There is a TPU finger on the bench with a tube pushed into its base. You push air in with a large syringe and the finger curls round an egg. No motor, no hinge, no sliding seal: a closed chamber whose walls only let it grow in one direction. Printed in TPU, it bends by opening pleats over a layer that does not stretch. That gives you two problems: how far it bends and how hard it pushes at a given pressure, and how to keep the air in.

Why it bends

Pressure pushes outwards on every inside face equally. If one side of the chamber cannot lengthen (the strain-limiting layer, here called the inextensible layer) and the opposite side can, because it is pleated, the only way the chamber can grow is by curling toward that side. The geometry decides the direction of bending, not the air.

The arithmetic does not depend on the material. The inextensible layer keeps its length L. If the finger bends through an angle θ (in radians) about it, a fiber at height h above it has to lengthen by:

Δ = θ·h, with curvature κ = θ/L

With h = 14 mm and θ = 90° (π/2), Δ ≈ 22 mm, whether the finger is silicone or TPU. The question is where those 22 mm come from.

A cast silicone finger (the PneuNets of soft robotics) gets them by stretching rubber. Ecoflex 00-30 has a 100 % modulus of about 0.07 MPa according to the Smooth-On datasheet, and stretching it 30 % takes very little force. TPU 95A sits around E ≈ 9 MPa, the design value (9.2 MPa in XY and 7.8 in Z on the Bambu datasheet, the figures Accordion bellows uses): more than 100 times stiffer. Stretching a printed wall by 30 % would take more pressure than the wall can hold. So the printed finger gets Δ by opening a row of pleats along its spine, each turning only θ/N. The walls flex like the flanks of a bellows and barely stretch.

This is the idea Mosadegh and colleagues published in 2014 ("fast PneuNets"): inner walls between chambers thinner than the outer ones, and a gap between neighboring chambers, so the pressure works where the finger bends. The volume needed for a full bend fell tenfold, and their silicone finger bent in about 50 ms at 345 kPa. The pleated printed finger takes the idea to its extreme: soft in one direction and stiff in all the others.

A translucent TPU pneumatic finger on a workbench, inflated with a syringe: curled through 90° toward its flat base, with the gaps between chambers opened into wedges on the outside.
A translucent TPU pneumatic finger on a workbench, inflated with a syringe: curled through 90° toward its flat base, with the gaps between chambers opened into wedges on the outside.
Three families of printed actuator
Family Geometry What it does when actuated What for
Pneumatic finger pleats along the spine + inextensible layer under pressure, curls toward the inextensible layer gripping, wrapping
Linear bellows pleats all round, capped at one end under pressure, extends along its axis, F = p·A pushing, lifting
Vacuum actuator the same pleats, evacuated by a pump shortens, or bends the other way contracting with no risk of bursting

Without air, a finger bends in two other ways: passively, conforming to the load (Gripper fingers that wrap the load), or pulled by a cable (Tendon-driven mechanisms).

At restp·A_cForce on the wallRoot blockChamberPleatCrestAir inletInextensible layerEmbedded stripehM = p·A_c·eBends this way45°45° roofInflatedθΔ = θ·hLTTensionF_tip ≤ M/LTip force
A pneumatic finger at rest and bent through 90°. The inextensible layer keeps its length; the pleat crests separate by Δ = θ·h. Pressure pushes on each chamber wall with a force p·A_c, applied at a height e above the layer, and that layer works in tension.

Sizing a finger

Every pressure here is gauge pressure, above atmospheric, unless marked "absolute". 1 bar is 100 kPa.

Force on the walls of each chamber. Pressure pushes on the two end walls of each chamber with a force F = p·A_c, where A_c is the inside cross-section of the chamber. That force acts at the centroid of A_c, at a height e above the mid-plane of the inextensible layer.

Moment. M = p·A_c·e. This is what bends the finger and the most it can deliver. The blocked force, the force at the tip when you hold it still at a distance L from the root, satisfies F_tip ≤ M/L. The root chamber, the one furthest from the tip, sets the limit. And the stiffness of the walls themselves soaks up part of the moment, so the real force is lower. Bigger chambers and taller fingers (more A_c and more e) give more force; a longer finger gives less.

