kapy academy

Sizing a gear that holds

18 min readUpdated Nov 2026

A module 1 PLA pinion on a NEMA 17 turns quietly and loses a tooth at the first hard stop: the profile was fine; the load calculation was missing. Module, face width and material come from motor torque with the Lewis equation, which you then check on the bench. It all starts from one idea: a tooth is a short cantilever beam that breaks in bending at the root. Its strength depends on that root's thickness, set by the module, and its length, set by the face width. Infill does not come into it.

The smallest module your nozzle can print

Tooth thickness at the pitch circle is s = π·m/2. Divide it by a 0.45 mm bead and you know how many beads fit across it.

Tooth thickness at the pitch circle and how many 0.45 mm beads fit
Module s = π·m/2 0.45 mm beads Use
0.8 1.26 mm ≈ 2.8 motion only; the limit with a 0.2 nozzle
1 1.57 mm ≈ 3.5 minimum for light load (0.4 nozzle)
1.5 2.36 mm ≈ 5.2 real load
2 3.14 mm ≈ 7 real load, output stages

The tooth is thinner than that at the tip and thicker at the root. On a 17-tooth, m 1 pinion the tip is about 0.7 mm: a bead and a half. At m 0.8 it drops to about 0.54 mm, a single bead. When the tip is one bead it prints rounded, and the involute is lost in the stepped outline. Hence the rule: with a 0.4 nozzle, m ≥ 1 for any gear that transmits torque, and m 1.5 to m 2 when there is real load, such as a stepper at full torque or an arm. With a 0.2 nozzle, m 0.8 is the limit.

Modules 0.5 and 0.8 do print with a 0.4 nozzle, and they mesh. They are for transmitting motion without load: an indicator, a dial, a model. As soon as the gear has to push something, go back to m ≥ 1.

The pinion's tooth count affects strength too. Without profile shift, 17 teeth avoid undercut; at 14 the undercut is small and tolerable. On a printed pinion, stay at 17 teeth or more, ideally 18–20, for another reason: the rounded tip and the backlash reduce the contact ratio. Why undercut appears is explained in Spur gears, and how to correct it with profile shift in Gear design tools. What matters here is its effect: undercut thins the root, and a thinner root gives a lower form factor Y.

Module 0.8Thickness at pitch circles = 1.26 mm≈ 2.8 0.45 mm beadsMotion onlyModule 1Thickness at pitch circles = 1.57 mm≈ 3.5 0.45 mm beadsLight-load minimumModule 1.5Thickness at pitch circles = 2.36 mm≈ 5.2 0.45 mm beadsLoadModule 2Thickness at pitch circles = 3.14 mm≈ 7.0 0.45 mm beadsLoad1 mm0.45 mm
The same tooth at four modules, to scale. Below m 1 the tip is down to a single bead.

The tooth as a beam: the Lewis equation

The tangential force Ft pushing on each tooth comes from the torque and the pitch diameter:

Ft = 2·T / d, with d = m·z

The Lewis equation, in its simplified form, treats the tooth as a cantilever and gives the stress at the root:

σ = Ft / (b·m·Y)

where b is the face width and Y the form factor, which grows with the number of teeth.

Lewis form factor Y, 20°, full-depth teeth (Shigley, table 14-2)
z 12 14 17 20 25 30 40 50 100 rack
Y 0.245 0.277 0.303 0.322 0.340 0.359 0.389 0.409 0.447 0.485

Ft is the same on the pinion and the wheel. The wheel has more teeth and a larger Y, so if both are the same material, the pinion is the critical one. Calculate the pinion.

Do not mix tables. This Y includes π and goes with σ = Ft/(b·m·Y). Other texts tabulate another Y: Hamrock gives somewhat different values (0.210, 0.264…), and some use y = Y/π (≈ 0.078 for 12 teeth) with σ = Ft/(b·p·y). Take Y and the formula from the same source: mix them and you are off by anything from 15 % to a factor of π.

Rearrange for force and you get what your gear can carry:

Ft max = σallow·b·m·Y and T max = Ft max·d/2

The simplified form leaves out the dynamic factor, load sharing between tooth pairs and the stress concentration at the root fillet. You do not need them here: the allowable stress you are about to use is low and covers them. The full method for plastic gears is VDI 2736 (2014), but it only tabulates a handful of injection-molded thermoplastics and nothing printed.

