Using bought steel springs

18 min readUpdated Nov 2026

A steel spring costs pennies and, loaded within its catalog limits, does not relax at room temperature: it gives the same force for years. A printed one is free and built into the part, but it loses force if it sits loaded and it is bulky for the rate it gives. Buy steel when the spring stays loaded, runs thousands of cycles or gets warm, and design the printed part around its catalog line. The coil formulas are in Coil springs; here they are only used.

When steel wins

The shear modulus decides it. Hard-drawn spring wire and music wire have G ≈ 81.5 GPa; printed PLA, about 0.9 GPa. In shear, steel is about 90 times stiffer. With the same mean diameter and the same number of coils, a steel spring gives the same rate with wire about 3 times thinner (the fourth root of 90). Or, keeping the wire and the coil count, it gets there with a coil diameter about 4.5 times smaller (the cube root of 90).

Buy steel when:

  • The spring is always loaded: a latched catch, a preloaded lid, a detent sitting in its holding position. Printed plastic relaxes under a sustained strain.
  • Cycles run into the thousands.
  • The part gets warm. Under load, PLA works up to about 40 °C and PETG to about 50 °C (Heat, cold, sunlight and chemicals).
  • You need to know the force before you print. A catalog rate is a given; a printed G has to be calibrated.
  • Space is tight.

Print it when the force is light and intermittent and a failure costs nothing (a toy, a quick mock-up of a movement), when nobody sells the shape (a leaf, a serpentine, a flexure built into the part: Leaf and cantilever springs, TPU and lattice springs) or when the part cannot carry metal.

For damp, outdoor or food-adjacent parts, use 1.4310 stainless (G ≈ 70 GPa): with the same geometry it gives 14 % less force (R × 70/81.5). Indoors, zinc-plated or oiled music wire is enough.

Reading a catalog line

printed buttoncentering spigotDd (spigot)Di (inside diameter)flat seatDe (outside diameter)Dh (bore)printed housing0.5 × 45° chamferpocketF = R·(L0 − L)L0 (free)restpressedLnLc (solid)do not go below
Every symbol in the catalog becomes a dimension on the printed part: Dh sets the bore and Dd the spigot; the working lengths must stay above Ln.

A catalog line for a compression spring gives:

  • d: wire diameter.
  • De: outside diameter. From it come the inside diameter, Di = De − 2d, and the mean, Dm = De − d.
  • L0: free length.
  • Lc: solid length, with every coil touching.
  • Ln: minimum working length, as far as the maker allows you to compress it. It leaves a small gap between coils so the spring is never the end stop.
  • R: the rate, in N/mm: the k of Coil springs.
  • Fn: the force at Ln.
  • Dd max and Dh min: the thickest guide rod or spigot that fits inside and the narrowest bore it goes into. These are the two figures you need to design the housing. Lee Spring calls them suggested rod diameter and suggested hole diameter.

The force at any installed length L is F = R·(L0 − L). Preload is the force at the rest length. At the end of the stroke, the spring must never go below Ln. If the sheet does not give Ln, use at most 80–85 % of the travel to solid, L0 − Lc.

Within one series (same d and De), Fn is the same at every length, because it is a stress limit of the wire. With d 1.0 and De 8.7, free lengths of 12, 18, 27 and 42 mm give R = 6.29, 4.00, 2.59 and 1.63 N/mm, and all reach about 37 N at Ln. Longer means a lower rate and more travel, with the same maximum force.

Look at the ends. Closed ends, which from 0.5–1 mm wire upwards are usually ground as well, sit flat and square. With open ends, the cut tip of the wire digs into the printed seat and tilts the spring. Ask for closed and ground ends. With closed ends, total coils are active coils plus two (EN 13906-1).

Easy-to-find sizes (stock series similar to DIN 2098)
d (mm) De (mm) L0 (mm) R (N/mm) Dd max (mm) Dh min (mm)
0.5 2.8 4–13 14.8–3.8 1.6 3.1
0.5 5.3 8–29 1.6–0.42 4.0 5.8
0.63 11.6 26–98 0.34–0.09 10.0 12.7
0.8 6.0 8–28 8.4–2.2 4.0 6.6
1.0 8.7 12–42 6.3–1.6 6.3 9.3
1.25 13.0 18–63 4.3–1.1 10.0 14.0
1.6 13.6 17–59 10.9–2.8 10.0 14.3

The values come from a European catalog of standard springs (Federnfabrik Schmid, checked in November 2026). Similar series, with the same d × De pairs or nearly, are in almost every European catalog (Gutekunst, Vanel…), and the values differ by a few tenths from one maker to the next. Always work from your supplier's sheet.