The inextensible layer has to be inextensible. It works in tension under the chamber force, T = p·A_c, and stretches by:

ε_b = T / (E·b·t_b)

where b is its width and t_b its thickness. In TPU 95A that is not small (10 % in the example), and every percentage point of stretch is bending lost, and a finger that grows longer as well. That 10 % is the soft case: the modulus of 95A varies about sevenfold from one datasheet to another (67 MPa on UltiMaker's, measured differently), and at 67 MPa the stretch would drop to a little over 1 %. Measure your filament, or assume the soft case. Fixes, from mildest to strongest: make the layer thicker and wider than the chamber walls; embed a sheet that does not stretch (fabric, paper or a thin strip of PETG or PLA) with a pause (Printing onto fabric, Embedding magnets and nuts mid-print); or print it as a rigid strip in a two-material print (Functional multi-material parts). A thin rigid strip bends without trouble: spread along the whole finger, its bending strain, ε = t·θ/(2L), is tiny. A PETG strip 0.5 mm thick and 80 mm long, bent through 90°, sees about 0.5 %, below the 2 % PETG tolerates in repeated use (Print-friendly snap fits).

Ballooning. The relation σ = p·r/t from Watertight printed parts holds for a curved wall. A flat side wall works in bending, like a plate built in at its edges. In the example finger, each side wall is a 12 × 6 mm panel between two pleats, and for a panel twice as long as it is wide σ ≈ 0.5·p·b²/t², with b the short side. With b = 6 mm, t = 1.28 mm and 1.5 bar you get about 1.6 MPa, and in TPU, with E ≈ 9 MPa, that is not a small bulge: the flat wall swells until it curves and works as a membrane. Three remedies, and they stack: draw the side walls and the roof slightly convex, so they work as membranes from the start; give them one more line than the pleat walls, so the pleats move first (the PneuNets rule); and, on a wide span, add ribs. Measure the bulge in the test. A finger that swells sideways instead of bending has its wall thicknesses the wrong way round.

Pressure required. There is no reliable closed-form formula for printed pleats: TPU is non-linear and the walls flex like the flanks of a bellows, whose stiffness k ≈ 1.6·E·D_m·t³/(N·h³) only shows the trend. As a guide, published printed-TPU fingers need between 1 and 4 bar to bend through 90°, against tenths of a bar for a cast silicone one. The figure for your finger comes from its angle–pressure curve (below). The parameters you can change are those of Accordion bellows: wall thickness (× t³), pleat depth (× 1/h³), number of pleats (× 1/N) and hardness. 85A is about three times softer than 95A (TPU and flexible filaments).

Linear bellows and vacuum actuators

A linear bellows is the accordion bellows with one end capped. It pushes with:

F = p·A_eff − k·δ, with A_eff ≈ π·D_m²/4

With D_m = 26 mm, A_eff ≈ 530 mm²; at 1 bar that is 53 N, minus the spring force k·δ of the pleats compressed or stretched by a distance δ. Under pressure it buckles sideways sooner than under vacuum: guide it with a rod inside or a sleeve outside, as in Accordion bellows.

If you evacuate it instead of inflating it, the atmosphere does the work. The pleats close and the bellows shortens like a muscle or, in a finger designed for it, bends. The pressure difference can never exceed atmospheric pressure, about 1.01 bar at sea level and less at altitude, and a mini vacuum pump stays well below that (figures in "Air supply and safety"). The maximum force is F ≈ Δp·A_eff: about 35 N with 530 mm² at −0.65 bar. Tawk and colleagues (University of Wollongong) printed linear vacuum actuators in TPU in a single piece, without supports: depending on the version of the work, they measured 27–30 N of blocked force and between 21,500 and 26,000 cycles, at several hertz. In a home-made vacuum actuator, the pump's flow rate limits the speed.

Vacuum suits a printed part: it cannot burst it, a failure crushes the part instead of blowing it apart, and the maximum force has a physical ceiling. It still needs an airtight wall, because a leak lets air in. And the pleats must not collapse inwards unevenly: if the bellows folds over sideways, stiffen each pleat with a rigid collar or inner rings.

There are variants that twist or extend with helical pleats or fiber-reinforced silicone, but they do not print well in TPU.

Worked example: a gripper finger in TPU 95A

The brief: two opposed fingers to pick up objects 60 to 80 mm across and up to about 150 g. Air comes from a small compressor with a regulator, and the planned working pressure is 1.5 bar (0.15 MPa). TPU 95A, printed lying on the inextensible layer.