For a printed tooth in continuous service, take ¼ to ⅓ of the datasheet's XY tensile strength as the allowable stress: PLA 8–12 MPa (the examples use 10) and PETG 12–15 MPa (the examples use 12; the rule would give 13–17 from its 51 MPa, and the book stays on the safe side). It is the same figure Fixing a part to a shaft uses for bearing pressure on a printed hub.

That fraction is already your margin against repeated load. Do not stack the safety factor from Estimating whether a part will hold on top: you would count the margin twice and end up with gears twice as wide for no reason. What you must do is calculate with the motor's peak torque (holding or stall), not its working torque. The hard stop in the opening example applied at least that much. If the output can hit an end stop or jam, the peak is higher: the inertia of the spinning rotor and load dumps into the mesh and exceeds the holding torque. In that case, fit a soft stop or a torque limiter, or leave more margin.

Root sectionRoot filletStarts hereFtTangentialRadialσ = Ft / (b·m·Y)Root section+−Face width bWallsInfill
The tooth is a cantilever: the force at the tip bends it and the crack starts at the root, on the side in tension. Walls form it, not infill.

Face width: the cheapest lever, up to 12·m

σ is inversely proportional to face width. Double b and you double the torque the tooth can take without touching the kinematics or the center distance. It is the first thing to change.

Face width as a function of module
Case Face width b
Printed gear, recommended 8–10·m
Minimum for plastic gears 6–8·m
Metal (Shigley, 3p–5p) ≈ 9.4–15.7·m
Practical limit ≈ 12·m

The limit exists because above about 12·m the load no longer spreads across the whole face. A shaft that deflects or a housing that gives tilts one gear relative to the other, and only one edge carries the load. The rest of the width contributes nothing. If 12·m is not enough, go up a module.

To make the whole width work:

  • Support the shaft on both sides of the gear, not at one end with the gear far from the bearing.
  • Stiffen the housing between the two shafts. The radial component, Ft·tan 20° (36 % of Ft), tries to push them apart.
  • Give both gears the same width and line them up.

The order is: face width up to 12·m, then module, and material last. Raising the module has a cost: keep the diameter and z drops, so the pinion may undercut; keep z and the diameter and center distance grow.

diagram
The method in order: face width, module, material; before you trust it, the hub and the bench.

Worked example: a 3:1 reduction for a NEMA 17

The brief: a pinion on the shaft of a NEMA 17 with 0.45 N·m holding torque and a 3:1 reduction, all in PLA, at 10 MPa allowable. A typical NEMA 17 gives 0.40 to 0.55 N·m holding torque; check your motor's datasheet.

Attempt 1: m 1, z 17, b 10. d = 17 mm. Ft = 2·450 / 17 = 52.9 N. σ = 52.9 / (10·1·0.303) = 17.5 MPa. That exceeds 10: it will not hold. Making m 1 work would need b = 17.5 mm, that is 17.5·m, well past the 12·m limit. Time to raise the module.

Attempt 2: m 1.5, z 17, b 12 (8·m). d = 25.5 mm. Ft = 900 / 25.5 = 35.3 N. σ = 35.3 / (12·1.5·0.303) = 6.5 MPa, below 10. The pinion's capacity is Ft max = 10·12·1.5·0.303 = 54.5 N, and T max = 54.5·12.75 ≈ 0.70 N·m. The margin over holding torque is 0.70 / 0.45 ≈ 1.6. In PETG, at 12 MPa, it reaches about 0.83 N·m.

The wheel. z 51 gives you 3:1. d = 76.5 mm, outside diameter m·(z + 2) = 79.5 mm and center distance a = 1.5·(17 + 51)/2 = 51 mm. It sees the same Ft, but with Y ≈ 0.41 its stress is σ ≈ 4.8 MPa: not the critical one. In service, the output torque is 3 × 0.45 N·m times the efficiency of a dry printed spur stage (0.9–0.95): between 1.2 and 1.3 N·m.

If there were a second stage, its pinion would see the first stage's output torque. When checking peak torque, do not take efficiency off: with the motor stalled, friction may not be on your side, so count 3·0.45 = 1.35 N·m. The same m 1.5, b 12 pinion only takes 0.70: not enough. With m 2, z 17 and b 16 (8·m): d = 34 mm, Ft = 2·1350 / 34 = 79.4 N, σ = 79.4 / (16·2·0.303) = 8.2 MPa. It passes. The module grows toward the output. Ratios and efficiency over several stages are in Compound gear trains; if one spur stage is not enough, see Choosing a reducer.

