and, if it matters, test with cycles.

Snap fits and living hinges work with an imposed displacement. For them you compare the strain ε with the allowable strain, rather than stress with strength, and each has its own formula: in a snap fit, ε ≈ 1.5·t·y / L², with t the thickness, L the length and y the deflection at the tip (Print-friendly snap fits); in a hinge or a flexure, ε = t·θ / (2L), with θ the fold angle (Living hinges and flexures).

When finite element analysis pays off

FEA pays off when the geometry has no textbook formula: organic shapes, several load paths, plates with cut-outs, a bracket with ribs and holes. It also helps you locate the peak stress before printing and compare two versions. For a beam, a pin, a plate or a hook it does not pay: the hand calculation is quicker and equally reliable.

diagram
Pick the tool by the shape of the part, but every route ends at the printed part: if it does not break where you expected, go back to the shape or the orientation.

As of late 2026, several tools build linear static analysis into the CAD itself, all of them paid: Autodesk Fusion (with a commercial subscription; the free personal license does not include simulation), Onshape Simulation (Professional and Enterprise plans) and SolidWorks Simulation. The free option is FreeCAD's FEM workbench with the CalculiX solver.

What the analysis assumes. A solid, isotropic, linear elastic part. Yours is a skin around sparse infill, and it is weak between layers. So the absolute stress and deflection figures it reports are optimistic. What you can trust is the map (where the stress concentrates) and the comparison between versions A and B.

wallboltsFstress peaklowhigh
An L-bracket bolted to the wall by its vertical flange, with the load at the tip of the arm: almost the whole part in cool tones and the stress peak at the sharp inside corner, on the top face of the arm, which is the one in tension.

That color map describes a solid, isotropic model: trust where the red is, not the number.

Two misleading peaks.

  • A perfectly sharp inside corner is a singularity. Add a fillet, however small, before you compare.
  • If you fix an entire face, artificial peaks appear along its edge.

The test is to refine the mesh: a real stress raiser converges to a value; a singularity keeps climbing.

From the FEA figure to a decision, with the same criteria as the hand calculation. If the tension in the critical zone runs along the bead, take the maximum von Mises stress away from the singularities and compare it with XY. If the critical face crosses the layers, von Mises is the wrong measure: interlayer failure is brittle and is driven by tension perpendicular to the layer. Read the maximum principal stress (or the Z component, if your tool shows it) and compare it with 0.5 or 0.3 × XY. Then apply the safety factor. If your tool lets you model skin and infill, so much the better; most hobbyist tools do not, so treat the deflection as a minimum.

Displacement is the stiffness check and is separate from strength. A part that does not break but deflects 4 mm may be no use at all.

When it fails

Symptom, cause and fix
Symptom Cause Fix
It breaks under a load the calculation passed You calculated with the static weight and the part takes knocks Put the impacts into the factor (3 or more) instead of refining the formula
The part is far softer or weaker than calculated The depth was measured the wrong way: h is the dimension in the direction of bending, not the thinnest one Redo the sum; the error goes squared into W and cubed into the deflection
The calculation shows a margin the part does not have You used the datasheet's flexural strength σ = M / W takes the tensile value
The part comes out thick and heavy for no reason You counted the anisotropy twice Orientation factor only if the tension crosses layers, safety factor separately
A large section bends more than expected You assumed a solid section Run the skin-only check
It passes on strength and bends too much You did not calculate the deflection; PETG is the classic case Always calculate the deflection, then add depth or a rib
The FEA shows a huge peak at a sharp corner It is a singularity Round it and remesh before you trust the figure
It held in the workshop and gave way in summer Creep in the heat Design below the service temperature under load: 40 °C for PLA, 50 °C for PETG

How to test it

Print the candidate in its final orientation, material and profile. Hang the design load multiplied by the safety factor on it for 24 hours and check that it has not cracked or taken a permanent set. Then add weight in steps of 10–20 % of the design load until it breaks, and note the load and where it broke. Water bottles make good weights, and a luggage scale measures the pull.

Read the break:

If a failure has consequences, test at least two parts: one is an anecdote. To test the material before the part, print a break bar oriented like the final part, as explained in Test coupons.

See also

Design it in KapyCAD

Draw the part with these clearances and walls, and change any dimension later without redrawing it.

Free plan, no card. Runs in your browser, nothing to install.

Open the editor