Geometry.

Gripper finger in TPU 95A
Dimension Value
Active length L 80 mm, plus a rigid root block
Inside chamber section 12 × 12 mm, A_c = 144 mm², starting 1.6 mm above the bed
Pleats N 8, 10 mm pitch
Inside length of each chamber 6 mm, with a gap of about 2 mm between neighboring chambers
Pleat walls 3 lines of 0.32 mm = 0.96 mm
Side walls and roof 4 lines, ≈ 1.28 mm, sides slightly convex
Width b 12 + 2 × 1.28 ≈ 14.6 mm
Inextensible layer t_b 1.6 mm (16 layers of 0.10), with a pocket for the strip
Air channel Ø3 along the inextensible side, linking all the chambers

The gap between chambers matters: two pleat walls that touch fuse into one 2 mm wall, which no longer opens.

What has to open. With a gabled roof, the crests at the ridge sit at h ≈ 20.6 mm above the mid-plane of the inextensible layer (the eaves at about 14 mm). For 90°, Δ = (π/2)·20.6 ≈ 32 mm: about 4 mm of opening at the crest of each pleat (2.75 mm at eave height), 11° of rotation each. So that they open that far without the strain concentrating on an edge, round the crests with a radius ≥ t, as in Accordion bellows.

Force. The chamber runs from z = 1.6 to 13.6 mm (ignoring the gabled roof, which keeps the calculation on the safe side). Its centroid is 7.6 mm above the bed and the mid-plane of the layer is at 0.8 mm, so e ≈ 6.8 mm. With the embedded strip the finger bends about the mid-plane of the strip, at z ≈ 0.65 mm, and e becomes 6.95 mm: 2 %, which changes nothing.

  • Per chamber: F = 0.15 × 144 ≈ 21.6 N.
  • Moment: M = 21.6 × 6.8 ≈ 147 N·mm.
  • Blocked force at the tip: ≤ 147/80 ≈ 1.8 N per finger.

That 1.8 N is what the finger would give if its walls cost nothing to bend, and they cost a lot. Call p_contact the pressure that brings the free finger into contact with the object. What is left for squeezing is roughly (p_working − p_contact)·A_c·e. If the finger needs a little over 1 bar to close on a 70 mm object, at 1.5 bar it has barely 0.5 bar left to squeeze: about 0.6 N per finger, and with μ ≈ 0.5 two fingers hold 2 × 0.6 × 0.5 ≈ 0.6 N, the weight of about 60 g. At 1.5 bar there is no guaranteed margin for 150 g. Measure p_contact on the angle–pressure curve and decide from that figure: raise the working pressure well above p_contact, lower p_contact with 85A or deeper pleats, raise e with taller chambers, or add a TPU 85A pad on the gripping face to raise μ.

The inextensible layer. T = 21.6 N. With TPU alone, ε_b = 21.6 / (9 × 14.6 × 1.6) ≈ 10 %: too much. Embed a 0.5 mm PETG strip (or fabric). Model a pocket in the layer as deep as the strip is thick, plus clearance, and put the pause at the layer that closes it; if you lay the strip on top of a layer with no pocket, the nozzle hits it on the next one (Embedding magnets and nuts mid-print). Drill the strip with 2–3 mm holes every few millimeters so the TPU passes through and anchors it: a plain strip peels off with cycling. Its bending strain, ε = 0.5 × 1.571 / 160 ≈ 0.5 %, is harmless, and the strip removes the stretch of the layer.

The walls. Slightly convex sides with one more line than the pleats, as in "Ballooning"; if they swell in the test, add another line or a rib.

Air and energy. Volume ≈ 8 chambers × (12 × 12 × 6) mm³ ≈ 6.9 ml, about 7.5 ml with the channel. The energy a gas releases as it escapes to atmosphere is W = p_abs·V·ln(p_abs/p_atm) − (p_abs − p_atm)·V. At 1.5 bar (2.5 bar absolute): 0.25 MPa × 7500 mm³ × ln 2.5 − 0.15 MPa × 7500 mm³ ≈ 1.7 − 1.1 ≈ 0.6 J. Harmless. The tank of a 24 L workshop compressor at 8 bar holds about 28 kJ, tens of thousands of times more: that is why a regulator and a relief valve sit between the compressor and the finger.