The shaft connection fails before the teeth do. A plain D-shaft in a 12 mm printed hub carries 0.1 to 0.2 N·m, far below the 0.70 you have calculated. Fixing a part to a shaft uses this same pinion (m 1.5, z 17, b 12) as its example and gets it to about 0.8 N·m with a clamping hub. The motor's torque curve is explained in Choosing a motor.

Material: strength, heat, wear and moisture

Indicative allowable tooth stress and service temperature under load
Material Allowable tooth stress Service temperature under load
PLA 8–12 MPa ≈ 40 °C
PETG 12–15 MPa ≈ 50 °C
ASA ≈ 13–17 MPa (indicative) ≈ 80–85 °C
PC ≈ 15–20 MPa (indicative) ≈ 92–102 °C
PA-CF / PAHT-CF ≈ 23–30 MPa dry (indicative); lower once conditioned: measure it ≈ 150 °C dry; less when conditioned

The ASA, PC and PA-CF figures come from applying the same ¼–⅓ rule to the XY strength on current datasheets (52, 62 and 92 MPa; the PA-CF figure dry). They are indicative and vary by grade. Under load, design 15–20 °C below the HDT at 0.45 MPa if the plastic is amorphous (PLA, PETG, ABS, ASA, PC), and 15–20 °C below the HDT at 1.8 MPa if it is semi-crystalline, with or without fiber (nylon, PP, PA-CF, PET-CF, PPA-CF, PPS-CF).

PLA. Good for proving the mesh and for intermittent motion at room temperature. Turning fast or under load, it usually fails from heat before it breaks: friction between the flanks heats them, they soften and smear plastic, and the tips round over. The motor also heats the pinion through the shaft. Measure the temperature of the motor's front face after an hour's work: if it approaches 40 °C, PLA will not do. To know what "fast" means for you, work out the pitch-line velocity, v = π·d·n: the 25.5 mm pinion at 600 rpm runs at 0.8 m/s. There is no reliable limit figure for a printed gear; measure the flank temperature at your speed.

PETG. Tougher, with a little more thermal headroom. In a test of printed gears running against a steel pinion (Tunalioglu and Agca, Polymers, 2022), PETG outlasted PLA and ABS. It is one test, and not enough to generalize to other printed pairs.

Nylon (PA, CoPA, PA12). The material for a gear that racks up revolutions. In tests at the University of Warwick (Zhang et al., Tribology International, 2020), one of the printed nylons beat injection-molded PA66 gears at low and medium torque; other printed nylons and composites in the same study did not. The specific filament matters. The catch is moisture: nylon absorbs it, swells and softens. Leave a little more backlash and measure parts once conditioned; the details are in Nylons and polyamides.

PA-CF and PAHT-CF. Stiff, and they hold the tooth shape when hot. Exposed fiber wears the mating gear if it is softer, and they need a hardened nozzle (Carbon and glass fiber filaments). POM is the plastic of molded gears, but as of late 2026 it is still a specialist filament. Tribological filaments (igus iglidur, for example) perform better against steel; against plastic, test them. The general comparison is in Which plastic for which mechanism.

Sustained load. A gear that holds a stationary weight, such as an arm that must not drop, works like a hook: constant stress for hours, and the problem becomes creep. For that part use PC, ASA or a fiber-filled filament, and bring the stress down (Creep and fatigue).

The pairing. Two different materials usually run with less friction and less wear than two identical ones, PA against PETG for instance; treat that as indicative and test it. A bought steel or brass pinion against a printed wheel works well, and it carries heat away too.

Printing it so the calculation holds

A gear is always printed flat: axis vertical, profile in XY. That way root bending acts along the beads, which is why the calculation uses XY strength. The reasons are in Layer orientation for mechanisms and Spur gears.

Walls form the tooth. An m 1.5 tooth is 2.36 mm thick at the pitch circle, but at the root, where Lewis puts the maximum, it is over 3 mm. Three walls per side (about 1.25 mm) fill the pitch circle and leave a gap at the root that the slicer plugs with gap fill; with 4 per side, about 1.65 mm, the root comes out all wall at m 1–1.5. Check it in the preview. Infill only works in the web and the hub. If a tooth breaks, more infill will not fix it; face width and module will. More in Walls, perimeters and infill.

Keep the seam off the working flanks and check it in the slicer preview (Where the seam goes). A seam on a flank is a weak spot and a step in the mesh.