In that table, Dh min sits 5 to 11 % above De, and always at least 0.3 mm above. Dd max sits 3 to 11 % below Di; Lee Spring recommends around 10 %. These clearances are meant for machined parts; a printed bore needs more.

The housing: bore, spigot and seat

The bore needs clearance for three reasons. The outside diameter has a tolerance, about ±0.1 mm on small springs. The spring is not perfectly straight. And the diameter grows as it compresses: each coil keeps its length of wire, so when the pitch goes from p to p' it opens out, Dm' = √(Dm² + (p² − p'²)/π²), with p' = d at solid. That is a maximum, worked out with the ends free to turn. On a close-pitched spring it amounts to hundredths of a millimeter: +0.04 mm with d 1.0, De 8.7 and L0 12. On a long, open-pitched one, tenths: +0.21 mm with d 0.63, De 11.6 and L0 40. Dh min already covers it. For an assortment spring with no sheet, work it out.

Printed bore = Dh min + whatever the printer takes off a hole. A small vertical hole prints 0.1–0.3 mm tight on the diameter because of facets, the bead bulging into the curve and shrinkage (Why holes print small). Model Dh min + 0.2–0.3 mm and tune it with a coupon. With the axis vertical, the bore prints round. With the axis horizontal, a hole up to 6 mm prints clean; between 6 and 10 mm the roof sags 0.1–0.3 mm, acceptable except in a pivot or a precision hole; above 10 mm, draw it as a teardrop or with a flat roof (Designing out supports).

Printed spigot = Dd max − the sliding fit on diameter. Printed spigots come out on size or slightly fat. Sliding fit: 0.20 mm per side (0.40 on the diameter) on a modern bedslinger and 0.15 (0.30 on the diameter) on an enclosed CoreXY (Real printed clearances). Chamfer the tip (0.5 × 45°) or taper it so the spring finds it. A spigot one or two coils tall is enough to center the spring. A rod running the full length of the spring guides it against buckling and must stay below Di along its whole length.

Buckling, for reference only (it is worked out in Coil springs): with flat, parallel ends that cannot tilt, the spring is stable while L0/Dm < 5.26; if the ends can tilt, while L0/Dm < 2.63. Above that, guide it along its full length with the bore or a rod. Inside a blind bore it cannot kick out sideways.

The seat must be flat, square to the axis and as wide as the end coil. Bearing pressure is low: in the example below, the coil sits on π·Dm·d/2 ≈ 10.8 mm², so 3.5 N gives about 0.3 MPa. With light springs, the plastic is enough. With tens of newtons, or with an open end that digs in, put a steel washer underneath. Keep the seam away from the seat and the bore wall.

Orientation follows the rules in Layer orientation for mechanisms. A spigot that only centers and takes the load along its axis, pressing the layers together, can print standing up. A vertical post loaded from the side is stance C: avoid it. Orient the boss that takes the spring force so the spring pushes it into the part, pressing the layers together, rather than pulling a thin wall off its base.

Keeping it in during assembly. This is the most common complaint: you turn the part over and the spring jumps out. Depth alone does not hold it: a blind bore deep enough for at least half the free length keeps it upright while you close the part, but only if you assemble with the pocket facing up. To actually retain it, you have two options. The first is a spigot 0.1–0.2 mm thicker than Di over only the bottom millimeter: the bottom coil screws onto it and stays put, and the rest of the spigot stays clear. Try it on a coupon. The second is a threaded plug in a heat-set insert, which closes the pocket and lets you set the preload too (Designing for heat-set inserts).

The printed part carries the preload

Steel does not relax; the printed part around it does. Whatever holds the spring compressed (a snap, a lid, a screwed boss) carries the preload for the whole life of the product and, over time, creeps. At room temperature, PLA holds a light sustained load about as well as PETG: no reliable data on printed parts says which creeps more. PETG only wins when the part gets warm. For a sustained load, use PC or ASA, or a fiber-filled filament if the part is not a spring (Creep and fatigue).