The source. A 12 V mini pump does not reach 1.5 bar (figures in "Air supply and safety"). If that is your source, redesign the finger in 85A or with deeper pleats.

Printing it airtight

The leak paths (the seam, the joint between wall and solid infill, the gaps between lines, porosity) and the table of settings are in Watertight printed parts; drying, direct drive and TPU's flow limit, in TPU and flexible filaments. Here is only what changes when the wall is thin and flexes under air.

Air gets through where water does not: a finger that holds water can still hiss with air. And the wall moves on every cycle, so it opens any weak joint. Airtightness depends on the print settings, not only on thickness. A 2026 study (Abboodi, University of Ottawa) found that three lines of 0.32 mm (0.96 mm) sealed better than two of 0.8 mm (1.6 mm), and that walls of one or two lines did not seal reliably. The lesson is the line count: several lines seal better than a few very wide ones. It does not show that a 0.32 mm line seals better than a 0.45 mm one, the usual width with a 0.4 mm nozzle. To close the diamonds between lines: flow or line width 5–10 % up, thin layers, low speed and dry filament (Drying and storing filament).

Print the finger lying on the inextensible layer. The bed face is the most closed (The face on the bed) and the inextensible layer comes out solid from the first layer. This is stance A, lying flat (Layer orientation for mechanisms). The roof of a 12 mm chamber cannot be a flat bridge in TPU: draw it as a 45° gable or a pointed arch so it prints without supports (Orientation and overhangs). A support inside a closed chamber cannot come out without tearing the wall. The pleat walls rise vertically, and the flexing at the crests crosses layers, as at the corners of a printed bellows in any orientation. Soft TPU tolerates it: 85A keeps 88 % of its XY strength in Z, and 95A a little over 80 %. Do not use the "AMS-compatible" TPU 68D: with 31 % elongation in Z, it cracks at the crests.

The alternative is to print the finger on its side, with the bending plane parallel to the bed. The crests become vertical lines and flex along the beads (stance B, on edge), but the inextensible layer becomes a vertical wall and the chamber needs 45° roofs on both faces. Turn to it if the finger cracks at the crests when printed flat.

PauseInextensible layerStripBedAir channelPleat wall: 3 linesRoofSeam hereNot hereSide wall: 4 linesOverhang ≤ 45°FittingRigid rootOverlapTPU bodyOption: O-ring
Section through a chamber as printed, with the strip embedded at a pause, the lines of each wall, the 45° roof and the seam on the inextensible side. On the right, the rigid root with the fitting and the overlap with the TPU body.

The seam goes on the inextensible side or in the root block, where strain is lowest. Never on the crests: a seam notch on every crest is the classic bellows failure. If your slicer has it, use the scarf seam (Where the seam goes).

The walls come in whole lines (line count × line width), with one more line on the outer walls than on the pleat walls (Walls, perimeters and infill). No infill: the walls are the part, and any infill inside a wall that flexes under pressure is a network of leaks.

The air inlet. A printed TPU spigot is not a calibrated tube: its size is imprecise and its layers porous, so without a rigid root or a clamping collar it leaks or pulls out under pressure. And TPU will not hold a thread. Give the root a rigid part: a PETG block printed into the same part in two materials (Multi-material print-in-place) or screwed to the body with a face O-ring. In that block goes a brass barb or a bought push-fit fitting, pressed or glued in. The dimensions are in Hose barbs and fittings, Push-fit fittings and PTFE tube (push-fit fittings for 4 mm polyurethane tube) and O-ring grooves. The Ø3 channel and the fitting bore print small, for the reasons in Why holes print small: compensate for them or run a drill through.

As a last resort, and only if the print is already good, a thin elastic coating inside or out seals isolated pores (Coatings and epoxy). Epoxy is rigid and cracks on a wall that flexes: never epoxy on the pleats.

Air supply and safety

As of late 2026, datasheets for 12 V mini diaphragm pumps give a maximum of 0.6 to 1.2 bar (60–120 kPa) against a closed outlet, and −0.58 to −0.70 bar on vacuum (how they work: Gear and diaphragm pumps). An airbrush compressor or a small piston compressor gives a few bar through a regulator, and a workshop compressor 8 bar. Choose the actuator for the source or the source for the actuator: the finger in the example, at 1.5 bar, is out of a mini pump's reach.