Keep the root fillet the gear comes with. A sharp-cornered root concentrates stress exactly where Lewis puts the maximum.

Watch heat on small parts. On a 25 mm pinion each layer prints in very little time. If the slicer slows down to respect minimum layer time, the bead cools in time; if not, the tooth comes out distorted because the previous layer is still soft (Speed and cooling).

Lubrication

Gear flanks roll at the pitch point and slide away from it. Dry, between plastic flanks, the coefficient of friction μ sits between 0.15 and 0.4; greased or with PTFE it drops to 0.05–0.15. Less friction means less heat, so PLA survives more revolutions before softening, and wear goes down.

Use silicone grease, a plastic-safe PTFE grease or, with PC, PFPE grease, as a thin film on the flanks. Never use ester-based oils with ABS or PC; with PC, test any lubricant first, because it can cause environmental stress cracking. In a closed housing, use grease. In an open train that collects dust, use dry PTFE spray, because grease plus dust becomes abrasive paste. Many sprays carry a solvent that attacks PC, ABS and even PLA: let it flash off and try it on a sacrificial part first.

Grease will not fix an overloaded gear. If the tooth fails the Lewis check, greasing only delays the break. The lubricant table and the PC compatibility test are in Friction and wear.

When it fails

Three printed spur gears with different failures: a tooth snapped at the root, flanks melted and rounded by heat, and worn flanks with dust of the same color next to the gear
Three printed spur gears with different failures: a tooth snapped at the root, flanks melted and rounded by heat, and worn flanks with dust of the same color next to the gear
Printed gear failures
Symptom Cause Fix
Tooth snapped cleanly at the root σ above the allowable: module or face width too small, undercut, sharp-cornered root, or a crash into an end stop Face width up to 12·m, then module; keep the root fillet; z ≥ 17; soft stop or torque limiter
Several broken teeth in the same angular zone Local defect: seam, cold layer, eccentric hub forcing the mesh tight in that zone Move the seam; check the hub's radial runout (Fixing a part to a shaft)
Shiny flanks, smeared plastic and rounded tips (PLA) Friction heats the flanks above the service temperature Grease, lower speed, wider face; PETG or PA
Dust the color of the part and growing backlash Wear: same material pair running dry, rough flanks Pair different materials, grease, PA or a tribological filament
Skips teeth under load Too much backlash, or the center distance opens up (housing that gives, shaft supported at one end only) Less backlash; stiffen the housing between shafts; support the shaft on both sides
Binds or heats up running unloaded Not enough backlash Give backlash one way only: the "Spur gear" object already includes it, so do not also spread the centers (Spur gears)
Only one edge of the face worn or broken Misalignment, or a face too wide for the shaft's deflection b ≤ 12·m; shaft supported on both sides
Slips on the shaft with teeth intact The hub fails, not the tooth Fixing a part to a shaft
Tooth deforms over weeks holding a stationary load Creep PC, ASA or a fiber-filled filament; lower the stress
Nylon gear that binds after a few days It absorbed moisture and swelled More backlash; measure the conditioned part

How to test it

Torque bench. Lock the input, fit an arm of radius r on the output and hang a known mass M, or pull with a luggage scale. Output torque is T = M·g·r. A 1 kg mass at 100 mm gives 1·9.81·0.1 = 0.98 N·m. The output wheel sees that torque; the pinion sees it divided by the ratio. On the 3:1 reduction, 0.98 N·m at the output is 0.33 N·m at the pinion.

Test to failure. Print a sacrificial pair and raise the torque until it breaks. Convert the breaking torque to the gear that broke, dividing by the ratio if it was the pinion, and Lewis gives you the stress at which your tooth fails, on your printer and with your filament. Design with ¼–⅓ of that figure instead of the datasheet one: it is the allowable stress calibrated for your machine.

Endurance test. At real speed and load, for hours, not minutes. Measure backlash at the start and the end with a pointer on the output arm, measure the flank temperature (or touch it) and look for dust. Growing backlash is the first sign of wear.

Before printing the whole housing, print only the pair and a rigid bracket at the center distance. It is this mechanism's test coupon: in an hour you know whether the mesh and the face width work. How to set up the bench and run the endurance test is covered in Testing a mechanism before you trust it; the idea of printing only the part you doubt, in Test coupons.

See also

Design it in KapyCAD

Sketch the mechanism with these dimensions. Each one stays a value you can change after the first test print.

Free plan, no card. Runs in your browser, nothing to install.

Open the editor

Still have a question?