That is why a soft, long spring pays off. Any error in installed length changes the force by R × error. A ±0.3 mm tolerance stack on that length (Assemblies and tolerance stackups) moves the force by ±0.07 N with R 0.22 N/mm (L0 40), and by ±1.2 N with R 4.0 N/mm (L0 18). The same happens if the housing gives 0.1–0.2 mm over the months.

force F (N)compression from rest (mm) →0102030R 0.22 N/mm (L0 40)R 4.0 N/mm (L0 18)12 mm strokeout of travel±0.3 mm±0.07 N±1.2 N
The same ±0.3 mm band on installed length changes the force by ±0.07 N on the soft spring and by ±1.2 N on the stiff one. The stiff one also reaches Ln before the 12 mm stroke is done.

If a printed snap holds the preload, size it for the sustained load, not for the click (Print-friendly snap fits). If screws hold it, they should thread into heat-set inserts.

Worked example: a push-button return

It is the same brief as the printed example in Coil springs, so you can compare: the return for a large push button, 12 mm of stroke, a little preload at rest so it does not rattle, about 3–3.5 N when pressed, with the button sliding in a printed Ø16 bore, PLA housing, daily use.

The rate. (F pressed − F rest)/stroke ≈ (3.5 − 0.9)/12 ≈ 0.22 N/mm. In the catalog: d 0.63, De 11.6, Dm 10.97, L0 40, R 0.22 N/mm, Lc 4.7, Ln 6.5, Fn 7.3 N, Dd max 10.0, Dh min 12.7. Its index is C = 10.97/0.63 ≈ 17, above the 12 that Coil springs recommends: it is a soft spring that tangles in the bag and has a looser tolerance on De. In a pocket this makes no difference, and no other row in the series gives 0.22 N/mm with 12 mm of stroke: the longest d 0.5 × De 5.3 gives 0.42 N/mm and L0/Dm ≈ 6, too slender.

The lengths. At rest, 36 mm: 4 mm of compression, 0.88 N. Pressed, 24 mm: 16 mm of compression, 3.52 N. That length is well above Ln: it uses 48 % of the usable travel (L0 − Ln = 33.5 mm) and works far from its stress limit, so it will not take a set.

Why not a stiffer, shorter one. The d 1.0, De 8.7, L0 18, with R 4.00 and Ln 8.8, has only 9.2 mm of usable travel: it cannot reach 12 mm.

Buckling. L0/Dm = 40/10.97 ≈ 3.7, above 2.63. The button slides guided in the Ø16, so both seats stay parallel: the 5.26 limit applies, and 3.7 is below it. It is stable and needs no side guide; the pocket around the spring only adds margin.

The pocket and the spigot. The spring sits in a pocket of Dh min 12.7 at the bottom of the housing: model Ø13.0 and tune it with a coupon. The hole will print at 12.7–12.9 mm. Even if the spring went solid, its outside diameter would grow to about 11.6 + 0.21 = 11.8 mm, leaving about 0.9–1.1 mm of diametral clearance; besides, the end stop never lets it get there. The button's spigot: Dd max 10.0 → Ø9.6, 3 mm tall, 0.5 mm chamfer. The pocket does not have to hold the whole spring: at rest, part of the 36 mm stands proud and sits inside the button's Ø16. What stops the stroke at 24 mm is the button's end stop, not the spring.

Tolerance. With this spring, the ±0.3 mm stack moves the force by ±0.07 N, under 8 % of the preload. Even if the housing gives, the feel does not change.

The push-button return with a catalog spring
Requirement Value Check
Spring d 0.63 × De 11.6 × L0 40, R 0.22 N/mm stock series
Force at rest / pressed 0.88 N at 36 mm / 3.52 N at 24 mm 24 mm > Ln 6.5 mm
Usable travel used 16 of 33.5 mm (48 %) far from Fn 7.3 N
L0/Dm 3.7 < 5.26 (button guided in the Ø16)
Spring pocket Ø13.0 De at solid ≈ 11.8 mm
Spigot Ø9.6 × 3, 0.5 chamfer Dd max 10.0 − 0.4
±0.3 mm tolerance stack ±0.07 N < 8 % of preload

The printed spring in Coil springs (d 2, D 12, 7 coils, about 35 mm) works right at PLA's limit; this one sits far below steel's limit and will not lose force even if the button is left pressed.