The circuit, in order: pump → pressure regulator (or the pump's own maximum pressure) → relief valve set slightly above the working pressure → 3/2 solenoid valve, which fills and vents → actuator. A check valve holds the pressure with the pump off; flap and duckbill valves work with air (Check valves and taps). While you are designing, put a gauge between the solenoid valve and the actuator.

A printed actuator fails when a wall ruptures and, if it is full of air, the stored energy is released all at once. A small volume at 1–2 bar is little energy (0.6 J in the example); the danger is the source behind it. Never connect a printed actuator straight to a compressor: always a regulator and a relief valve, and safety glasses while you test. Proof-test a new design with water, never with air: fill it with a syringe and take it to 1.5 times the working pressure for 10–15 min, as in Watertight printed parts. Burst a sacrificial sample with water and never work above half that pressure. Without that margin, nothing near the face and nothing worn on the body.

TPU does not take sustained load: it creeps (Creep and fatigue). A finger that stays inflated for hours takes a set and the pleats no longer close. A vacuum actuator is also TPU under load and creeps the same way. Design it to rest unloaded and to hold in short cycles; for long holds, use a mechanical latch.

When it fails

Symptom, cause and fix
Symptom Cause Fix
Hisses or loses pressure Gaps between lines, wet filament, seam on a crest One more line or flow +5–10 %, dry the filament, seam on the inextensible side
Leaks only at the inlet TPU spigot with no rigid root or collar Rigid root block, push-fit fitting, face O-ring
Bends less than expected and gets longer The inextensible layer stretches Embed fabric or a rigid strip
Swells sideways instead of bending Flat sides, as thin as the pleats Convex sides, one more line, ribs
Needs more pressure than the source gives 95A, shallow pleats, thick walls 85A, deeper pleats, one line fewer on the pleats but never below 3
Squeezes weakly though it bends well Nearly all the pressure goes into closing the finger Measure p_contact, raise the working pressure or lower p_contact
Tears at a crest after a few cycles Sharp crest, TPU 68D, seam notch Crest radius ≥ t, 95A or 85A, seam off the crests
Bends sideways or twists Asymmetric walls, off-center inextensible layer, uneven print Symmetric section; check the line count of each wall on both sides
Collapses unevenly under vacuum The pleats buckle inwards Rigid collars between pleats
Stays bent after a long hold Creep Rest unloaded, short holds, mechanical latch
The chamber roof sags or closes up Flat roof over a wide chamber 45° gabled roof

How to test it

Water first. The proof test in "Air supply and safety" comes before any test with air.

Bubble test. Bring it to working pressure and put it under water, or paint the walls with soapy water. A stream of bubbles marks the leak; note whether it comes from the seam, a crest or the inlet.

Pressure-decay test. Pressurize it and wait a few minutes for it to settle: TPU creeps, the finger grows a little and the pressure drops with no leak at all. Then close the valve and watch the gauge for 60 s. A drop of a few percent is a slow leak; with under 10 ml of volume any leak shows quickly, but the tube and the gauge count too. To separate leak from creep, use the bubble test, or repeat the measurement with the same line closed against a rigid plug. Repeat the decay test after the cycle test.

Angle–pressure curve. Photograph the finger in front of a printed protractor at every 0.25 bar step, up to the working pressure and back down. It gives you the real pressure for 90°, the hysteresis and the p_contact from the example. For the blocked force, rest the tip on a kitchen scale with the root fixed and the finger stopped at a known angle.

Cycles. Run as many cycles as the application demands (a cheap counter on the solenoid valve) and repeat the pressure decay and the curve. For reference, Torzini and colleagues measured in 2024 an average of about 6,400 cycles at 3 bar on bellows-shaped printed-TPU bending actuators. The more than 2 × 10⁶ folds of a TPU living hinge (Living hinges and flexures) are not the life of a pressurized chamber: the wall loses air or tears long before. How to set up the test and when to call it good: Testing a mechanism before you trust it.

See also

Design it in KapyCAD

Sketch the mechanism with these dimensions. Each one stays a value you can change after the first test print.

Free plan, no card. Runs in your browser, nothing to install.

Open the editor

Still have a question?