Bought extension and torsion springs

Extension. The force is F = F0 + R·x, where F0 is the initial tension: the coils leave the factory pressed against each other, which a printed spring cannot achieve. Do not stretch it past the catalog's maximum length: the hooks yield first. Run each hook over a steel pin or the shank of a screw passing through a printed boss, never over a printed peg that grows in Z and is loaded from the side (stance C). A printed anchor lying flat in the layer plane takes light loads. The hook slot is d + 0.4 mm (0.3 on an enclosed CoreXY), with a rounded bearing edge. If it must not come apart even when overloaded, use a drawbar spring (a compression spring between two loops): when it goes solid it acts as a stop instead of opening its hooks. It is covered in Coil springs.

Torsion. Load it in the direction that winds the coils tighter. As it winds up, the diameter shrinks: D' = D·Nb/(Nb + θ), with Nb the body coils and θ the rotation in turns. With 5 coils and 90° (0.25 turns), D' = D × 0.952. Make the arbor 10 % thinner than the smallest inside diameter the spring reaches. The legs bear in printed slots: make the bearing face a wall in XY, so the leg pushes across the thickness of several layers and not against the edge of one. Slot width: leg d + 0.4 mm (0.3 on an enclosed CoreXY). You will see this applied in Spring-return hinge and Spring-return trigger.

Music wire bent by hand, such as a bail or a detent wire, is sized as a beam: see Over-center draw latch.

Springs with no sheet: assortments and salvage

Boxed assortments and springs salvaged from pens, battery contacts or old appliances come with no data. Measure d and De, work out Dm = De − d, count the total coils and take off two if the ends are closed. With that, R = G·d⁴/(8·Dm³·n), with G = 81.5 GPa. If you do not know whether it is stainless, use 81.5 GPa and let the scale decide.

Measure d with a micrometer. R goes with d⁴: an error of 0.025 mm when measuring a 0.5 mm wire throws the calculated rate out by about 20 % ((0.525/0.5)⁴ = 1.22). Digital callipers read hundredths, but their accuracy is around ±0.02–0.03 mm, exactly that error. If all you have is callipers and the spring has ground ends, compress it to solid, measure that length and divide it by the total coils.

Then check it with kitchen scales and a stop: measure the force at two lengths and work out R = ΔF/Δx (Test coupons). Solid length is roughly total coils × d with ground ends, and (total coils + 1.5) × d with ends that are only closed; apply the same 80–85 % margin.

A typical assortment box of 200 springs covers diameters from 4 to 12 mm and lengths from 10 to 70 mm, with no rates. It is fine for prototypes. For a product, pick a catalog spring you can buy again with the same rate.

When it fails

Bought springs in printed parts: what goes wrong and the fix
Symptom Cause Fix
Rubs or jams in the bore printed hole comes out small, diameter growth on an open-pitched spring, elephant's foot at the mouth bore = Dh min + 0.2–0.3, chamfer the mouth, coupon
Tilts and the button wobbles open ends, crooked seat, L0/Dm over the limit with no guide closed and ground ends, spigot, guide in the bore
Force drops after a few weeks the part holding it has crept: snap opened up, boss sunk softer, longer spring, PC or ASA support, screws in inserts
Force far from the calculated value d measured with callipers, n counted including the end coils d with a micrometer, n = total − 2, check on scales
Bottoms out hard or loses height compressed below Ln or to solid printed end stop that halts the stroke above Ln
Falls out during assembly nothing retains it: depth does not hold it upside down spigot that grips the bottom coil, or a plug; deep bore if you assemble face up
Extension hook tears off the peg vertical peg loaded from the side (stance C) steel pin through a boss
Torsion spring binds on its arbor the inside diameter shrinks as it winds up arbor 10 % thinner than the wound-up inside diameter

How to test it

Print the housing on its own first: a short coupon with the bore and spigot at the chosen size and two variants at ±0.1 mm. Fit the spring and compress it to the pressed length with a screw or by hand: it must go in and come out without snagging (Test coupons, Iterate and measure).

Measure the force at rest and pressed with kitchen scales and compare it with R·(L0 − L).

Then the assembly: leave it 48 hours in the latched or pressed position, in the place where it will work, and measure the force again. If it has dropped, it is the printed part that has given, not the spring (Testing a mechanism before you trust it).

See also

Design it in KapyCAD

Model the joint with these dimensions. Each one stays a value you can change after the first test print.

Free plan, no card. Runs in your browser, nothing to install.